Comparative Study of Solution Heat Treatment of IN738LC Superalloy in Conventional Conditions and Salt Bath

被引:8
|
作者
Shajari, Yazdan [1 ]
Razavi, Seyed Hossein [2 ]
Seyedraoufi, Zahra-Sadat [3 ,4 ]
机构
[1] Mat & Energy Res Ctr, Karaj 141554777, Iran
[2] Iran Univ Sci & Technol IUST, Sch Met & Mat Engn, Tehran, Iran
[3] Islamic Azad Univ, Dept Mat Engn, Karaj Branch, Karaj, Iran
[4] Islamic Azad Univ, Adv Mat Engn Res Ctr, Karaj Branch, Karaj, Iran
关键词
heating rate; IN738LC superalloy; salt bath; solutionizing heat treatment; gamma' precipitates; NICKEL-BASE SUPERALLOY; MECHANICAL-PROPERTIES; GAMMA'-CHARACTERISTICS; TURBINE BLADE; COOLING RATE; MICROSTRUCTURE; REJUVENATION; KINETICS; PRIME;
D O I
10.1007/s11665-021-06344-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, to investigate the impact of heating rate, the IN738LC superalloy was solutionized both in standard and salt bath conditions. For this purpose, the samples were solutionized in the temperature range of 1090-1200 degrees C for 30-120 minutes in normal conditions and 10-120 minutes in the salt bath. Afterward, samples were aged at 850 degrees C for 24 hours. The results of scanning electron microscopy (SEM) and field emission scanning electron microscopy (FESEM) showed that as the heating rate increased, the dissolution process improved. In contrast, as the time and temperature increased, the gamma' precipitates' volume fraction decreased in both the normal condition and the salt bath by 26.01 and 50.28 %, respectively. The size of the remaining gamma' precipitates after dissolution in the salt bath was about 16 nm smaller than normal ones. The size and volume fraction of the residual precipitates in the salt bath increased at high temperatures compared to the normal ones due to the attachment mechanisms' activation. Solubility in the salt bath reduced the size of primary gamma' in the normal range and increased the volume fraction of the secondary gamma' precipitates after the aging. This alloy's hardness is strongly influenced by the characteristics of the gamma precipitates and the solutionizing process variables. Therefore, the results indicated that the secondary gamma' precipitates are about 16 nm smaller than the usual one, which has a remarkable impact. After aging, increasing the heating rate during the solutionizing resulted in a further rise in the hardness and reduced the hardness after solutionizing. However, in both conditions, as the time of solutionizing reduced and temperature increased, the samples' hardness after solution decreased, and the hardness after aging increased.
引用
收藏
页码:2525 / 2541
页数:17
相关论文
共 50 条
  • [1] Comparative Study of Solution Heat Treatment of IN738LC Superalloy in Conventional Conditions and Salt Bath
    Yazdan Shajari
    Seyed Hossein Razavi
    Zahra-Sadat Seyedraoufi
    Journal of Materials Engineering and Performance, 2022, 31 : 2525 - 2541
  • [2] Effect of Solid Solution Treatment on the Microstructure and Mechanical Properties of IN738LC Superalloy
    Kim, Jeong-Min
    Park, Joon-Sik
    Yun, Ho-Seob
    Lee, Seung-Jin
    An, Seong-Uk
    APPLIED MATERIALS AND ELECTRONICS ENGINEERING, PTS 1-2, 2012, 378-379 : 744 - +
  • [3] Heat Input and the Liquation Cracking of Laser Welded IN738LC Superalloy
    Montazeri, M.
    Ghaini, F. Malek
    Ojo, O. A.
    WELDING JOURNAL, 2013, 92 (09) : 258S - 264S
  • [4] Segregation Phenomenon of As-Cast and Heat Treatment Microstructures in Investment Casting of IN738LC Superalloy
    Choe, Byung Hak
    Han, Sung Hee
    Kim, Dae Hyun
    Ahn, Jong Kee
    Lee, Jae Hyun
    KOREAN JOURNAL OF MATERIALS RESEARCH, 2021, 31 (07): : 409 - 419
  • [5] Preferred Orientations in the Superalloy IN738LC after Different Aging Heat Treatments
    Balikci, Ercan
    Ferrell, R.E.
    Raman, Aravamudhart
    International Journal of Materials Research, 1999, 90 (02): : 141 - 146
  • [6] Preferred orientations in the superalloy IN738LC after different aging heat treatments
    Balikci, E
    Ferrell, RE
    Raman, A
    ZEITSCHRIFT FUR METALLKUNDE, 1999, 90 (02): : 141 - 146
  • [7] Preferred orientations in the superalloy IN738LC after different aging heat treatments
    Louisiana State University, Baton Rouge, LA, United States
    不详
    不详
    Z Metallkd, 2 (141-146):
  • [8] A study of the LCF characteristics of the Ni-based superalloy IN738LC
    Dongkeun Lee
    To Kang
    Jae-Mean Koo
    Chang-Sung Seok
    Sung-Jin Song
    International Journal of Precision Engineering and Manufacturing, 2015, 16 : 775 - 780
  • [9] A Study of the LCF Characteristics of the Ni-based Superalloy IN738LC
    Lee, Dongkeun
    Kang, To
    Koo, Jae-Mean
    Seok, Chang-Sung
    Song, Sung-Jin
    INTERNATIONAL JOURNAL OF PRECISION ENGINEERING AND MANUFACTURING, 2015, 16 (04) : 775 - 780
  • [10] A Study of TMF Characteristics of Ni-base Superalloy IN738LC
    Lee, Dongkeun
    Lee, Jeong-Min
    Koo, Jae-Mean
    Seok, Chang-sung
    Kim, Jaewon
    ADVANCED MATERIALS, MECHANICS AND INDUSTRIAL ENGINEERING, 2014, 598 : 28 - 32