Surface modification and deuterium retention in hot-rolled potassium doped tungsten alloy exposed to deuterium plasma

被引:4
|
作者
Ma, Xiaolei [1 ]
Wang, Ting [2 ,3 ]
Zhang, Xiaoxin [1 ,7 ]
Yuan, Yue [2 ,3 ]
Cheng, Long [2 ,3 ]
Zhu, Jipeng [4 ]
Lv, Wei [5 ]
Lang, Shaoting [6 ]
Wang, Zihao [1 ]
Ge, Changchun [1 ]
Yan, Qingzhi [1 ,7 ]
机构
[1] Univ Sci & Technol Beijing, Inst Nucl Mat, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
[2] Beihang Univ, Sch Phys, Beijing 100191, Peoples R China
[3] Beihang Univ, Beijing Key Lab Adv Nucl Mat & Phys, Beijing 100191, Peoples R China
[4] Scicence & Technol Surface Phys & Chem Lab, Chengdu 621908, Sichuan, Peoples R China
[5] North China Elect Power Univ, Inst Adv Mat, Beijing 102206, Peoples R China
[6] Xinxiang Univ, Mech & Elect Engn, Xinxiang 453000, Peoples R China
[7] Univ Sci & Technol Beijing, Xueyuan Rd 30, Beijing 100089, Peoples R China
基金
中国国家自然科学基金;
关键词
Potassium doped tungsten alloy; Deuterium plasma exposure; Surface blistering; Deuterium retention; HIGH-FLUX; THERMAL-SHOCK; MECHANICAL-PROPERTIES; HEAT-TREATMENTS; LOW-ENERGY; HELIUM; MICROSTRUCTURE; IRRADIATION; PURE; DEPENDENCE;
D O I
10.1016/j.jnucmat.2022.153890
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A 25 kg potassium doped tungsten (KW) plate dispersed with similar to 71 nm K bubbles was prepared by hot rolling firstly. In order to evaluate the radiation resistance of KW, the surface blistering and deuterium (D) retention were investigated on KW and pure tungsten (PW), which were exposed to low-energy (50 eV) and high-flux ( similar to 10 22 D m -2 s -1 ) D plasmas at 523 K and 573 K to a fluence of 1.08 x 10 26 m -2 . After irradiation, D desorption information of all the irradiated samples were measured by thermal desorption spectroscopy (TDS). The results indicate that severe blistering occurs on both PW and KW under different irradiation conditions. Compared to PW, KW tends to form more but smaller blisters on the surface. Nevertheless, the blistering area ratio of KW is comparable with that of PW. In addition, the blisters prefer to form on those grains with surface orientation close to (111). In terms of D retention, compared with PW, the total D retention of KW increases by a factor of similar to 2.5 under both irradiation conditions. The present results indicate that the presence of K bubbles will increase the D retention. The reasons for the difference in surface morphology evolution and total D retention of PW and KW are discussed in detail. (c) 2022 Elsevier B.V. All rights reserved.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] Surface modification and deuterium retention in hot-rolled potassium doped tungsten alloy exposed to deuterium plasma
    Ma, Xiaolei
    Wang, Ting
    Zhang, Xiaoxin
    Yuan, Yue
    Cheng, Long
    Zhu, Jipeng
    Lv, Wei
    Lang, Shaoting
    Wang, Zihao
    Ge, Changchun
    Yan, Qingzhi
    Journal of Nuclear Materials, 2022, 568
  • [2] Surface modification and deuterium retention in rhenium doped tungsten exposed to low energy deuterium plasma
    Xia, Tongjun
    Yan, Jing
    Han, Wenjia
    Wang, Zizhao
    Jiang, Zhenyu
    Wu, Jianwei
    Shi, Yongzhi
    Wang, Zhanlei
    Ye, Xiaoqiu
    Wu, Jiliang
    Zhu, Kaigui
    FUSION ENGINEERING AND DESIGN, 2021, 173
  • [3] Deuterium retention in chemically vapor deposited tungsten carbide coatings and hot-rolled tungsten exposed to low-energy deuterium plasma
    Vladimir Kh.Alimov
    Joachim Roth
    Tungsten, 2022, (01) : 10 - 19
  • [4] Deuterium retention in chemically vapor deposited tungsten carbide coatings and hot-rolled tungsten exposed to low-energy deuterium plasma
    Vladimir Kh. Alimov
    Joachim Roth
    Tungsten, 2022, 4 : 10 - 19
  • [5] Deuterium retention in chemically vapor deposited tungsten carbide coatings and hot-rolled tungsten exposed to low-energy deuterium plasma
    Vladimir KhAlimov
    Joachim Roth
    Tungsten, 2022, 4 (01) : 10 - 19
  • [6] Deuterium retention in chemically vapor deposited tungsten carbide coatings and hot-rolled tungsten exposed to low-energy deuterium plasma
    Alimov, Vladimir Kh
    Roth, Joachim
    TUNGSTEN, 2022, 4 (01) : 10 - 19
  • [7] Surface modification and deuterium retention of tungsten and tungsten-rhenium alloys exposed to deuterium plasma
    Zhang, Xuexi
    Qiao, Li
    Zhang, Hong
    Yao, Weizhi
    He, Wenhao
    Li, Yuhong
    Wang, Peng
    NUCLEAR MATERIALS AND ENERGY, 2021, 29
  • [8] Decreased surface blistering and deuterium retention in potassium-doped tungsten exposed to deuterium plasma following ion irradiation
    Ma, Xiaolei
    Zhang, Xiaoxin
    Wang, Ting
    Gao, Yuan
    Yuan, Yue
    Cheng, Long
    Zhu, Jipeng
    Lv, Wei
    Lang, Shaoting
    Ge, Changchun
    Yan, Qingzhi
    NUCLEAR FUSION, 2023, 63 (02)
  • [9] Deuterium retention and surface morphology modification in oxidized tungsten exposed to D plasma
    Puyang, S. A.
    Lyu, Y. M.
    Nian, F. F.
    Xu, Y. P.
    Yang, Z. S.
    Zhou, H. S.
    Luo, G. -N.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2021, 46 (61) : 31346 - 31352
  • [10] Surface blistering and deuterium retention behaviors in pure and ZrC-doped tungsten exposed to deuterium plasma
    Zhang, Xue-Xi
    Qiao, Li
    Zhang, Hong
    Li, Yu-Hong
    Wang, Peng
    Liu, Chang-Song
    NUCLEAR FUSION, 2021, 61 (04)