Mechanical properties of V-4Cr-4Ti alloy after first-wall coating with tungsten

被引:7
|
作者
Nagasaka, Takuya [1 ]
Muroga, Takeo [1 ]
Watanabe, Hideo [2 ]
Kasada, Ryuta [3 ]
Iwata, Noriyuki [3 ]
Kimura, Akihiko [3 ]
机构
[1] Natl Inst Nat Sci, Natl Inst Fus Sci, Toki, Gifu 5095292, Japan
[2] Kyushu Univ, Appl Mech Res Inst, Fukuoka 8168580, Japan
[3] Kyoto Univ, Inst Adv Energy, Kyoto 6110011, Japan
关键词
ACTIVATION VANADIUM ALLOY; TI ALLOYS; MICROSTRUCTURE;
D O I
10.1016/j.jnucmat.2011.02.035
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A first-wall coating was fabricated with tungsten on a reference V-4Cr-4Ti alloy (NIFS-HEAT-2, NH2) substrate by a vacuum plasma spray (VPS) process and brazing (BR). The hardness, fracture stress, and elastic modulus of tungsten (W) coating applied by the vacuum plasma spray process (VPS-W) were lower than the tungsten used for brazing (BR-W). The low mass density and defects of VPS-W are thought to be responsible for the degradation of the strength. The NH2 substrate indicated hardening and embrittlement produced by the W coating and some post-coating heat treatment (PCHT). Hardening and embrittlement by a VPS coating can be recovered by removing hydrogen from the NH2 substrate in a vacuum by annealing at 673 K. Oxygen transfer from the W coating to the NH2 substrate was indicated above 1173 K but did not induce embrittlement of the substrate. Hardening by the BR process can be recovered by PCHT at 1273 K, but embrittlement was not improved. The mechanisms of the hardening and embrittlement are discussed based on a microstructural analysis. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:306 / 309
页数:4
相关论文
共 50 条
  • [1] Mechanical properties of laser weldment of V-4Cr-4Ti alloy
    Heo, NJ
    Nagasaka, T
    Muroga, T
    Nishimura, A
    Shinozaki, K
    Watanabe, H
    FUSION SCIENCE AND TECHNOLOGY, 2003, 44 (02) : 470 - 474
  • [2] Pulse current electrodeposition of tungsten coatings on V-4Cr-4Ti alloy
    Jiang, Fan
    Zhang, Yingchun
    Li, Xuliang
    FUSION ENGINEERING AND DESIGN, 2015, 93 : 30 - 35
  • [3] Helium thermal desorption and retention properties of V-4Cr-4Ti alloy used for first wall of breeding blanket
    Hirohata, Y
    Yamada, T
    Yamauchi, Y
    Hino, T
    Nagasaka, T
    Muroga, T
    FUSION ENGINEERING AND DESIGN, 2006, 81 (1-7) : 193 - 198
  • [4] Verification of mechanical properties of a V-4CR-4TI alloy using finite element method
    Lee, CY
    Donahue, EG
    Odette, GR
    ADVANCES IN FRACTURE AND STRENGTH, PTS 1- 4, 2005, 297-300 : 1013 - 1018
  • [5] Metallurgical and mechanical properties of laser weldment for low activation V-4Cr-4Ti alloy
    Heo, NJ
    Nagasaka, T
    Muroga, T
    Nishimura, A
    Shinozaki, K
    Takeshita, N
    FUSION ENGINEERING AND DESIGN, 2002, 61-62 : 749 - 755
  • [6] Thermomigration of tritium in V-4Cr-4Ti alloy
    Hashizume, Kenichi
    Ogushi, Kazuhiro
    Otsuka, Teppei
    Tanabe, Tetsuo
    JOURNAL OF NUCLEAR MATERIALS, 2011, 417 (1-3) : 1175 - 1178
  • [7] Recrystallization nucleation in V-4Cr-4Ti alloy
    Ding, Jianwen
    Yang, Shanwu
    Liu, Guoliang
    Li, Qiufan
    Zhu, Boling
    Zhang, Mengqi
    Zhou, Lujun
    Shang, Chengjia
    Zhan, Qian
    Wan, Farong
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 777 : 663 - 672
  • [8] Tungsten coating prepared on V-4Cr-4Ti alloy substrate by electrodeposition from molten salt in air atmosphere
    Jiang, Fan
    Zhang, Yingchun
    Li, Xuliang
    Sun, Ningbo
    Wang, Lili
    FUSION ENGINEERING AND DESIGN, 2014, 89 (02) : 83 - 87
  • [9] Tritium diffusion in V-4Cr-4Ti alloy
    Hashizume, K.
    Masuda, J.
    Otsuka, K. T.
    Tanabe, T.
    Hatano, Y.
    Nakamura, Y.
    Nagasaka, T.
    Muroga, T.
    FUSION SCIENCE AND TECHNOLOGY, 2008, 54 (02) : 553 - 556
  • [10] Hydrogen solubility in V-4Cr-4Ti alloy
    Buxbaum, RE
    Smith, DL
    Park, JH
    JOURNAL OF NUCLEAR MATERIALS, 2002, 307 : 576 - 579