The Effect of Preceramic Soldering on Fracture Resistance of 4-Unit Zirconia Fixed Dental Prostheses

被引:1
|
作者
Irem, Diler Ozkan
Comert, Zekeriya Yasar [1 ]
Alpkilic, Dilara Seyma [2 ]
Kelesoglu, Ergun [3 ]
Deger, Sabire Isler [2 ]
机构
[1] Yildiz Tech Univ, Fac Chem & Met, Istanbul, Turkey
[2] Istanbul Univ, Fac Dent, Dept Prosthodont, TR-34452 Istanbul, Turkey
[3] Turkish German Univ, Fac Mat Sci & Technol, Istanbul, Turkey
关键词
Zirconia; fixed dental prostheses; FDPs; preceramic soldering; fracture resistance; monolithic zirconia; ALL-CERAMIC BRIDGES; CRACK-GROWTH; RESTORATIONS; FAILURE; FATIGUE;
D O I
10.1111/jopr.13488
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose Preceramic soldering of zirconia may deliver better fitting restorations. However, there is not sufficient evidence regarding the influence of preceramic soldering of zirconia restorations on mechanical strength. The aim of this study was to evaluate the effect of preceramic soldering on the fracture load of 4-unit zirconia fixed dental prostheses (FDPs). Materials and methods Eighty samples of 4-unit FDPs between maxillary right first premolar and maxillary right second molar were prepared and two restorative materials were used as a framework (Z) and monolithic restoration (M). The samples were divided into two subgroups as control (C) and study (S). The restorations of study groups (S) were divided into two pieces and soldered with a bonding material (DCM HotBond Zirkon). The groups were divided into two subgroups for thermal cycle (T) application. After soldering and thermal cycling application, 4-point bending test was applied to the samples at a cross-head speed of 1 mm/min in a universal testing machine and the fracture load was recorded. The data was analyzed statistically, and the level of significance was set at alpha = 0.001. Results Statistically significant differences were found among the groups, based on the results of maximum failure loads (p < 0.001). The highest mean failure load was observed in the ZCT(-) group (1094.1 + 139.77 N), while the lowest mean failure load was obtained in the ZST(+) group (627.7 + 82.14 N). No significant difference was found among the groups MC and MS, MC, and ZC groups (p > 0.001). Thermal aging application caused lower fracture resistance in control and soldering groups (p < 0.001). Conclusions The preceramic soldering applications affected zirconia group negatively. However, the values were above the clinically acceptable static load bearing capacity for posterior teeth. Soldering did not cause a statistically significant difference for the fracture strengths of monolithic zirconia groups. Thermal cycling affected the fracture strength of zirconia and monolithic zirconia restorations negatively.
引用
收藏
页码:815 / 821
页数:7
相关论文
共 50 条
  • [1] The effect of pre-ceramic soldering on marginal and internal fit of 4-unit zirconia frameworks and monolithic zirconia fixed dental prostheses
    Irem, Diler Ozkan
    Alpkilic, Dilara Seyma
    Deger, Sabire Isler
    ODONTOLOGY, 2024, 112 (01) : 169 - 176
  • [2] The effect of pre-ceramic soldering on marginal and internal fit of 4-unit zirconia frameworks and monolithic zirconia fixed dental prostheses
    Diler Ozkan Irem
    Dilara Seyma Alpkilic
    Sabire Isler Deger
    Odontology, 2024, 112 : 169 - 176
  • [3] Effect of veneering technique on the fracture resistance of zirconia fixed dental prostheses
    Chaar, M. S.
    Witkowski, S.
    Strub, J. R.
    Att, W.
    JOURNAL OF ORAL REHABILITATION, 2013, 40 (01) : 51 - 59
  • [4] Fracture load of different veneered and implant-supported 4-UNIT cantilever PEEK fixed dental prostheses
    Soldatovic, Danka Micovic
    Liebermann, Anja
    Huth, Karin C.
    Stawarczyk, Bogna
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2022, 129
  • [5] Fracture load of different veneered and implant-supported 4-UNIT cantilever PEEK fixed dental prostheses
    Micovic Soldatovic, Danka
    Liebermann, Anja
    Huth, Karin C.
    Stawarczyk, Bogna
    Journal of the Mechanical Behavior of Biomedical Materials, 2022, 129
  • [6] Effect of connector configuration on the fracture load in conventional and translucent zirconia three-unit fixed dental prostheses
    Subsomboon, Chonticha
    Urapepon, Somchai
    JOURNAL OF ADVANCED PROSTHODONTICS, 2023, 15 (04): : 171 - 178
  • [7] In vitro study of the fracture resistance of monolithic lithium disilicate, monolithic zirconia, and lithium disilicate pressed on zirconia for three-unit fixed dental prostheses
    Choi, Jae-Won
    Kim, So-Yeun
    Bae, Ji-Hyeon
    Bae, Eun-Bin
    Huh, Jung-Bo
    JOURNAL OF ADVANCED PROSTHODONTICS, 2017, 9 (04): : 244 - 251
  • [8] Fracture behaviour of zirconia ceramic cantilever fixed dental prostheses in vitro
    Gabbert, Olaf
    Ohlmann, Brigitte
    Schmitter, Marc
    Gilde, Herbert
    Ruef, Thomas
    Rammelsberg, Peter
    ACTA ODONTOLOGICA SCANDINAVICA, 2008, 66 (04) : 200 - 206
  • [9] Precision of fit: zirconia three-unit fixed dental prostheses
    Beuer, Florian
    Naumann, Michael
    Gernet, Wolfgang
    Sorensen, John A.
    CLINICAL ORAL INVESTIGATIONS, 2009, 13 (03) : 343 - 349
  • [10] Precision of fit: zirconia three-unit fixed dental prostheses
    Florian Beuer
    Michael Naumann
    Wolfgang Gernet
    John A. Sorensen
    Clinical Oral Investigations, 2009, 13