Fischer-Tropsch synthesis: Effect of ammonia in syngas on the Fischer-Tropsch synthesis performance of a precipitated iron catalyst

被引:34
|
作者
Ma, Wenping [1 ]
Jacobs, Gary [1 ]
Sparks, Dennis E. [1 ]
Pendyala, Venkat Ramana Rao [1 ]
Hopps, Shelley G. [1 ]
Thomas, Gerald A. [1 ]
Hamdeh, Hussein H. [2 ]
MacLennan, Aimee [3 ]
Hu, Yongfeng [3 ]
Davis, Burtron H. [1 ]
机构
[1] Univ Kentucky, Ctr Appl Energy Res, Lexington, KY 40511 USA
[2] Wichita State Univ, Dept Phys, Wichita, KS 67260 USA
[3] Canadian Light Source Inc, Saskatoon, SK S7N 2V3, Canada
基金
加拿大创新基金会; 加拿大健康研究院; 加拿大自然科学与工程研究理事会;
关键词
Fischer-Tropsch synthesis; Fe catalyst; Biomass-to-liquids (BTL); Slurry phase reactor; Ammonia (NH3); Ammonium nitrate (NH4NO3); Nitric acid (HNO3); XRD; Mossbauer spectroscopy; XANES/EXAFS; SULFUR; KINETICS; SPECTROSCOPY; REDUCTION; OXIDE;
D O I
10.1016/j.jcat.2015.04.004
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The effect of ammonia in syngas on the Fischer-Tropsch synthesis (FTS) reaction over 100Fe/5.1Si/2.0Cu/3.0K catalyst was studied at 220-270 degrees C and 1.3 MPa using a 1-L slurry phase reactor. The ammonia added in syngas originated from adding ammonia gas, ammonium hydroxide solution, or ammonium nitrate (AN) solution. A wide range of ammonia concentrations (i.e., 0.1-400 ppm) was examined for several hundred hours. The Fe catalysts withdrawn at different times (i.e., after activation by carburization in CO, before and after co-feeding contaminants, and at the end of run) were characterized by ICP-OES, XRD, Mossbauer spectroscopy, and synchrotron methods (e.g., XANES, EXAFS) in order to explore possible changes in the chemical structure and phases of the Fe catalyst with time; in this way, the deactivation mechanism of the Fe catalyst by poisoning could be assessed. Adding up to 200 ppmw (wt. NH3/av. Wt. feed) ammonia in syngas did not significantly deactivate the Fe catalyst or alter selectivities toward CH4, C5+, CO2, C-4-olefin, and 1-C-4 olefin, but increasing the ammonia level (in the AN form) to 400 ppm rapidly deactivated the Fe catalyst and simultaneously changed the product selectivities. The results of ICP-OES, XRD, and Mossbauer spectroscopy did not display any evidence for the retention of a nitrogen-containing compound on the used catalyst that could explain the deactivation (e.g., adsorption, site blocking). Instead, Mossbauer spectroscopy results revealed that a significant fraction of iron carbides transformed into iron magnetite during co-feeding high concentrations of AN, suggesting that oxidation of iron carbides occurred and served as a major deactivation path in that case. Oxidation of chi-Fe5C2 to magnetite during co-feeding high concentrations of AN was further confirmed by XRD analysis and by the application of synchrotron methods (e.g., XANES, EXAFS). It is postulated that AN oxidized chi-Fe5C2 during FTS via its thermal dissociation product, HNO3. This conclusion is further supported by reaction tests with co-feeding of similar concentrations of HNO3. Additional oxidation routes of iron carbide to magnetite by HNO3 and/or by its thermal decomposition products are also considered: Fe5C2 + NOx (and/or HNO3) -> Fe3O4. In this study, ion chromatography detected that 50-80% HNO3 directly added or dissociated from AN eventually converted to ammonia during or after its oxidation of iron carbide, resulting from the reduction of NOx (NOx + H-2 + CO -> NH3 + CO2 + N-2 + H2O) by H-2 and/or CO. (C) 2015 Elsevier Inc. All rights reserved.
引用
收藏
页码:149 / 160
页数:12
相关论文
共 50 条
  • [1] FISCHER-TROPSCH SYNTHESIS ON A PRECIPITATED IRON CATALYST
    MADON, RJ
    TAYLOR, WF
    JOURNAL OF CATALYSIS, 1981, 69 (01) : 32 - 43
  • [2] Fischer-Tropsch Synthesis: Effects of Hydrohalic Acids in Syngas on a Precipitated Iron Catalyst
    Ma, Wenping
    Jacobs, Gary
    Thomas, Gerald A.
    Shafer, Wilson D.
    Sparks, Dennis E.
    Hamdeh, Hussein H.
    Davis, Burton H.
    ACS CATALYSIS, 2015, 5 (05): : 3124 - 3136
  • [3] PRECIPITATED IRON CATALYSTS FOR FISCHER-TROPSCH SYNTHESIS
    HAMMER, H
    BITTNER, D
    ERDOL & KOHLE ERDGAS PETROCHEMIE, 1978, 31 (08): : 369 - 369
  • [4] Effect of Hydrothermal Treatment on Precipitated Iron Catalyst for Fischer-Tropsch Synthesis
    Ma, Cailian
    Chen, Jiangang
    CATALYSIS LETTERS, 2015, 145 (02) : 702 - 711
  • [5] Effect of H2S in syngas on the Fischer-Tropsch synthesis performance of a precipitated iron catalyst
    Ma, Wenping
    Jacob, Gary
    Sparks, Dennis E.
    Shafer, Wilson D.
    Hamdeh, Hussein H.
    Hopps, Shelley D.
    Pendyala, Venkat Ramana Rao
    Hu, Yongfeng
    Xiao, Qunfeng
    Davis, Burtron H.
    APPLIED CATALYSIS A-GENERAL, 2016, 513 : 127 - 137
  • [6] Detailed kinetics of Fischer-Tropsch synthesis on a precipitated iron catalyst
    Pour, Ali Nakhaei
    Khodabandeh, Hamideh
    Izadyar, Mohammad
    Housaindokht, Mohammad Reza
    REACTION KINETICS MECHANISMS AND CATALYSIS, 2014, 111 (01) : 29 - 44
  • [7] KINETICS OF FISCHER-TROPSCH SYNTHESIS OVER PRECIPITATED IRON CATALYST
    SHEN Wen-Jie ZHOU Jing-Lai ZHANG Bi-JiangInstitute of Coal Chemistry
    Journal of Natural Gas Chemistry, 1994, (04) : 385 - 400
  • [8] Preparation of a new precipitated iron catalyst for Fischer-Tropsch synthesis
    Hayakawa, Hiroshi
    Tanaka, Hisanori
    Fujimoto, Kaoru
    CATALYSIS COMMUNICATIONS, 2007, 8 (11) : 1820 - 1824
  • [9] CHARACTERIZATION OF A PROMOTED PRECIPITATED IRON CATALYST FOR FISCHER-TROPSCH SYNTHESIS
    LOX, ES
    MARIN, GB
    DEGRAVE, E
    BUSSIERE, P
    APPLIED CATALYSIS, 1988, 40 (1-2): : 197 - 218
  • [10] POISONING OF IRON CATALYST BY COS IN SYNGAS FOR FISCHER-TROPSCH SYNTHESIS
    LIU, ZT
    ZHOU, JL
    ZHANG, BJ
    JOURNAL OF MOLECULAR CATALYSIS, 1994, 94 (02): : 255 - 261