Fracture strength of flawed cylindrical pressure vessels under cryogenic temperatures

被引:6
|
作者
Christopher, T
Sankarnarayanasamy, K
Rao, BN [1 ]
机构
[1] Vikram Sarabhai Space Ctr, Struct Engn Grp, Propellants & Special Chem Grp, Trivandrum 695022, Kerala, India
[2] Alagappa Chettiar Coll Engn & Technol, Fac Mech Engn, Karaikkudi 630004, Tamil Nadu, India
[3] Reg Engn Coll, Fac Mech Engn, Tiruchirappalli 620015, Tamil Nadu, India
关键词
failure pressure; aluminium; titanium; steels; cylindrical vessels; through-wall cracks; surface cracks; elastic stress intensity factor; failure assessment diagram;
D O I
10.1016/S0011-2275(02)00114-5
中图分类号
O414.1 [热力学];
学科分类号
摘要
Damage tolerant and fail-safe approaches have been employed increasingly in the design of critical engineering components. In these approaches, one has to assess the residual strength of a component with an assumed pre-existing crack. In other cases, cracks may be detected during service. Then, there is a need to evaluate the residual strength of the cracked components in order to decide whether they can be continued safely or repair and replacement are imperative. A three-parameter fracture criterion is applied to correlate the fracture data on aluminium, titanium and steel materials from test results on cylindrical tanks/pressure vessels at cryogenic temperatures. Fracture parameters to generate the failure assessment diagram are determined for the materials considered in the present study. Failure pressure estimates were found to be in good agreement with test results. (C) 2003 Elsevier Science Ltd. All rights reserved.