摘要
A continuous S2 silicide ([TiZr](x)S-y) segregation layer was found in the fibre matrix interface of SCS6-SiC/Ti-5.8Al-4Sn-3.5Zr-0.7Nb-0.5Mo-0.35Si (IMI834) composites (composition in wt.%). The S2 layer separates completely the titanium matrix from the reaction layer. It was shown that the S2 layer stabilises the interface during thermal treatment. The thermal stability of composites was tested in which artificial coatings were introduced into the interface. For the artificial coatings a composition and structure of the S2 silicides were aspired. The interface of the composites was investigated with analytical transmission electron microscope in the as-processed condition and annealed at 700 degreesC for 3 000 h and at 800 degreesC for 1000 h. The coatings of the same composition and structure can be introduced into the interface of SiC-SCS6/IMI834 composites as those of the S2 silicide obtained by self-segregation. The composites with the artificial coatings have a similar interface stability at 700 degreesC as those obtained by self-segregation.
引用
收藏
页码:1172 / 1176
页数:5
相关论文
共 50 条
  • [1] Graded titanium boride fibre protective coatings for titanium matrix composites
    Dudek, HJ
    Werner, A
    Leucht, R
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 212 (02): : 242 - 246
  • [2] HIGH-TEMPERATURE OXIDATION OF TITANIUM SILICIDE COATINGS ON TITANIUM
    ABBA, A
    GALERIE, A
    CAILLET, M
    OXIDATION OF METALS, 1982, 17 (1-2): : 43 - 54
  • [3] Dynamic recrystallization and silicide precipitation behavior of titanium matrix composites under different strains
    ZHAO E.-T.
    SUN S.-C.
    YU J.-R.
    AN Y.-K.
    CHEN W.-Z.
    CHEN R.-R.
    Transactions of Nonferrous Metals Society of China (English Edition), 2021, 31 (11): : 3416 - 3427
  • [4] MICROINDENTATION CHARACTERIZATION OF SILICIDE COATINGS ON NIOBIUM AND TITANIUM
    GUILLE, J
    MATINI, L
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1988, 7 (09) : 952 - 954
  • [5] BARRIER HEIGHT OF TITANIUM SILICIDE SCHOTTKY-BARRIER DIODES
    KIKUCHI, A
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS, 1986, 25 (11): : L894 - L895
  • [6] Dynamic recrystallization and silicide precipitation behavior of titanium matrix composites under different strains
    Zhao, Er-tuan
    Sun, Shi-chen
    Yu, Jin-rui
    An, Yu-kun
    Chen, Wen-zhen
    Chen, Rui-run
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2021, 31 (11) : 3416 - 3427
  • [7] Carbon-fibre titanium Silicide interphase titanium-matrix composites: Fabrication, structure and mechanical properties
    Mileiko, ST
    Rudnev, AM
    Gelachov, MV
    COMPOSITES SCIENCE AND TECHNOLOGY, 1995, 55 (03) : 255 - 260
  • [8] Improved properties of silicide matrix composites
    Augustin, S.
    Broglio, M.
    Lipetzky, P.
    Stoloff, N.S.
    Nazmy, M.
    Ceramic Engineering and Science Proceedings, 1997, 18 (4 B): : 339 - 346
  • [9] Molybdenum and titanium silicide based composites and alloys
    Mitra, R
    Prasad, NE
    Rao, AV
    Mahajan, YR
    STRUCTURAL INTERMETALLICS 1997, 1996, : 959 - 968
  • [10] Research Progress in Environmental Barrier Coatings of SiC Ceramic Matrix Composites
    Liu Qiao-mu
    Huang Shun-zhou
    He Ai-jie
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2018, 46 (10): : 1 - 8