Formation Mechanism of Type IV Failure in High Cr Ferritic Heat-Resistant Steel-Welded Joint

被引:62
|
作者
Liu, Y. [1 ]
Tsukamoto, S. [1 ]
Shirane, T.
Abe, F. [1 ]
机构
[1] Natl Inst Mat Sci, Struct Mat Ctr, Tsukuba, Ibaraki 3050047, Japan
关键词
CREEP STRENGTH; AFFECTED ZONE; CRACKING; MICROSTRUCTURE; SUPPRESSION; FRACTURE;
D O I
10.1007/s11661-013-1801-0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The mechanism of type IV failure has been investigated by using a conventional 9Cr ferritic heat-resistant steel Gr.92. In order to clarify the main cause of type IV failure, different heat treatments were performed on the base metal in order to change the prior austenite grain (PAG) size and precipitate distribution after applying the heat-affected zone (HAZ) simulated thermal cycle at the peak temperature of around A (c3) (A (c3) HAZ thermal cycle) and postweld heat treatment (PWHT). The microstructural evolution during the A (c3) HAZ thermal cycle and PWHT was investigated by means of scanning electron microscope (SEM), electron backscatter diffraction (EBSD), electron probe microanalysis (EPMA), and transmission electron microscope (TEM). It was found that M23C6 carbides were scarcely precipitated at the newly formed fine PAG, block, and lath boundaries in A (c3) HAZ-simulated Gr.92, because the carbide forming elements such as Cr and C were segregated at the former PAG and block boundaries of the base metal. On the other hand, if all the boundaries were covered by sufficient M23C6 carbides by homogenization of the alloying elements prior to applying the HAZ thermal cycle, the creep strength was much improved even if the fine PAG was formed. From these results, it is concluded that fine-grained microstructure cannot account for the occurrence of type IV failure, and it only has a small effect during long-term creep. The most important factor is the precipitate formation behavior at various boundaries. Without sufficient boundary strengthening by precipitates, the microstructure of A (c3) HAZ undergoes severe changes even during PWHT and causes premature failure during creep. (C) The Minerals, Metals & Materials Society and ASM International 2013
引用
收藏
页码:4626 / 4633
页数:8
相关论文
共 50 条
  • [1] Formation Mechanism of Type IV Failure in High Cr Ferritic Heat-Resistant Steel-Welded Joint
    Y. Liu
    S. Tsukamoto
    T. Shirane
    F. Abe
    [J]. Metallurgical and Materials Transactions A, 2013, 44 : 4626 - 4633
  • [2] Prevention of Type IV Failure in High Cr Ferritic Heat Resistant Steel Welded Joint
    Tsukamoto, S.
    Tabuch, M.
    Shirane, T.
    Abe, F.
    [J]. TRENDS IN WELDING RESEARCH, 2009, : 296 - 302
  • [3] Role of Boundary Strengthening on Prevention of Type IV Failure in High Cr Ferritic Heat-Resistant Steels
    Liu, Yuan
    Tsukamoto, Susumu
    Sawada, Kota
    Abe, Fujio
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2014, 45A (03): : 1306 - 1314
  • [4] Role of Boundary Strengthening on Prevention of Type IV Failure in High Cr Ferritic Heat-Resistant Steels
    Yuan Liu
    Susumu Tsukamoto
    Kota Sawada
    Fujio Abe
    [J]. Metallurgical and Materials Transactions A, 2014, 45 : 1306 - 1314
  • [5] Formation and evolution of precipitates in high Cr ferritic heat-resistant steels
    Zhou, X. S.
    Liu, Y. C.
    Liu, C. X.
    Yu, L. M.
    Li, H. J.
    [J]. MATERIALS RESEARCH INNOVATIONS, 2015, 19 : S193 - S198
  • [6] The isochronal δ → γ transformation of high Cr ferritic heat-resistant steel during cooling
    Gao, Qiuzhi
    Liu, Yongchang
    Di, Xinjie
    Dong, Zhizhong
    Yan, Zesheng
    [J]. JOURNAL OF MATERIALS SCIENCE, 2011, 46 (21) : 6910 - 6915
  • [7] Kinetics of isochronal austenization in modified high Cr ferritic heat-resistant steel
    Liu, Chenxi
    Liu, Yongchang
    Zhang, Dantian
    Yan, Zesheng
    [J]. APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2011, 105 (04): : 949 - 957
  • [8] Kinetics of isochronal austenization in modified high Cr ferritic heat-resistant steel
    Chenxi Liu
    Yongchang Liu
    Dantian Zhang
    Zesheng Yan
    [J]. Applied Physics A, 2011, 105 : 949 - 957
  • [9] The isochronal δ → γ transformation of high Cr ferritic heat-resistant steel during cooling
    Qiuzhi Gao
    Yongchang Liu
    Xinjie Di
    Zhizhong Dong
    Zesheng Yan
    [J]. Journal of Materials Science, 2011, 46 : 6910 - 6915
  • [10] Identification and formation mechanism of a deformation process determining microstructure of type IV creep damage of the advanced high Cr containing ferritic heat resistant steel
    Hasegawa, Yasushi
    Muraki, Tarou
    Ohgami, Masahiro
    [J]. TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2006, 92 (10): : 609 - 617