Crystallography of the High-Temperature Ca2SiO4-Ca3P2O8Solid Solutions

被引:9
|
作者
Yu, Huafang [1 ]
Miki, Takahiro [1 ]
Sasaki, Yasushi [1 ]
Nagasaka, Tetsuya [1 ]
机构
[1] Tohoku Univ, Grad Sch Engn, Sendai, Miyagi 9808579, Japan
关键词
DI-CALCIUM SILICATE; MAGNETIC SEPARATION; STEELMAKING SLAG; PHOSPHORUS; PHASE; DEPHOSPHORIZATION; RECOVERY; PHOSPHATE; P2O5;
D O I
10.1007/s11663-020-01945-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The crystallography of the Ca2SiO4-Ca(3)P(2)O(8)solid solutions in the dephosphorization slag in current steelmaking process was determined in this study. Understanding the physical and chemical properties of these Ca2SiO4-Ca(3)P(2)O(8)solid solutions is a preliminary step towards understanding the role of the Ca2SiO4-Ca(3)P(2)O(8)solid solutions in the dephosphorization process. The range of Ca(3)P(2)O(8)in the Ca2SiO4-Ca(3)P(2)O(8)solid solutions synthesized for analysis varied from 10 to 90 mol pct, with an incremental increase of 10 mol pct per solid solution. In solid solutions with a Ca(3)P(2)O(8)content of up to 40 mol pct, the crystal structure at 1773 K was found to be hexagonal, while the solid solutions with a Ca(3)P(2)O(8)content over 70 mol pct had a trigonal structure. The silicocarnotite solid solutions observed when the Ca(3)P(2)O(8)content was 50 to 60 mol pct were likely formed by phase transformation during cooling. In the stable solid solution with a Ca(3)P(2)O(8)content of 50 to 60 mol pct at 1773 K before the occurrence of transformation, the crystal structure is trigonal since it is in the Ca3P2O8-rich range. A linear increase in the lattice parameterscof the solid solutions in the range of (0, 40 mol pct) and (70 mol pct, 100 mol pct) was found with increasing Ca(3)P(2)O(8)content. The lattice parametera, however, was almost independent of the Ca(3)P(2)O(8)content in the solid solutions.
引用
收藏
页码:3007 / 3015
页数:9
相关论文
共 50 条
  • [1] Crystallography of the High-Temperature Ca2SiO4-Ca3P2O8 Solid Solutions
    Huafang Yu
    Takahiro Miki
    Yasushi Sasaki
    Tetsuya Nagasaka
    Metallurgical and Materials Transactions B, 2020, 51 : 3007 - 3015
  • [2] HIGH-TEMPERATURE EQUILIBRIUM REDUCTION WITH ALUMINUM OF CA3P2O8, CA2NB2O7 AND FE2SIO4 MIXTURES
    VATOLIN, NA
    MOISEYEV, GK
    RUSSIAN METALLURGY, 1980, (06): : 40 - 45
  • [3] Phosphorous Recovery from Ca2SiO4-Ca3P2O8 Solid Solution By Carbothermic Reduction
    Yu, Huafang
    Lu, Xin
    Miki, Takahiro
    Sasaki, Yasushi
    Nagasaka, Tetsuya
    JOURNAL OF SUSTAINABLE METALLURGY, 2021, 7 (02) : 459 - 469
  • [4] Activities of FexO in Molten Slags Coexisting with Solid CaO and Ca2SiO4-Ca3P2O8 Solid Solution
    Miwa, Kohei
    Matsugi, Ryota
    Hasegawa, Masakatsu
    ISIJ INTERNATIONAL, 2017, 57 (10) : 1725 - 1732
  • [5] Solubility and Activity of Iron Oxide in Solid Solutions between Ca2SiO4 and Ca3P2O8 at 1 573 K
    Saito, Keijiro
    Kashiwaya, Yoshiaki
    Hasegawa, Masakatsu
    ISIJ INTERNATIONAL, 2023, 63 (04) : 631 - 638
  • [6] Phosphorous Recovery from Ca2SiO4–Ca3P2O8 Solid Solution By Carbothermic Reduction
    Huafang Yu
    Xin Lu
    Takahiro Miki
    Yasushi Sasaki
    Tetsuya Nagasaka
    Journal of Sustainable Metallurgy, 2021, 7 : 459 - 469
  • [7] Modification of the Activities of Components in Ca2SiO4-Ca3P2O8 Solid Solution at 1 573 K
    Saito, Keijiro
    Hasegawa, Masakatsu
    ISIJ INTERNATIONAL, 2024, 64 (15) : 2149 - 2155
  • [8] Activities of FexO in Molten Slags Coexisting with Solid CaO and Ca2SiO4-Ca3 P2O8 Solid Solution
    Miwa, Kohei
    Matsugi, Ryota
    Hasegawa, Masakatsu
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2019, 105 (06): : 587 - 594
  • [9] CA-2O.SIO2 SOLID SOLUTIONS WITH METAL OXIDES
    EREMIN, NI
    EGEREVA, AI
    DMITRIEV.AM
    FIRFAROV.IB
    ZHURNAL PRIKLADNOI KHIMII, 1970, 43 (01) : 18 - &
  • [10] Lattice vibrations in the HgBa2Ca2Cu3O8 high-temperature superconductor
    Jha, Prafulla K.