摘要
The purpose of this study was to evaluate microstructural and crystallographic phase changes after grinding 3Y-TZP dental ceramics. Ceramic blanks were sintered according to manufacturer's recommendations and divided into four groups: (A) as-sintered control, (B) diamond-ground manually under water, (C) ground and polished, and (D) ground and annealed at 1000 degrees C for 1 h. Bulk specimens were analyzed by X-ray diffraction to characterize the crystalline phases. The microstructure was investigated by SEM. XRD analyses showed that the control group and the group that was ground and annealed contained only tetragonal zirconia. However, after grinding or after grinding followed by polishing, rhombohedral zirconia and strained tetragonal zirconia were present, without any detectable amount of monoclinic zirconia. Annealing led to the disappearance of both residual lattice strain and the rhombohedral phase. The microstructure of the ground and polished specimens was characterized by significant residual surface damage associated with grain pullout to a depth of about 20 gm. This type of damage could have an impact on the long-term fatigue behavior of 3Y-TZP.
引用
收藏
页码:440 / 448
页数:9
相关论文
共 50 条
  • [1] Laser surface texturing of zirconia-based ceramics for dental applications: A review
    Han, Jide
    Zhang, Fei
    Van Meerbeek, Bart
    Vleugels, Jozef
    Braem, Annabel
    Castagne, Sylvie
    MATERIALS SCIENCE AND ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2021, 123
  • [2] Depth-of-cut errors in ELID surface grinding of zirconia-based ceramics
    Tang, H.
    Deng, Z. H.
    Guo, Y. S.
    Qian, J.
    Reynaerts, D.
    INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2015, 88 : 34 - 41
  • [3] Y-TZP zirconia regeneration firing: Microstructural and crystallographic changes after grinding
    Obelenis Ryan, Daniel Patrick
    Grassi Fais, Laiza Maria
    Antonio, Selma Gutierrez
    Hatanaka, Gabriel Rodrigues
    Candido, Lucas Miguel
    Pereira Pinelli, Ligia Antunes
    DENTAL MATERIALS JOURNAL, 2017, 36 (04) : 447 - 453
  • [4] Contrast Ratio of Six Zirconia-Based Dental Ceramics
    Kanchanavasita, Widchaya
    Triwatana, Premwara
    Suputtamongkol, Kallaya
    Thanapitak, Alisa
    Chatchaiganan, Mathura
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2014, 23 (06): : 456 - 461
  • [5] Characterization of Zirconia-Based Ceramics After Microgrinding
    Fook, Pablo
    Riemer, Oltmann
    JOURNAL OF MICRO AND NANO-MANUFACTURING, 2019, 7 (02):
  • [6] Surface microstructural changes of spark plasma sintered zirconia after grinding and annealing
    Melk, Latifa
    Mouzon, Johanne
    Turon, Miguel
    Akhtar, Farid
    Antti, Marta-Lena
    Anglada, Marc
    CERAMICS INTERNATIONAL, 2016, 42 (14) : 15610 - 15617
  • [7] Surface wear structures and mechanisms in zirconia-based ceramics
    Savchenko, NL
    Kul'kov, SN
    TECHNICAL PHYSICS LETTERS, 2004, 30 (08) : 654 - 656
  • [8] Surface wear structures and mechanisms in zirconia-based ceramics
    N. L. Savchenko
    S. N. Kul’kov
    Technical Physics Letters, 2004, 30 : 654 - 656
  • [9] Superplasticity in zirconia-based ceramics
    Chokshi, AH
    SUPERPLASTICITY AND SUPERPLASTIC FORMING 1998, 1998, : 257 - 265
  • [10] The bending stress distribution in bilayered and graded zirconia-based dental ceramics
    Fabris, Douglas
    Souza, Julio C. M.
    Silva, Filipe S.
    Fredel, Marcio
    Mesquita-Guimaraes, Joana
    Zhang, Yu
    Henriques, Bruno
    CERAMICS INTERNATIONAL, 2016, 42 (09) : 11025 - 11031