Influence of accelerated aging on clay-reinforced polyamide 6

被引:59
|
作者
Kiliaris, P. [1 ]
Papaspyrides, C. D. [1 ]
Pfaendner, R. [2 ]
机构
[1] Natl Tech Univ Athens, Sch Chem Engn, Lab Polymer Technol, Athens 15780, Greece
[2] Ciba Lampertheim GmbH, D-68623 Lampertheim, Germany
关键词
Aging; Polyamides; Layered silicate nanocomposites; Thermo-oxidative degradation; LAYERED SILICATE NANOCOMPOSITES; MECHANICAL-PROPERTIES; THERMAL-DEGRADATION; RESTABILIZATION TECHNIQUE; NYLON-6; NANOCOMPOSITES; CRYSTALLIZATION BEHAVIOR; STABILIZATION; STABILITY;
D O I
10.1016/j.polymdegradstab.2008.11.016
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Organically modified clay-reinforced polyamide 6 was subjected to accelerated heat aging to estimate its long-term thermo-oxidative stability and useful lifetime compared to the virgin material. Changes in molecular weight, and thermal and mechanical properties were monitored and connected to the polymer modification encountered during aging. The incorporation of the clay filler was found to result in moderate polymer degradation during processing, which became more pronounced with aging time at elevated temperature, imparting discoloration. Post-crystallization was favoured by short periods of heat exposure, leading to an increase of crystalline content. Conversely, extended chain scission occurring after prolonged residence time negatively affected crystallites' size, lowering the degree of crystallinity. The aging-induced transformations of crystal structures correlated well with materials' mechanical performance, yielding initially hard and brittle specimens which gradually adopted a softening behavior. Relative to the unfilled polymer, the loss of ductility during aging was milder in the case of nano-composite, indicating that the clay filler restricted degradation, prolonging durability. (C) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:389 / 396
页数:8
相关论文
共 50 条
  • [1] Clay-reinforced polyamide:: Influence of the nanofillers dispersion.
    Reynaud, E
    Klopffer, MH
    Cavaillé, JY
    Gauthier, C
    Varlet, J
    Vigier, G
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2000, 219 : U480 - U480
  • [2] Mechanical properties of clay-reinforced polyamide
    Masenelli-Varlot, K
    Reynaud, E
    Vigier, G
    Varlet, J
    JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 2002, 40 (03) : 272 - 283
  • [3] Selective Laser Sintering of Clay-Reinforced Polyamide
    Jain, Prashant K.
    Pandey, Pulak M.
    Rao, P. V. M.
    POLYMER COMPOSITES, 2010, 31 (04) : 732 - 743
  • [4] Clay-reinforced polyamide: Preferential orientation of the montmorillonite sheets and the polyamide crystalline lamellae
    Varlot, K
    Reynaud, E
    Kloppfer, MH
    Vigier, G
    Varlet, J
    JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 2001, 39 (12) : 1360 - 1370
  • [5] Infrared spectroscopy studies of structure and orientation in clay-reinforced polyamide-6 nanocomposites
    Cole, KC
    Denault, J
    Bureau, MN
    MACROMOLECULAR SYMPOSIA, 2004, 205 : 47 - 60
  • [6] CLAY-REINFORCED EPOXY NANOCOMPOSITES
    LAN, T
    PINNAVAIA, TJ
    CHEMISTRY OF MATERIALS, 1994, 6 (12) : 2216 - 2219
  • [7] Mechanical Properties of Clay-Reinforced Polyamide 6 Nanocomposite Liner Materials of Type IV Hydrogen Storage Vessels
    Kis, David Istvan
    Bata, Attila
    Takacs, Janos
    Kokai, Eszter
    NANOMATERIALS, 2024, 14 (17)
  • [8] Clay-reinforced epoxy nanocomposites
    Ratna, D
    Manoj, NR
    Varley, R
    Raman, RKS
    Simon, GP
    POLYMER INTERNATIONAL, 2003, 52 (09) : 1403 - 1407
  • [9] Clay-reinforced PVC composites and nanocomposites
    Boraei, Seyyed Behnam Abdollahi
    Bakhshandeh, Behnaz
    Mohammadzadeh, Fatemeh
    Haghighi, Dorrin Mohtadi
    Mohammadpour, Zahra
    HELIYON, 2024, 10 (07)
  • [10] New clay-reinforced polyamide nanocomposite based on 4-phenylenediacrylic acid: Synthesis and properties
    Faghihi, Khalil
    Abootalebi, Ashraf Sadat
    Shabanian, Meisam
    JOURNAL OF SAUDI CHEMICAL SOCIETY, 2013, 17 (02) : 191 - 197