A comparison of the hot-compaction behavior of oriented, high-modulus, polyethylene fibers and tapes

被引:59
|
作者
Hine, PJ
Ward, IM [1 ]
Jordan, ND
Olley, RH
Bassett, DC
机构
[1] Univ Leeds, Dept Phys & Astron, IRC Polymer Sci & Technol, Leeds LS2 9JT, W Yorkshire, England
[2] Univ Reading, Dept Phys, Reading RG6 6AF, Berks, England
来源
关键词
D O I
10.1081/MB-100107570
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The purpose of this article is twofold. First, there is an account of the hot-compaction behavior of a new, Highly oriented, high-modulus polyethylene (PE) tape with the trade name of Tensylon(R) (manufactured by Synthetic Industries, USA). This tape, produced by a melt spinning route, has mechanical properties comparable to those of commercially available gel-spun fibers. Unidirectional samples were produced for a range of compaction temperatures to determine the optimum compaction conditions to obtain the best mechanical properties of the resulting compacted sheets. Second, the mechanical properties of the best Tensylon sample, manufactured at a compaction temperature of 153 degreesC, was compared with three other hot-compacted, highly oriented PE materials, based on Certran(R), Dyneema(R), and Spectra(R) commercial PE fibers. The results showed that the optimum compaction temperature was in most cases about 1 degreesC below the point at which substantial crystalline melting occurred. At this optimum temperature, differential scanning calorimetry (DSC) melting studies showed that approximately 30% of the original oriented phase had been lost to bond the structure together. In the case of Dyneema, the properties of the fiber were not translated into the properties of a compacted sheet, and morphological studies showed that this was because melting did not occur on the fiber surfaces, but rather in the interior of the fiber due to a skin structure. The properties of the compacted Tensylon tapes were found to be exceptional, combining very high modulus and strength with interlayer bonding and good creep resistance. Moreover, the optimum temperature appeared to be about 2 degreesC below the point at which complete melting occurred, giving a wider processing window for this material.
引用
收藏
页码:959 / 989
页数:31
相关论文
共 50 条
  • [1] The development of morphology during hot compaction of Tensylon high-modulus polyethylene tapes and woven cloths
    Jordan, ND
    Olley, RH
    Bassett, DC
    Hine, PJ
    Ward, IM
    [J]. POLYMER, 2002, 43 (12) : 3397 - 3404
  • [2] ACHIEVEMENT OF HIGH-MODULUS POLYETHYLENE FIBERS AND THE MODULUS OF POLYETHYLENE CRYSTALS
    BARHAM, PJ
    KELLER, A
    [J]. JOURNAL OF POLYMER SCIENCE PART C-POLYMER LETTERS, 1979, 17 (09) : 591 - 593
  • [3] HOT-COMPACTION BEHAVIOR OF COALS
    CHOW, C
    CHAKLADER, ACD
    WARREN, IH
    LEEDER, WR
    [J]. FUEL, 1980, 59 (01) : 27 - 34
  • [4] THE HOT COMPACTION OF HIGH MODULUS MELT-SPUN POLYETHYLENE FIBERS
    HINE, PJ
    WARD, IM
    OLLEY, RH
    BASSETT, DC
    [J]. JOURNAL OF MATERIALS SCIENCE, 1993, 28 (02) : 316 - 324
  • [5] A MODEL FOR THE CREEP OF ORIENTED HIGH-MODULUS FIBERS
    SCHUPPERT, AA
    [J]. MAKROMOLEKULARE CHEMIE-THEORY AND SIMULATIONS, 1993, 2 (05): : 643 - 651
  • [6] COMPACTION OF HIGH-MODULUS MELT-SPUN POLYETHYLENE FIBERS AT TEMPERATURES ABOVE AND BELOW THE OPTIMUM
    KABEEL, MA
    BASSETT, DC
    OLLEY, RH
    HINE, PJ
    WARD, IM
    [J]. JOURNAL OF MATERIALS SCIENCE, 1994, 29 (18) : 4694 - 4699
  • [7] On the gauche bond content in high-modulus polyethylene fibers
    Meier, RJ
    [J]. SOFT MATERIALS, 2005, 3 (01) : 45 - 49
  • [8] SCANNING FORCE MICROSCOPY OF HIGH-MODULUS POLYETHYLENE FIBERS
    WAWKUSCHEWSKI, A
    CANTOW, HJ
    MAGONOV, SN
    HEWES, JD
    KOCUR, MA
    [J]. ACTA POLYMERICA, 1995, 46 (02) : 168 - 177
  • [9] STUDY ON ACHIEVEMENT OF HIGH-MODULUS POLYETHYLENE FIBERS BY DRAWING
    BARHAM, PJ
    KELLER, A
    [J]. JOURNAL OF MATERIALS SCIENCE, 1976, 11 (01) : 27 - 35
  • [10] THE DETECTION OF RADICALS IN STRAINED, HIGH-MODULUS POLYETHYLENE FIBERS
    WANG, DM
    KLAASSEN, AAK
    JANSSEN, GE
    DEBOER, E
    MEIER, RJ
    [J]. POLYMER, 1995, 36 (22) : 4193 - 4196