Microstructure and Texture Evolution in a Yttrium-Containing ZM31 Alloy: Effect of Pre- and Post-deformation Annealing

被引:3
|
作者
Tahreen, N. [1 ]
Zhang, D. F. [2 ,3 ]
Pan, F. S. [2 ,3 ,4 ]
Jiang, X. Q. [5 ,6 ]
Li, D. Y. [7 ]
Chen, D. L. [1 ]
机构
[1] Ryerson Univ, Dept Mech & Ind Engn, Toronto, ON M5B 2K3, Canada
[2] Chongqing Univ, Coll Mat Sci & Engn, Chongqing 400045, Peoples R China
[3] Chongqing Univ, Natl Engn Res Ctr Magnesium Alloys, Chongqing 400044, Peoples R China
[4] Chongqing Acad Sci & Technol, Chongqing 401123, Peoples R China
[5] Chongqing Acad Sci & Technol, Adv Mat Res Ctr, Chongqing 401123, Peoples R China
[6] Southwest Univ, Fac Mat & Energy, Adv Mat Res Ctr, Chongqing 400715, Peoples R China
[7] Univ Alberta, Dept Chem & Mat Engn, Edmonton, AB T6G 2V4, Canada
基金
加拿大创新基金会; 加拿大自然科学与工程研究理事会; 中国国家自然科学基金;
关键词
AZ31 MAGNESIUM ALLOY; MN-Y ALLOY; HOT DEFORMATION; RARE-EARTH; HARDENING BEHAVIOR; TENSILE DUCTILITY; MG; STRAIN; BOUNDARIES; ANISOTROPY;
D O I
10.1007/s11663-015-0544-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Microstructure and texture evolution of as-extruded ZM31 magnesium alloys with different amounts of yttrium (Y) during pre- and post-deformation annealing were examined with special attention given to the effect of Y on recrystallization. It was observed that the extruded ZM31 alloys exhibited a basal texture with the basal planes parallel to the extrusion direction (ED). The compression of the extruded alloys in the ED to a strain amount of 10 pct resulted in c-axes of hcp unit cells rotating toward the anti-compression direction due to the occurrence of extension twinning. Annealing of the extruded alloys altered the microstructure and texture, and the subsequent compression after annealing showed a relatively weak texture and a lower degree of twinning. A reverse procedure of pre-compression and subsequent annealing was found to further weaken the texture with a more scattered distribution of orientations and to lead to the vanishing of the original basal texture. With increasing Y content, both the extent of extension twinning during compression and the fraction of recrystallization during annealing decreased due to the role of Y present in the substitutional solid solution and in the second-phase particles, leading to a significant increase in the compressive yield strength. (C) The Minerals, Metals & Materials Society and ASM International 2015
引用
收藏
页码:3318 / 3325
页数:8
相关论文
共 50 条
  • [1] Microstructure and Texture Evolution in a Yttrium-Containing ZM31 Alloy: Effect of Pre- and Post-deformation Annealing
    N. Tahreen
    D. F. Zhang
    F. S. Pan
    X. Q. Jiang
    D. Y. Li
    D. L. Chen
    Metallurgical and Materials Transactions B, 2016, 47 : 3318 - 3325
  • [2] Effect of Y Addition on the Microstructure and Mechanical Properties of ZM31 Alloy
    Ye, Xue
    Cao, Hongshuai
    Qi, Fugang
    Ouyang, Xiaoping
    Ye, Zhisong
    Hou, Caihong
    Li, Lianhui
    Zhang, Dingfei
    Zhao, Nie
    MATERIALS, 2020, 13 (03)
  • [3] Effect of pre-deformation on microstructure characteristics, texture evolution and deformation mechanism of AZ31 magnesium alloy
    Li, Yuyu
    Yang, Bowen
    Han, Tingzhuang
    Chu, Zhibing
    Tuo, Leifeng
    Xue, Chun
    Yang, Qianhua
    Zhao, Xiaodong
    Gao, Hong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 845
  • [4] Evolution of microstructure, mechanical and functional properties in cold-rolled TiNiCuNb alloy after post-deformation annealing
    Zhou, X. J.
    Shuitcev, A. V.
    Huang, Z. . H.
    Chen, F.
    Tong, Y. X.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 923
  • [5] Texture evolution during equal channel angular extrusion (ECAE) - Part II. An effect of post-deformation annealing
    Ferrasse, S
    Segal, VM
    Alford, F
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 372 (1-2): : 235 - 244
  • [6] Effect of Post-Deformation Heat Treatment on the Microstructure and Properties of Inconel 617 Alloy
    Ji, Jinjin
    Jia, Zhi
    Yang, Peiyao
    Wang, Yanjiang
    Kou, Shengzhong
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2024, 77 (09) : 2479 - 2487
  • [7] Texture evolution and deformation activity of an extruded magnesium alloy: Effect of yttrium and deformation temperature
    Tahreen, N.
    Zhang, D. F.
    Pan, F. S.
    Jiang, X. Q.
    Li, D. Y.
    Chen, D. L.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 688 : 270 - 284
  • [8] Tracking microstructure, texture and boundary misorientation evolution of hot deformed and post-deformation annealed Ti-6Al-4V alloy
    Lim, S. C. V.
    Yang, K. V.
    Yang, Y.
    Cheng, Y.
    Huang, A.
    Wu, X.
    Davies, C. H. J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 651 : 524 - 534
  • [9] Mechanisms for influence of post-deformation annealing on microstructure of NiTiFe shape memory alloy processed by local canning compression
    Zhang, Yanqiu
    Jiang, Shuyong
    Tang, Ming
    Yan, Bingyao
    Yu, Junbo
    Zhao, Chengzhi
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2021, 291
  • [10] Effect of Cu on Amorphization of a TiNi Alloy during HPT and Shape Memory Effect after Post-Deformation Annealing
    Shahmir, Hamed
    Nili-Ahmadabadi, Mahmoud
    Mohammadi, Mahdi
    Huang, Yi
    Andrzejczuk, Mariusz
    Lewandowska, Malgorzata
    Langdon, Terence G.
    ADVANCED ENGINEERING MATERIALS, 2020, 22 (01)