Epitaxial growth of Ni films sputter-deposited on a GaAs(001) surface covered with a MgO film

被引:0
|
作者
Makihara, Kenji [1 ]
Maruyama, Susumu [1 ]
Zota, Yasutami [1 ]
Hashimoto, Mituru [2 ]
Shi, Ji [3 ]
机构
[1] Tokyo Univ Technol, Nanotechnol Ctr, Katayanagi Adv Res Lab, Hachioji, Tokyo 1920982, Japan
[2] Japan Physitech Co, Tokyo 1820046, Japan
[3] Tokyo Inst Technol, Fac Engn, Meguro Ku, Tokyo 2268552, Japan
关键词
Epitaxial; Thickness; Annealing; Nickel; Magnesium oxide; Gallium arsenide (001); X-ray diffraction; Electron microscopy; FE;
D O I
10.1016/j.tsf.2012.07.095
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
We studied the epitaxial growth of a Ni film prepared on a GaAs(001) substrate covered with a thin epitaxial MgO buffer film, assuming that this buffer film plays a key role in the epitaxial growth of the Ni film. The MgO and Ni films were deposited by radio-frequency magnetron sputtering of the MgO and Ni targets in pure Ar gas. First, a MgO film of thickness ranging from 78 to 4.4 nm was deposited on the GaAs(001) substrate at a temperature ranging from ambient temperature to 700 degrees C, and then, a 136-nm-thick Ni film was deposited on the MgO/GaAs substrate at a temperature range 300-500 degrees C. Using transmission electron microscopy and X-ray diffractometry, we showed that the MgO film grows with the epitaxial relationship MgO(001) [001]//GaAs(001)[001] on GaAs(001) at 500 degrees C, and that the structure of the Ni film depends on three factors: the MgO/GaAs substrate temperature, the MgO thickness, and the annealing condition of the MgO/GaAs substrate before the Ni deposition. In conclusion, we proved that the Ni film grows with the epitaxial relationship Ni(001)[001]//MgO(001)[001]//GaAs(001)[001] on MgO/GaAs with the 4.4-nm-thick MgO film when the MgO/GaAs substrate is annealed in situ at room temperature before the Ni deposition and maintained at 300 degrees C during the Ni deposition. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:6831 / 6835
页数:5
相关论文
共 50 条
  • [1] Growth and structure of Ni films radio frequency sputter deposited on GaAs(001) covered with Ti film
    Makihara, K
    Yang, JP
    Shi, J
    Hashimoto, M
    Maruyama, S
    Barna, A
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 2001, 19 (05): : 2494 - 2498
  • [2] FERROMAGNETIC-RESONANCE IN NI FILMS BIASED DC SPUTTER-DEPOSITED ON MGO(001)
    MARUYAMA, H
    QIU, H
    NAKAI, H
    HASHIMOTO, M
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1995, 13 (04): : 2157 - 2160
  • [3] Growth of sputter-deposited metamagnetic epitaxial Ni-Co-Mn-In films
    Niemann, R. (r.niemann@ifw-dresden.de), 1600, American Institute of Physics Inc. (111):
  • [4] Growth of sputter-deposited metamagnetic epitaxial Ni-Co-Mn-In films
    Niemann, R.
    Schultz, L.
    Faehler, S.
    JOURNAL OF APPLIED PHYSICS, 2012, 111 (09)
  • [5] RBS ANALYSIS OF SPUTTER-DEPOSITED MGO FILMS
    VUORISTO, P
    MANTYLA, T
    KETTUNEN, P
    VACUUM, 1991, 42 (15) : 1001 - 1004
  • [6] The structure of sputter-deposited Co2MnSi thin films deposited on GaAs(001)
    Kohn, A.
    Lazarov, V. K.
    Singh, L. J.
    Barber, Z. H.
    Petford-Long, A. K.
    JOURNAL OF APPLIED PHYSICS, 2007, 101 (02)
  • [7] The structure of sputter-deposited Co2 MnSi thin films deposited on GaAs (001)
    Kohn, A.
    Lazarov, V.K.
    Singh, L.J.
    Barber, Z.H.
    Petford-Long, A.K.
    Journal of Applied Physics, 2007, 101 (02):
  • [8] Evolution of interface diffusion and structure of Ni films sputter-deposited on Si(001)
    Qiu, H
    Tian, Y
    Hashimoto, M
    VACUUM, 2003, 70 (04) : 493 - 497
  • [9] Surface growth and anomalous scaling of sputter-deposited Al films
    Fu, T.
    Shen, Y. G.
    PHYSICA B-CONDENSED MATTER, 2008, 403 (13-16) : 2306 - 2311
  • [10] Initial growth structure of Ni0.30Fe0.70 films dc-biased plasma-sputter-deposited on MgO(001), MgO(110), MgO(111) and on MgO(001) covered with Fe or Permalloy
    Yang, JP
    Amatatsu, Y
    Hashimoto, M
    Barna, A
    Barna, PB
    THIN SOLID FILMS, 2000, 371 (1-2) : 47 - 52