Carbide behaviour during high temperature low cycle fatigue in a cobalt-base superalloy

被引:37
|
作者
Jiang, WH
Yao, XD
Guan, HR
Hu, ZQ
机构
[1] Chinese Acad Sci, Dept 6, Met Res Inst, Shenyang 110015, Peoples R China
[2] Shenyang Polytech Univ, Dept Met Mat Engn, Shenyang 110023, Peoples R China
关键词
Fatigue; Carbide; Uniform Distribution; Fatigue Crack; Crack Initiation;
D O I
10.1023/A:1004683301816
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The carbide behaviour of a directionally solidified cobalt-base superalloy has been investigated after low cycle fatigue at 900 degrees C. During fatigue, primary carbides, M7C3 and MC, decomposed sluggishly and a great amount of secondary carbide, chromium-rich M23C6 precipitated. The inhomogeneous distribution of M23C6 brought about a different dislocation substructure. In the vicinity of the primary carbides, densely-distributed fine M23C6 pinned up dislocations effectively, resulting in a uniform distribution of dislocations, while in the interior of grains, since precipitates were coarse and scarce, dislocations were arranged in a planar array and piled up in the front of the precipitates. M23C6 also acted as an obstacle deflecting fatigue crack. Primary carbides on the surface of specimens were oxidizied preferentially, causing a precipitate depletion around them. The oxidized primary carbides were crack initiation sites. The primary carbides hindered fatigue crack propagation, causing the formation of shear steps. (C) 1999 Kluwer Academic Publishers.
引用
收藏
页码:2859 / 2864
页数:6
相关论文
共 50 条
  • [1] Carbide behaviour during high temperature low cycle fatigue in a cobalt-base superalloy
    W. H. Jiang
    X. D. Yao
    H. R. Guan
    Z. Q. Hu
    Journal of Materials Science, 1999, 34 : 2859 - 2864
  • [2] High temperature fatigue behaviour of a directionally solidified cobalt-base superalloy
    Jiang, W.H.
    Yao, X.D.
    Guan, H.R.
    Hu, Z.Q.
    Acta Metallurgica Sinica (English Letters), 1998, 11 (02): : 111 - 115
  • [3] HIGH TEMPERATURE FATIGUE BEHAVIOUR OF A DIRECTIONALLY SOLIDIFIED COBALT-BASE SUPERALLOY
    W.H.JIANG
    X.D.YAO
    H.R.GUAN
    Z.Q.HU
    ActaMetallurgicaSinica(EnglishLetters), 1998, (02) : 111 - 115
  • [4] On the low cycle fatigue deformation of K40S cobalt-base superalloy at elevated temperature
    Yang, FM
    Sun, XF
    Guan, HR
    Hu, ZQ
    MATERIALS LETTERS, 2003, 57 (19) : 2823 - 2828
  • [5] High-temperature low-cycle fatigue behavior of K40S cobalt-base superalloy
    F. M. Yang
    X. F. Sun
    H. R. Guan
    Z. Q. Hu
    Metallurgical and Materials Transactions A, 2003, 34 : 979 - 986
  • [6] High-temperature low-cycle fatigue behavior of K40S cobalt-base superalloy
    Yang, FM
    Sun, XF
    Guan, HR
    Hu, ZQ
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2003, 34A (04): : 979 - 986
  • [7] Low cycle fatigue behavior of K40S cobalt-base superalloy at elevated temperature - II. Fatigue fractography
    Yang, FM
    Sun, XF
    Guan, HR
    Hu, ZQ
    ACTA METALLURGICA SINICA, 2002, 38 (10) : 1053 - 1056
  • [8] THERMAL FATIGUE TESTING OF A COBALT-BASE SUPERALLOY SYSTEM
    PASKIET, GF
    BOONE, DH
    SULLIVAN, CP
    JOURNAL OF METALS, 1969, 21 (03): : A30 - &
  • [9] Secondary carbide precipitation in a directionally solidified cobalt-base superalloy
    Jiang, WH
    Yao, XD
    Guan, HR
    Hu, ZQ
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (03): : 513 - 520
  • [10] Secondary carbide precipitation in a directionally solified cobalt-base superalloy
    W. H. Jiang
    X. D. Yao
    H. R. Guan
    Z. Q. Hu
    W. H. Jiang
    Metallurgical and Materials Transactions A, 1999, 30 : 513 - 520