摘要
The influence of both solid KCl and solid K2CO3 on the oxidation behavior of a ferritic 10CrMo type steel and a nickel-based Alloy 625 type steel was investigated in the laboratory. Samples were exposed for a week at temperatures of 500 degrees C, 550 degrees C, and 600 degrees C. The role of water vapor was also studied by carrying out exposures under two different atmospheres: dry air, and air with a water content of 30%. Analyses were performed with SEM/EDXA to determine the extent of corrosion, the elemental distribution, and the identification of corrosion products. Both salts were found to be corrosive towards both steels, but the influence of KCl was significantly greater than that of K2CO3. In terms of durability. Alloy 625 exhibited higher corrosion resistance than 10CrMo. In the case of 10CrMo, the oxide formed always consisted of iron oxide with a chromium-rich region near the original steel surface. In the case of Alloy 625, the oxide consisted mainly of nickel oxide when it formed in the presence of KCl, and chromium oxide when it formed in the presence of K2CO3. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:253 / 264
页数:12
相关论文
共 50 条
  • [1] The Effects of KCl, K2SO4 and K2CO3 on the High Temperature Corrosion of a 304-Type Austenitic Stainless Steel
    Pettersson, Jesper
    Folkeson, Nicklas
    Johansson, Lars-Gunnar
    Svensson, Jan-Erik
    OXIDATION OF METALS, 2011, 76 (1-2): : 93 - 109
  • [2] The Effects of KCl, K2SO4 and K2CO3 on the High Temperature Corrosion of a 304-Type Austenitic Stainless Steel
    Jesper Pettersson
    Nicklas Folkeson
    Lars-Gunnar Johansson
    Jan-Erik Svensson
    Oxidation of Metals, 2011, 76 : 93 - 109
  • [3] The Effects of KCl, NaCl and K2CO3 on the High-Temperature Oxidation Onset of Sanicro 28 Steel
    Jingxin Sui
    Juho Lehmusto
    Mikael Bergelin
    Mikko Hupa
    Oxidation of Metals, 2016, 85 : 565 - 598
  • [4] The Effects of KCl, NaCl and K2CO3 on the High-Temperature Oxidation Onset of Sanicro 28 Steel
    Sui, Jingxin
    Lehmusto, Juho
    Bergelin, Mikael
    Hupa, Mikko
    OXIDATION OF METALS, 2016, 85 (5-6): : 565 - 598
  • [5] Temperature-Dependent Double-Step CO2 Occlusion of K2CO3 under Moist Conditions
    Chioyama, Hideyuki
    Luo, Hongchao
    Ohba, Tomonori
    Kanoh, Hirofumi
    ADSORPTION SCIENCE & TECHNOLOGY, 2015, 33 (03) : 243 - 250
  • [6] Kinetic Behavior of Solid K2CO3 under Postcombustion CO2 Capture Conditions
    Jayakumar, Abhimanyu
    Gomez, Arturo
    Mahinpey, Nader
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2017, 56 (04) : 853 - 863
  • [7] Solubility of CO2 in aqueous solutions of KCl and in aqueous solutions of K2CO3
    Kamps, Alvaro Perez-Salado
    Meyer, Eckehard
    Rumpf, Bernd
    Maurer, Gerd
    JOURNAL OF CHEMICAL AND ENGINEERING DATA, 2007, 52 (03): : 817 - 832
  • [8] Effect of Alloying Additions on the Oxidation of High Speed Steels under Dry and Wet Conditions
    FCRIZZO
    MJMONTEIRO
    SRJSAUNDERS
    中国腐蚀与防护学报, 2009, 29 (04) : 241 - 247
  • [9] The influence of Ni alloying on corrosion behaviour of low alloy steels under wet/dry cyclic conditions
    Chen, X.
    Dong, J.
    Han, E.
    Ke, W.
    CANADIAN METALLURGICAL QUARTERLY, 2007, 46 (02) : 195 - 205
  • [10] Laboratory Studies of Potassium-Halide-Induced High-Temperature Corrosion of Superheater Steels. Part 2: Exposures in Wet Air
    Wu, Hao
    Bankiewicz, Dorota
    Yrjas, Patrik
    Hupa, Mikko
    ENERGY & FUELS, 2015, 29 (04) : 2709 - 2718