Glass-bonded iodosodalite waste form for immobilization of 129I

被引:56
|
作者
Chong, Saehwa [1 ]
Peterson, Jacob A. [3 ]
Riley, Brian J. [2 ,3 ]
Tabada, Diana [4 ]
Wall, Donald [4 ]
Corkhill, Claire L. [5 ]
McCloy, John S. [1 ,2 ,3 ]
机构
[1] Washington State Univ, Mat Sci & Engn Program, Pullman, WA 99164 USA
[2] Washington State Univ, Sch Mech & Mat Engn, POB 642920, Pullman, WA 99164 USA
[3] Pacific Northwest Natl Lab, Richland, WA 99354 USA
[4] Washington State Univ, Nucl Sci Ctr, Pullman, WA 99164 USA
[5] Univ Sheffield, Dept Mat Sci & Engn, NucleUS Immobilisat Sci Lab, Sheffield S1 3JD, S Yorkshire, England
基金
英国工程与自然科学研究理事会;
关键词
Iodosodalite; Sodalite; Glass ceramic waste form; Glass composite material; HYDROXY-SODALITE ZEOLITE; KAOLINITE; IODINE;
D O I
10.1016/j.jnucmat.2018.03.033
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Immobilization of radioiodine is an important requirement for current and future nuclear fuel cycles. Iodosodalite [Na-8(AlSiO4)(6)I-2] was synthesized hydrothermally from metakaolin, NaI, and NaOH. Dried unwashed sodalite powders were used to synthesize glass-bonded iodosodalite waste forms (glass composite materials) by heating pressed pellets at 650, 750, or 850 degrees C with two types of sodium borosilicate glass binders. These heat-treated specimens were characterized with X-ray diffraction, Fourier-transform infrared spectroscopy, scanning electron microscopy, energy dispersive spectroscopy, thermal analysis, porosity and density measurements, neutron activation analysis, and inductively-coupled plasma mass spectrometry. For the best waste form produced (pellets mixed with 10 mass% of glass binder and heat-treated at 750 degrees C), the maximum possible elemental iodine loading was 19.8 mass%, but only similar to 8-9 mass% waste loading of iodine was retained in the waste form after thermal processing. Other pellets with higher iodine retention either contained higher porosity or were incompletely sintered. ASTM C1308 and C1285 (product consistency test, PCT) experiments were performed to understand chemical durability under diffusive and static conditions. The C1308 test resulted in significantly higher normalized loss compared to the C1285 test, most likely because of the strong effect of neutral pH solution renewal and prevention of ion saturation in solution. Both experiments indicated that release rates of Na and Si were higher than for Al and I, probably due to a poorly durable Na-Si-O phase from the glass bonding matrix or from initial sodalite synthesis; however the C1308 test result indicated that congruent dissolution of iodosodalite occurred. The average release rates of iodine obtained from C1308 were 0.17 and 1.29 gm(-2) d(-1) for 80 or 8 m(-1), respectively, and the C1285 analysis gave a value of 2 x 10(-5) g m(-2) d(-1), which is comparable to or better than the durability of other iodine waste forms. (C) 2018 Elsevier B.V. All rights reserved.
引用
收藏
页码:109 / 121
页数:13
相关论文
共 50 条
  • [1] Immobilization of iodine waste via the gas-pressure sintering of glass-bonded iodosodalite ceramic
    Feng Y.
    Wei G.
    Zhang Z.
    Liu Y.
    Ceramics International, 2022, 48 (11) : 16312 - 16318
  • [2] Glass binder development for a glass-bonded sodalite ceramic waste form
    Riley, Brian J.
    Vienna, John D.
    Frank, Steven M.
    Kroll, Jared O.
    Peterson, Jacob A.
    Canfield, Nathan L.
    Zhu, Zihua
    Zhang, Jiandong
    Kruska, Karen
    Schreiber, Daniel K.
    Crum, Jarrod V.
    JOURNAL OF NUCLEAR MATERIALS, 2017, 489 : 42 - 63
  • [3] Fabrication of a glass-bonded zeolite waste form for waste LiCl salt
    Kim, Jeong-Guk
    Lee, Jae-Hee
    Kim, In-Tae
    Kim, Eung-Ho
    JOURNAL OF INDUSTRIAL AND ENGINEERING CHEMISTRY, 2007, 13 (02) : 292 - 298
  • [4] Glass-bonded sodalite: A ceramic nuclear waste form.
    Morss, LR
    Richmann, MK
    Lexa, D
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1999, 218 : U703 - U703
  • [5] Structural parameters and leachability of a glass-bonded ceramic waste form
    Moschetti, TL
    Frank, SM
    Johnson, SG
    ENVIRONMENTAL ISSUES AND WASTE MANAGEMENT TECHNOLOGIES IN THE CERAMIC AND NUCLEAR INDUSTRIES IV, 1999, 93 : 261 - 268
  • [6] Characterization and durability testing of a glass-bonded ceramic waste form
    Johnson, SG
    Frank, SM
    O'Holleran, TP
    Noy, M
    DiSanto, T
    Goff, KM
    Bateman, K
    ENVIRONMENTAL ISSUES AND WASTE MANAGEMENT TECHNOLOGIES IN THE CERAMIC AND NUCLEAR INDUSTRIES IV, 1999, 93 : 313 - 320
  • [7] Preliminary studies of the disposition of cesium in a glass-bonded socialite waste form
    Lambregts, MJ
    Frank, SM
    SCIENTIFIC BASIS FOR NUCLEAR WASTE MANAGEMENT XXV, 2002, 713 : 373 - 380
  • [8] Chemistry and chemical durability of a new 129I glass composite material (GCM) waste form
    Nenoff, M. Tina
    Patrick, Brady V.
    Terry, Garino J.
    Mowry, Curtis D.
    Sava Gallis, Dorina
    Rademacher, David X.
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2014, 247
  • [9] Electron microscopy study of a radioactive glass-bonded sodalite ceramic waste form
    Sinkler, W
    O'Holleran, TP
    Moschetti, TL
    PLUTONIUM FUTURES-THE SCIENCE, 2000, 532 : 166 - 167
  • [10] The precision of product consistency tests conducted with a glass-bonded ceramic waste form
    Ebert, WL
    Lewis, MA
    Johnson, SG
    JOURNAL OF NUCLEAR MATERIALS, 2002, 305 (01) : 37 - 51