Background. Yttrium-stabilized tetragonal zirconia polycrystal (Y-TZP) is used as a core material in all-ceramic restorations. The delamination and chipping of a veneering ceramic are the most common complications in the case of zirconia-based restorations. Objectives. The aim of the study was to investigate the effect of the combined treatment of the zirconium dioxide (ZrO2) surface (airborne-particle abrasion with liner application) on the shear bond strength (SBS) of a veneering ceramic. Material and methods. Thirty pre-sintered ZrO2 cuboidal specimens (VITA YZ (R) HT) were sub-divided into 3 groups: group C consisted of 10 specimens without treatment at the sintering stage; group SZ(1) consisted of 10 specimens treated with airborne-particle abrasion (50-micrometer paricles of aluminum oxide - Al2O3; Korox (R) 50), and then coated with a 0.1-millimeter liner (IPS e.max (R) Ceram ZirLiner) after sintering; group SZ(2) consisted of 10 specimens treated with airborne-particle abrasion (50-micrometer particles of Al2O3), and then coated with a 0.2-millimeter liner after sintering. Ceramic veneers (IPS e.max Ceram Dentin) were then applied using the layering technique. After that, the SBS tests were conducted. Results. The results showed that the combined treatment of the ZrO2 surface significantly affected SBS (p < 0.01). The highest mean value was shown in group C (12.441 +/- 2.284 MPa), followed by group SZ(2) (7.889 +/- 0.794 MPa), whereas the lowest mean value was observed in group SZ(1) (5.580 +/- 0.843 MPa). Conclusions. The combined treatment of the pre-sintered ZrO2 surface significantly reduced the SBS of a veneering ceramic. However, the combined surface treatment with a liner thickness of 0.2 mm significantly enhanced the SBS of a veneering ceramic compared to the same combined treatment but with a liner thickness of 0.1 mm.
引用
收藏
页码:177 / 183
页数:7
相关论文
共 50 条
  • [1] Effect of Cyclic Impact Load on Shear Bond Strength of Zirconium Dioxide Ceramics
    Kawai, Naoko
    Shinya, Akikazu
    Yokoyama, Daiichiro
    Gomi, Harunori
    Shinya, Akiyoshi
    JOURNAL OF ADHESIVE DENTISTRY, 2011, 13 (03): : 267 - 277
  • [2] Effect of Surface Treatment with Zirconium Dioxide Slurry on the Bond Strength of Resin Cement to Ultratranslucent Zirconia
    Colombino, A. C. L.
    Bellan, M. C.
    Correr-Sobrinho, L.
    Miranzi, B. A. S.
    Calabrez-Filho, S.
    Platt, J. A.
    Spohr, A. M.
    Borges, G. A.
    OPERATIVE DENTISTRY, 2024, 49 (05) : 574 - 585
  • [3] Influence of priming agents on the short-term bond strength of an indirect composite veneering material to zirconium dioxide ceramic
    Kobayashi, Kazuhisa
    Komine, Futoshi
    Blatz, Markus B.
    Saito, Ayako
    Koizumi, Hiroyasu
    Matsumura, Hideo
    QUINTESSENCE INTERNATIONAL, 2009, 40 (07): : 545 - 551
  • [4] The effect of surface treatment on bond strength of layering porcelain and hybrid composite bonded to zirconium dioxide ceramics
    Hatta, Minori
    Shinya, Akikazu
    Yokoyama, Daiichiro
    Gomi, Harunori
    Vallittu, Pekka K.
    Shinya, Akiyoshi
    JOURNAL OF PROSTHODONTIC RESEARCH, 2011, 55 (03) : 146 - 153
  • [5] EFFECT OF ZIRCONIA SURFACE TREATMENTS ON THE SHEAR BOND STRENGTH OF VENEERING CERAMIC
    Kim, Hong-Joo
    Lim, Hyun-Pil
    Park, Yeong-Joon
    Vang, Mong-Sook
    JOURNAL OF PROSTHETIC DENTISTRY, 2011, 105 (05): : 315 - 322
  • [6] Durability of bond between an indirect composite veneering material and zirconium dioxide ceramics
    Komine, Futoshi
    Kobayashi, Kazuhisa
    Blatz, Markus B.
    Fushiki, Ryosuke
    Koizuka, Mai
    Taguchi, Kohei
    Matsumura, Hideo
    ACTA ODONTOLOGICA SCANDINAVICA, 2013, 71 (3-4) : 457 - 463
  • [7] EFFECT OF POROUS STRUCTURE OF A CASTING OF SUBMICRON POWDERS ON THE STRENGTH OF A ZIRCONIUM DIOXIDE CERAMIC
    GALAKHOV, AV
    VYAZOV, IV
    SHEVCHENKO, VY
    EZHOV, AA
    INORGANIC MATERIALS, 1990, 26 (04) : 695 - 700
  • [8] Effect of surface treatment on the initial bond strength of different luting cements to zirconium oxide ceramic
    Nothdurft, F. P.
    Motter, P. J.
    Pospiech, P. R.
    CLINICAL ORAL INVESTIGATIONS, 2009, 13 (02) : 229 - 235
  • [9] Effect of surface treatment on the initial bond strength of different luting cements to zirconium oxide ceramic
    F. P. Nothdurft
    P. J. Motter
    P. R. Pospiech
    Clinical Oral Investigations, 2009, 13 : 229 - 235
  • [10] CERAMIC MATERIALS BASED ON ZIRCONIUM DIOXIDE
    MOROZOVA, LV
    IVASHKIN, VV
    GLUSHKOVA, VB
    RUSSIAN JOURNAL OF APPLIED CHEMISTRY, 1994, 67 (07) : 947 - 949