Glow discharge nitriding of AISI 316L austenitic stainless steel: Influence of treatment pressure

被引:97
|
作者
Borgioli, F [1 ]
Fossati, A [1 ]
Galvanetto, E [1 ]
Bacci, T [1 ]
Pradelli, G [1 ]
机构
[1] Univ Florence, Dipartimento Ingn Civile, I-50139 Florence, Italy
来源
SURFACE & COATINGS TECHNOLOGY | 2006年 / 200卷 / 18-19期
关键词
glow discharge nitriding; austenitic stainless steel; AISI; 316L; S phase;
D O I
10.1016/j.surfcoat.2005.07.073
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The influence of treatment pressure on the characteristics of the modified surface layers produced by low-temperature d.c. glow discharge nitriding on AISI 316L austenitic stainless steel samples is investigated. Glow discharge nitriding treatments were performed at 703 K for 5 h at working pressures in the range of 1.5-20 hPa. Morphology and microstructure of the untreated and nitrided samples were studied by means of microscopy techniques, energy dispersion spectroscopy and X-ray diffraction analysis; microhardness measurements and corrosion resistance tests were also performed. The nitriding treatments produce a hardened surface layer consisting mainly of the so-called S phase. The presence of nitrides and the thickness of the modified layer depend on the used treatment pressure. When treatments are performed at 2.5 hPa, a fairly large amount of nitrides is observed in the modified layer, while when the nitriding pressure is lower or higher than 2.5 hPa, the nitride amount decreases and the layer becomes thinner. When the treatments are performed at 10 or 20 hPa, only a very small amount of chromium nitride is present as small surface precipitates. Metallographic analysis shows that many slip lines are present both at the surface and in the cross-section of the modified layer, presumably due to high stresses occurring during the formation of the layer. X-ray diffraction analysis of the S phase shows that its diffraction peaks are shifted from those of a perfect f.c.c. lattice; the observed shifts may be explained assuming that the S phase has an f.c.c. structure with a high density of stacking faults. Corrosion resistance tests, performed in 5% NaCl aerated solution with the potentiodynamic method, show that with the used treatment parameters nitriding at a pressure of 10 hPa or higher allows to obtain a significant improvement of the corrosion resistance in respect of the untreated alloy, reducing the anodic currents up to about 4 orders of magnitude. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:5505 / 5513
页数:9
相关论文
共 50 条
  • [1] Glow-discharge nitriding of AISI 316L austenitic stainless steel: influence of treatment temperature
    Borgioli, F
    Fossati, A
    Galvanetto, E
    Bacci, T
    [J]. SURFACE & COATINGS TECHNOLOGY, 2005, 200 (07): : 2474 - 2480
  • [2] Glow-discharge nitriding of AISI 316L austenitic stainless steel: influence of treatment time
    Fossati, A
    Borgioli, F
    Galvanetto, E
    Bacci, T
    [J]. SURFACE & COATINGS TECHNOLOGY, 2006, 200 (11): : 3511 - 3517
  • [3] Unconventional Glow Discharge Nitriding of 316L Austenitic Steel
    Fraczek, Tadeusz
    Olejnik, Michel
    [J]. THERMEC 2009, PTS 1-4, 2010, 638-642 : 882 - 887
  • [4] Corrosion resistance of sintered austenitic stainless steel aisi 316L after active screen glow-discharge nitriding
    Brojanowska, Agnieszka
    Kaminski, Janusz
    Trojanowski, Janusz
    Kazior, Jan
    Wierzchon, Tadeusz
    [J]. OCHRONA PRZED KOROZJA, 2011, 54 (02): : 52 - 56
  • [5] ASSESSMENT OF THE EFFECTIVENESS OF 316L AUSTENITIC STEEL UNCONVENTIONAL GLOW DISCHARGE NITRIDING
    Fraczek, T.
    Kolmasiak, C.
    Olejnik, M.
    Skuza, Z.
    [J]. METALURGIJA, 2011, 50 (02): : 97 - 100
  • [6] Structure and wear resistance of the composite layers produced by glow discharge nitriding and PLD method on AISI 316L austenitic stainless steel
    Skolek-Stefaniszyn, E.
    Burdynska, S.
    Mroz, W.
    Wierzchon, T.
    [J]. VACUUM, 2009, 83 (12) : 1442 - 1447
  • [7] Nitriding of 316L Steel in a Glow Discharge Plasma
    Fraczek, Tadeusz
    Prusak, Rafal
    Ogorek, Marzena
    Skuza, Zbigniew
    [J]. MATERIALS, 2022, 15 (09)
  • [8] Unconventional Short-term Glow Discharge Nitriding of 316L Austenitic Steel
    Fraczek, Tadeusz
    Olejnik, Michel
    Jasinski, Jaroslaw
    [J]. PRICM 7, PTS 1-3, 2010, 654-656 : 366 - 369
  • [9] Corrosion resistance of austenitic steel 316l after unconventional glow discharge nitriding
    Fraczek, Tadeusz
    Jeziorski, Leopold
    Olejnik, Michal
    [J]. OCHRONA PRZED KOROZJA, 2009, 52 (11): : 488 - 491
  • [10] Low temperature nitriding of AISI 316L stainless steel and titanium in a low pressure arc discharge
    Renevier, N
    Collignon, P
    Michel, H
    Czerwiec, T
    [J]. SURFACE & COATINGS TECHNOLOGY, 1999, 111 (2-3): : 128 - 133