Thermal stability and oxidation resistance of V-alloyed TiAlN coatings

被引:52
|
作者
Xu, Yu X. [1 ]
Chen, Li [1 ]
Pei, Fei [1 ,2 ]
Yue, Jian L. [3 ]
Du, Yong [1 ]
机构
[1] Cent S Univ, State Key Lab Powder Met, Changsha 410083, Hunan, Peoples R China
[2] Chinese Acad Sci, Ningbo Inst Mat Technol & Engn, Key Lab Marine Mat & Related Technol, Ningbo 315201, Zhejiang, Peoples R China
[3] Cent S Univ, Sch Aeronaut & Astronaut, Changsha 410083, Hunan, Peoples R China
基金
中国国家自然科学基金;
关键词
Films; TiAlVN; Hardness; Thermal properties; SELF-ORGANIZED NANOSTRUCTURES; TRIBOLOGICAL PROPERTIES; TEMPERATURE; PERFORMANCE; FRICTION; BEHAVIOR; WEAR;
D O I
10.1016/j.ceramint.2017.10.100
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
V-containing nitride coatings recently attract a wide range of research interests owing to their excellent tribo-logical properties. To evaluate their comprehensive properties, a comparative study on the intrinsic thermal stability and oxidation resistance of TiAIN and TiA1VN coatings are conducted here. Ti0.56Al0.44N, Ti0.50Al0.44V0.06N, and Ti0.40Al0.50V0.10N coatings, deposited by cathodic arc evaporation, exhibit a single-phase face-centered cubic structure with a hardness of 28.9-29.8 GPa. The V-containing coatings show a pronounced age-hardening upon annealing, which contributes to a hardness increase of 3.7 and 4.8 GPa at 800 degrees C for Ti0..50Al0.44V0.06N and Ti0.40Al0.50V0.10N, respectively, corresponding to 2.9 GPa for Ti0.56Al0.44N. Also, alloying with V retards the formation of wurtzite AIN upon annealing, especially in Ti0.50Al0.44V0.06N, and thus contributes to a higher hardness above 30 GPa even annealing at 1100 degrees C, while the hardness of Ti0.56Al0.44N significantly reduces to 27.8 +/- 0.6 GPa. However, alloying with V into TiAlN leads to an earlier formation of rutile TiO2 and also Ti-rich oxide top-layer on the outside surface instead of dense A1203, and thus degrades the oxidation resistance. When exposed to air at 700 degrees C for 10 h, the Ti0.50Al0.44V0.06N and Ti0.40Al0.50V0.10N coatings suffer from a severe oxidation, whereas only a compact oxide scale with a thickness of similar to 80 nm for Ti0.56Al0.44N is formed.
引用
收藏
页码:1705 / 1710
页数:6
相关论文
共 50 条
  • [1] Thermal stability and oxidation resistance of TiAlN/CrN multilayer coatings
    Sheffield Hallam Univ, Sheffield, United Kingdom
    Surf Coat Technol, 1-3 (315-321):
  • [2] Thermal stability and oxidation resistance of arc evaporated TiAlN, TaAlN, TiAlTaN, and TiAlN/TaAlN coatings
    Koller, C. M.
    Hollerweger, R.
    Sabitzer, C.
    Rachbauer, R.
    Kolozsvari, S.
    Paulitsch, J.
    Mayrhofer, P. H.
    SURFACE & COATINGS TECHNOLOGY, 2014, 259 : 599 - 607
  • [3] Effect of B-doping on the mechanical properties, thermal stability and oxidation resistance of TiAlN coatings
    Zhou, Jian
    Hu, Chun
    Zhang, Jie
    Chen, Li
    Kong, Yi
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2021, 98
  • [4] Effect of V-addition on the thermal stability and oxidation resistance of CrAlN coatings
    Xu, Yu X.
    Hu, Chun
    Chen, Li
    Pei, Fei
    Du, Yong
    CERAMICS INTERNATIONAL, 2018, 44 (06) : 7013 - 7019
  • [5] Oxidation resistance of TiAlN/ZrN multilayer coatings
    Lei, Zhefeng
    Liu, Yashan
    Ma, Fei
    Song, Zhongxiao
    Li, Yanhuai
    VACUUM, 2016, 127 : 22 - 29
  • [6] Influence of Ru-addition on thermal decomposition and oxidation resistance of TiAlN coatings
    Liu, Zhe R.
    Chen, Li
    Du, Yong
    Zhang, Shuyan
    SURFACE & COATINGS TECHNOLOGY, 2020, 401
  • [7] Enhanced thermal stability and fracture toughness of TiAlN coatings by Cr, Nb and V-alloying
    Chen, Y. H.
    Roa, J. J.
    Yu, C. H.
    Johansson-Joesaar, M. P.
    Andersson, J. M.
    Anglada, M. J.
    Oden, M.
    Rogstrom, L.
    SURFACE & COATINGS TECHNOLOGY, 2018, 342 : 85 - 93
  • [8] Comparison of microstructure stability and oxidation resistance of Ti/TiN, Ti/TiAlN, and Cr/TiAlN multilayer coatings on TC4 titanium alloy under thermal cycling
    Zhang, Mingming
    Li, Ruizhe
    Zhang, Yaqi
    Li, Yongfeng
    Niu, Yunsong
    Xin, Li
    Zhu, Shenglong
    Wang, Fuhui
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1019
  • [9] Improved oxidation resistance of TiAlN coatings by doping with Si or B
    Pfeiler, M.
    Zechner, J.
    Penoy, M.
    Michotte, C.
    Mitterer, C.
    Kathrein, M.
    SURFACE & COATINGS TECHNOLOGY, 2009, 203 (20-21): : 3104 - 3110
  • [10] Hard nanocomposite coatings: Thermal stability, oxidation resistance and toughness
    Musil, J.
    SURFACE & COATINGS TECHNOLOGY, 2012, 207 : 50 - 65