Corrosion Behavior of TWIP Steels in 3.5% NaCl Solution

被引:4
|
作者
Razavi, Gholam Reza [1 ]
Monajati, Hossein [1 ]
机构
[1] Islamic Azad Univ, Najafabad Branch, Dept Mat Sci & Engn, Esfahan, Iran
关键词
TWIP Steel; Pitting corrosion; 3.5% NaCl Solution; TRIP/TWIP STEELS;
D O I
10.4028/www.scientific.net/AMR.457-458.334
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
TWIP steels are high Mn (17-35%) austenitic steels having strength and ductility concurrently. This makes them suitable for applications that need high strength and ductility like gas tanks and oil platforms. To these applications corrosion resistance of these steel is also of paramount importance and needs to be noticed. This was achieved by two usual methods of weight loss and potentiodynamic polarization of the samples, after that they casted and hot rolled in experimental scale. The observed corrosion pits are related to the chemical composition. It is connected with the high dissolution rate of Mn and Fe atoms in NaCl solution. Fractographic analyses of samples revealed corrosion products on their surface in a form of pits with diversified size.
引用
收藏
页码:334 / 337
页数:4
相关论文
共 50 条
  • [1] Corrosion of Novel Rail Steels in 3.5 % NaCl solution
    Panda, Bijayani
    Balasubramaniam, R.
    Dwivedi, Gopal
    Mahapatra, Sujata
    [J]. TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2008, 61 (2-3) : 177 - 181
  • [2] Corrosion of novel rail steels in 3.5 % NaCl solution
    Bijayani Panda
    R. Balasubramaniam
    Gopal Dwivedi
    Sujata Mahapatra
    [J]. Transactions of the Indian Institute of Metals, 2008, 61 : 177 - 181
  • [3] The corrosion behavior of niobium bearing cold deformed austenitic stainless steels in 3.5% NaCl solution
    Hamdy, Abdel Salam
    El-Shenawy, Eman
    El-Bitar, T.
    [J]. MATERIALS LETTERS, 2007, 61 (13) : 2827 - 2832
  • [4] Influence of chromium on the flow-accelerated corrosion behavior of low alloy steels in 3.5% NaCl solution
    Jiang, Shan
    Chai, Feng
    Su, Hang
    Yang, Caifu
    [J]. CORROSION SCIENCE, 2017, 123 : 217 - 227
  • [5] Effect of Quenching and Tempering Temperature on Corrosion Behavior of Boron Steels in 3.5 wt.% NaCl Solution
    Aydin, Gurkan
    Yazici, Aysel
    [J]. INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2019, 14 (03): : 2126 - 2135
  • [6] Pitting corrosion resistance of cast duplex stainless steels in 3.5%NaCl solution
    do Nascimento, A. M.
    Ierardi, M. C. F.
    Kina, A. Y.
    Tavares, S. S. M.
    [J]. MATERIALS CHARACTERIZATION, 2008, 59 (12) : 1736 - 1740
  • [7] Corrosion behavior of Al-Ce alloys in 3.5%NaCl solution
    Zhou, Xianjie
    Xiong, Hanqing
    [J]. INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2022, 17 (01):
  • [8] Corrosion wear behavior of Al-bronzes in 3.5% NaCl solution
    W. S. Li
    Z. P. Wang
    Y. Lu
    L. H. Yuan
    [J]. Journal of Materials Engineering and Performance, 2006, 15 : 102 - 110
  • [9] Corrosion wear behavior of Al-bronzes in 3.5% NaCl solution
    Li, WS
    Wang, ZP
    Lu, Y
    Yuan, LH
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2006, 15 (01) : 102 - 110
  • [10] Corrosion behavior of Ni-Cr alloys in 3.5% NaCl solution
    School of Science, Shenyang University of Technology, Shenyang 110870, China
    不详
    [J]. Shenyang Gongye Daxue Xuebao, 2009, 5 (512-515):