Effect of titanium ion implantation and deposition on hydrogenation behavior of Zr-1Nb alloy

被引:17
|
作者
Kashkarov, E. B. [1 ]
Nikitenkov, N. N. [1 ]
Sutygina, A. N. [1 ]
Syrtanov, M. S. [1 ]
Vilkhivskaya, O. V. [1 ,2 ]
Pryamushko, T. S. [1 ]
Kudiiarov, V. N. [1 ]
Volesky, L. [3 ]
机构
[1] Natl Res Tomsk Polytech Univ, Tomsk 634050, Russia
[2] Troitsk Inst Innovat & Fus Res, Troitsk 142190, Russia
[3] Tech Univ Liberec, Inst Nanomat Adv Technol & Innovat, Liberec 46117, Czech Republic
来源
基金
俄罗斯基础研究基金会;
关键词
Zirconium; Titanium; Ion implantation; Deposition; Hydrogenation; Hydrogen absorption; Optical emission spectroscopy; WT-PERCENT NB; SURFACE MODIFICATION; VACUUM-ARC; CORROSION BEHAVIOR; HYDRIDE FORMATION; ZIRCONIUM ALLOYS; FORCE MICROSCOPY; PLASMA; OXIDATION; METALS;
D O I
10.1016/j.surfcoat.2016.07.111
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In order to study the effect of titanium ion implantation and deposition on hydrogenation behavior of Zr-1Nb alloy, the samples were subjected to plasma immersion implantation and deposition (PIII&D) of titanium ions at the bias voltage of 0.5-1.5 kV using a filtered metal vapor vacuum arc source. The crystalline structure, surface morphology and depth distributions of elements in the surface layer of the samples were analyzed by X-ray diffraction (XRD), scanning electron microscopy (SEM) and glow-discharge optical emission spectroscopy (GD-OES), respectively. Hydrogen saturation was performed from hydrogen atmosphere at 673 IC temperature and 2 atm. pressure. It was found that hydrogen absorption rate by Zr-1Nb alloy decreased after PIII&D. The modified layers contained a mixing zone of titanium and zirconium, which decreases with increasing bias voltage. Hydrogenation causes the formation of titanium hydrides and lattice distortions of alpha-Zr at the low bias voltage that does not occur at higher bias voltages. The hydrogenation behavior of modified zirconium alloy was discussed. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:2 / 9
页数:8
相关论文
共 50 条
  • [1] High-intensity chromium ion implantation into Zr-1Nb alloy
    Ryabchikov, A. I.
    Kashkarov, E. B.
    Shevelev, A. E.
    Syrtanov, M. S.
    SURFACE & COATINGS TECHNOLOGY, 2020, 383 (383):
  • [2] Thermal stability and hydrogenation behavior of Zr-1Nb alloy with TiNx and Ti/TiNx coatings
    Kashkarov, E. B.
    Vilkhivskaya, O. V.
    Zakharchenko, S. A.
    3RD INTERNATIONAL SCHOOL AND CONFERENCE ON OPTOELECTRONICS, PHOTONICS, ENGINEERING AND NANOSTRUCTURES (SAINT PETERSBURG OPEN 2016), 2016, 741
  • [3] High temperature deformation behavior of Zr-1Nb alloy
    Sarkar, Apu
    Chandanshive, Sandeep A.
    Thota, Manoj K.
    Kapoor, Rajeev
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 703 : 56 - 66
  • [4] Effect of quenching on the corrosion resistance of the Zr-1Nb alloy
    Xue, XY
    Song, QZ
    Liu, JZ
    Li, PZ
    RARE METAL MATERIALS AND ENGINEERING, 1998, 27 (05) : 302 - 305
  • [5] Microstructure, defect structure and hydrogen trapping in zirconium alloy Zr-1Nb treated by plasma immersion Ti ion implantation and deposition
    Kashkarov, Egor
    Nikitenkov, Nikolay
    Sutygina, Alina
    Laptev, Roman
    Bordulev, Yuriy
    Obrosov, Aleksei
    Liedke, Maciej O.
    Wagner, Andreas
    Zak, Andrzej
    Weiss, Sabine
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 732 : 80 - 87
  • [6] Recrystallization behavior of cold-rolled Zr-1Nb alloy
    Tian, Hang
    Wang, Xitao
    Gong, Weijia
    Zhou, Jun
    Zhang, Hailong
    JOURNAL OF NUCLEAR MATERIALS, 2015, 456 : 321 - 328
  • [7] Oxidation Behavior of Zr-1Nb Corroded in Air at 400 °C after Plasma Immersion Titanium Implantation
    Obrosov, Aleksei
    Sutygina, Alina N.
    Manakhov, Anton
    Bolz, Sebastian
    Weiss, Sabine
    Kashkarov, Egor B.
    METALS, 2018, 8 (01)
  • [8] Structure Effect on the Diffusion and Accumulation of Hydrogen in the Zr-1Nb Alloy
    Grabovetskaya, G. P.
    Stepanova, E. N.
    Nikitenkov, N. N.
    Mishin, I. P.
    Vinokurov, V. A.
    Sypchenko, V. S.
    Kudiiarov, V. N.
    RUSSIAN PHYSICS JOURNAL, 2023, 65 (8) : 1340 - 1347
  • [9] Hydrogen Interaction with Deep Surface Modified Zr-1Nb Alloy by High Intensity Ti Ion Implantation
    Kashkarov, Egor B.
    Ryabchikov, Alexander, I
    Kurochkin, Alexander, V
    Syrtanov, Maxim S.
    Shevelev, Alexey E.
    Obrosov, Aleksei
    Weiss, Sabine
    METALS, 2018, 8 (12):
  • [10] Effect of neutron irradiation on microstructural evolution and deformation behavior of Zirconium (Zr-1Nb) alloy
    Jarugula, Rajesh
    Halodova, Patricie
    Zimina, Mariia
    Sundararaman, M.
    Mala, Martina
    Klouzal, Jan
    Sevecek, Martin
    Belac, Josef
    Rehacek, Radomir
    Linhart, Stanislav
    JOURNAL OF NUCLEAR MATERIALS, 2025, 605