Mechanical properties of fine-grained, sintered molybdenum alloys with dispersed particles developed by mechanical alloying

被引:25
|
作者
Takida, T [1 ]
Kurishita, H
Mabuchi, M
Igarashi, T
Doi, Y
Nagae, T
机构
[1] Allied Mat Corp, Toyama 9318543, Japan
[2] Tohoku Univ, Inst Mat Res, Oarai Branch, Oarai, Ibaraki 3111313, Japan
[3] Natl Inst Adv Ind Sci & Technol, Nagoya, Aichi 4638560, Japan
[4] Osaka Prefecture Univ, Sakai, Osaka 5998531, Japan
[5] Toyama Ind Technol Ctr, Takaoka, Toyama 9330981, Japan
关键词
molybdenum; zirconium carbide; tantalum carbide; mechanical alloying; fine grain; particle dispersion; thermal stability of microstructure; ductile brittle transition temperature; high-temperature strength;
D O I
10.2320/matertrans.45.143
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In order to develop Mo alloys with improved mechanical properties of low-temperature toughness and room- and high-temperature strengths without any plastic working after consolidation, fine-grained, particle-dispersed Mo alloys were fabricated by hot isostatic pressing (HIP) or spark plasma sintering (SPS) of mechanically alloyed powders of Mo and 0.8mol% ZrC or TaC (designated as ZRC08 and TAC08). The fabricated Mo alloys were subjected to high-temperature annealing for 3.6 ks up to 2470 K, three-point impact bending tests at temperatures from 270 to 470 K at 5 m s(-1) and static tensile tests at temperatures from 300 to 1970 K at initial strain rates from 4.2 x 10(-5) to 8.3 x 10(-2) s(-1). The fabricated alloys exhibited no significant grain growth even after annealing at 2470 K for 3.6 ks due to the pinning effect of the particles against grain boundary migration. The ductile-to-brittle transition temperatures (DBTT) assessed by impact bending were lower and the tensile strengths up to 1770 K were higher for the fabricated alloys than for recrystallized pure Mo. In particular, HIPed TAC08 was superior in low-temperature toughness having the DBTT lower by 30-40 K than recrystallized Mo-La2O3 (TEM) with an elongated coarse-grained microstructure. HIP- or SPS-treated ZRC08 was superior in room- and high-temperature strengths, respectively. Furthermore, HIPed ZRC08 showed a large elongation of 551% at 1770 K. These excellent mechanical properties of the fabricated Mo alloys were obtained for the first time in the as-consolidated state without subsequent plastic working, and are attributable to fine-grained microstructure and grain-boundary strengthening by the fine particles.
引用
收藏
页码:143 / 148
页数:6
相关论文
共 50 条
  • [1] Tensile properties of fine-grained sintered molybdenum alloys dispersed with ZrC or TaC particles
    Takida, Tomohiro
    Igarashi, Tadashi
    Mabuchi, Mamoru
    Nakamura, Mamoru
    Doi, Yoshiharu
    Nagae, Takekazu
    [J]. Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 1999, 46 (10): : 1031 - 1036
  • [2] MICROSTRUCTURES AND MECHANICAL PROPERTIES OF SINTERED FINE-GRAINED Al
    Le Guomin
    Andrew, Godfrey
    Liu Wei
    [J]. ACTA METALLURGICA SINICA, 2013, 49 (08) : 939 - 945
  • [3] Processing and mechanical properties of fine-grained magnesium alloys
    Kubota, K
    Mabuchi, M
    Higashi, K
    [J]. JOURNAL OF MATERIALS SCIENCE, 1999, 34 (10) : 2255 - 2262
  • [4] Review Processing and mechanical properties of fine-grained magnesium alloys
    K. Kubota
    M. Mabuchi
    K. Higashi
    [J]. Journal of Materials Science, 1999, 34 : 2255 - 2262
  • [5] SUPERPLASTICITY IN VERY FINE-GRAINED AL-BASED ALLOYS PRODUCED BY MECHANICAL ALLOYING
    HIGASHI, K
    OKADA, T
    MUKAI, T
    TANIMURA, S
    NIEH, TG
    WADSWORTH, J
    [J]. MATERIALS TRANSACTIONS JIM, 1995, 36 (02): : 317 - 322
  • [6] The Bauschinger effect in fine-grained Al-Ti alloys prepared by mechanical alloying
    Liao, SH
    Kao, PW
    Chang, CP
    [J]. SCRIPTA MATERIALIA, 1997, 36 (11) : 1227 - 1232
  • [7] Influence of strain rate on the mechanical properties in fine-grained aluminum alloys
    Mukai, T
    Ishikawa, K
    Higashi, K
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 204 (1-2): : 12 - 18
  • [8] Microstructure and mechanical properties of fine-grained high nitrogen steels fabricated through mechanical alloying treatment
    Uchida, Hiroyuki
    Kataoka, Kouta
    Tsuchiyama, Toshihiro
    Goto, Hideto
    Takaki, Setsuo
    [J]. Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 2001, 48 (10): : 980 - 985
  • [9] Preparation of fine-grained Mo-12Si-8.5B alloys with improved mechanical properties via a mechanical alloying process
    Li, Bin
    Zhang, Guo-jun
    Jiang, Feng
    Ren, Shuai
    Liu, Gang
    Sun, Jun
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 609 : 80 - 85
  • [10] Preparation of fine-grained Mo-12Si-8.5B alloys with improved mechanical properties via a mechanical alloying process
    Li, Bin
    Zhang, Guo-Jun
    Feng, Jiang
    Shuai, Ren
    Gang, Liu
    Jun, Sun
    [J]. Zhang, G.-J. (zhangguojun@mail.xjtu.edu.cn), 1600, Elsevier Ltd (609): : 80 - 85