Comparative Performance of Silicone Rubber Insulators with IEC Stipulated Test Methods

被引:0
|
作者
Vasudev, N. [1 ]
Vynatheya, S. [1 ]
Senthilkumar, R. T. [2 ]
机构
[1] Cent Power Res Inst, Bangalore, Karnataka, India
[2] KS Rangasamy coll Technol, Tiruchengode, Tamil Nadu, India
关键词
accelerated ageing; pollution; polymeric insulator; rotating wheel dip test; salt fog test;
D O I
暂无
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
IEC standard 61109 /62217 stipulates three alternatives for design tests for polymeric insulators, namely (a) tracking and erosion test(1000hours), (b) track wheel test (30,000 cycles) and (c) multi-stress ageing test (5000 hours). The minimum requirement for the insulator to comply with the design test is compliance with any one of these tests. However, experience in carrying out these tests in CPRI indicate that the assess the relative merits of the tracking and erosion test and the track wheel test, both the tests were carried out on a 33 kV polymeric insulator. Both the tests were terminated after 1000 hours. The results indicate track wheel test is severe. Analytical tests such as hydrophobicity test, EDX and XRD tests were performed to check the degree of degradation of the insulator material.
引用
收藏
页数:4
相关论文
共 50 条
  • [1] Comparative Performance of 11kV Silicone Rubber Polymeric Insulators under Rotating Wheel Dip Test
    Krzma, A. S.
    Albano, M.
    Haddad, A.
    2014 49TH INTERNATIONAL UNIVERSITIES POWER ENGINEERING CONFERENCE (UPEC), 2014,
  • [2] Performance of silicone rubber composite insulators in Sri Lanka
    Fernando, M. A. R. M.
    Rajamantri, H.
    Gubanski, S. M.
    2006 INTERNATIONAL CONFERENCE ON INDUSTRIAL AND INFORMATION SYSTEMS, VOLS 1 AND 2, 2006, : 14 - +
  • [3] Test Research on Operation Life of Silicone Rubber Composite Insulators
    Luo, Junhua
    Jin, Weidong
    Luo, Min
    2007 IEEE INTERNATIONAL CONFERENCE ON SOLID DIELECTRICS, VOLS 1 AND 2, 2007, : 110 - +
  • [4] Review of Aging Evaluation Methods for Silicone Rubber Composite Insulators
    Zeng, Zhou
    Guo, Pan
    Zhang, Ruoshuang
    Zhao, Zhirui
    Bao, Jiankang
    Wang, Qian
    Xu, Zheng
    POLYMERS, 2023, 15 (05)
  • [5] Comparative Performance of 11kV Silicone Rubber Insulators using Artificial Pollution Tests
    Krzma, A. S.
    Albano, M.
    Haddad, A.
    2015 50TH INTERNATIONAL UNIVERSITIES POWER ENGINEERING CONFERENCE (UPEC), 2015,
  • [6] Performance of Silicone Rubber Insulators Under Thermal and Electrical Stress
    Chakraborty, Rahul
    Reddy, Subba B.
    IEEE TRANSACTIONS ON INDUSTRY APPLICATIONS, 2017, 53 (03) : 2446 - 2454
  • [7] Effect of shed design on aging performance of silicone rubber insulators
    El-Hag, AH
    Jayaram, S
    Cherney, EA
    2002 ANNUAL REPORT CONFERENCE ON ELECTRICAL INSULATION AND DIELECTRIC PHENOMENA, 2002, : 363 - 366
  • [8] Anomalous flashovers of silicone rubber insulators under the artificial rain test
    Chrzan, Krystian Leonard
    Brzezinski, Henryk Marek
    ARCHIVES OF ELECTRICAL ENGINEERING, 2021, 70 (04) : 835 - 844
  • [9] Outdoor Polymeric Insulators: Role of Corona in Performance of Silicone Rubber Housings
    Gubanski, Stanislaw M.
    2015 IEEE CONFERENCE ON ELECTRICAL INSULATION AND DIELECTRIC PHENOMENA (CEIDP), 2015, : 1 - 9
  • [10] Performance Comparison of Silicone Rubber and EPDM Insulators in Humid and Contaminated Environments
    Arshad
    Nekahi, A.
    McMeekin, S. G.
    Farzaneh, M.
    2016 IEEE INTERNATIONAL CONFERENCE ON DIELECTRICS (ICD), VOLS 1-2, 2016, : 712 - 715