Effect of BN/SiC interfacial coatings on the tensile properties of SiC/SiC minicomposites fabricated by PIP

被引:18
|
作者
Dai, Jianwei [1 ,2 ]
Wang, Yiguang [1 ]
Xu, Zhenhua [2 ]
Mu, Rende [2 ]
Liu, Wei [2 ]
He, Limin [2 ]
机构
[1] Northwestern Polytech Univ, Sci & Technol Thermostruct Composite Mat Lab, Xian 710072, Peoples R China
[2] AECC Beijing Inst Aeronaut Mat, Key Lab Adv Corros & Protect Aviat Mat, Beijing 100095, Peoples R China
基金
中国国家自然科学基金;
关键词
Ceramic matrix composites; Interfacial coating; Precursor infiltration and pyrolysis; Chemical vapor infiltration; Tensile properties; Fracture mechanism; SIC FIBERS; XPS; DEGRADATION; TEMPERATURE; COMPOSITES; BEHAVIOR; DESIGN; FILMS;
D O I
10.1016/j.ceramint.2020.06.292
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Boron nitride and silicon carbide interfacial coatings were deposited by chemical vapor infiltration to prepare SiC/SiC minicomposites by the precursor infiltration and pyrolysis process. The tensile properties of the SiC/SiC minicomposites were assessed by the acoustic emission method. A single-layered BN coating increased the strength of the uncoated minicomposite from 416.4 MPa to 478.6 MPa, while the strengths of the BN/SiC-1 and BN/SiC-2 samples with a double-layered coating were 582.3 and 638.1 MPa, respectively. The total thickness of the BN/SiC-2 coating was the same as that of BN/SiC-1, while the BN/SiC-2 sample had a thicker BN layer. Besides the release of residual stress and elastic deformation stages, the stress-strain curve of minicomposite with interfacial coating contains a non-linear stage corresponding to the matrix crack generation, propagation, and deflection. Moreover, minimal fiber debonding was observed in the uncoated minicomposite, whereas fiber debonding of BN and BN/SiC-1 minicomposites occurred at the interface between the BN coating and fibers. In the double-layered BN/SiC-2 minicomposites, following matrix crack generation and propagation into the BN coating, cracks deflected both between the sublayers and at the interface between BN and fibers, where the debonding occurred.
引用
收藏
页码:25058 / 25065
页数:8
相关论文
共 50 条
  • [1] Effect of BN/SiC Multilayered Interphases on Mechanical Properties of SiC Fibers and Minicomposites by PIP
    Lu Xiaoxu
    Jiang Zhuyu
    Zhou Yiran
    Qi Zhe
    Zhao Wenqing
    Jiao Jian
    JOURNAL OF INORGANIC MATERIALS, 2020, 35 (10) : 1099 - 1104
  • [2] Microstructure and tensile behavior of (BN/SiC)n coated SiC fibers and SiC/SiC minicomposites
    Lue, Xiaoxu
    Li, Longbiao
    Sun, Jiajia
    Yang, Jinhua
    Jiao, Jian
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (05) : 1828 - 1842
  • [3] Effect of BN and BN/SiC coatings on tensile properties and failure behavior of SiC fiber monofilament
    Jiao, Jian
    Zhao, Wenqing
    Qi, Zhe
    Lyu, Xiaoxu
    Yang, Jinhua
    Liu, Hu
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2023, 51 (02): : 152 - 159
  • [4] Oxidation Behavior of SiCf/SiC Minicomposites with Multilayered (BN/SiC)n Interfacial Coatings under Humid Environment
    Dai, Jianwei
    He, Limin
    Xu, Zhenhua
    Shen, Zaoyu
    Zhen, Zhen
    Liu, Guanxi
    Mu, Rende
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (12) : 10343 - 10353
  • [5] Oxidation Behavior of SiCf/SiC Minicomposites with Multilayered (BN/SiC)n Interfacial Coatings under Humid Environment
    Jianwei Dai
    Limin He
    Zhenhua Xu
    Zaoyu Shen
    Zhen Zhen
    Guanxi Liu
    Rende Mu
    Journal of Materials Engineering and Performance, 2022, 31 : 10343 - 10353
  • [6] Influences of the dip-coated BN interface on mechanical behavior of PIP-SiC/SiC minicomposites
    Xu, Hao
    Li, Lu
    Zheng, Ruixiao
    Ma, Chaoli
    CERAMICS INTERNATIONAL, 2021, 47 (11) : 16192 - 16199
  • [7] Impact of fiber surface gas treatments on interfacial bonding in SiC/BN/SiC minicomposites
    Chanson, Charlotte
    Jouannigot, Stephane
    Jacques, Sylvain
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2024, 21 (04) : 2747 - 2756
  • [8] In-situ tensile damage and fracture behavior of PIP SiC/SiC minicomposites at room temperature
    Yang, Haitang
    Xu, Shenwei
    Zhang, Daxu
    Li, Longbiao
    Huang, Xiaozhong
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2021, 41 (14) : 6869 - 6882
  • [9] Oxidation behavior and damage mechanism of SiCf/SiC minicomposites with multilayered (BN/SiC)n interfacial coatings at 1200 celcius
    Dai, Jianwei
    He, Limin
    Mu, Rende
    Xu, Zhenhua
    Shen, Zaoyu
    Zhang, Rujing
    Liu, Guanxi
    COMPOSITE INTERFACES, 2023, 30 (01) : 1 - 19
  • [10] Evaluating the effect of oxygen content in BN interfacial coatings on the stability of SiC/BN/SiC composites
    More, KL
    Ailey, KS
    Lowden, RA
    Lin, HT
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1999, 30 (04) : 463 - 470