Effect of long-term aging on the fracture toughness of primary coolant piping material Z3CN20.09M

被引:11
|
作者
Yu, Weiwei [1 ,2 ]
Fan, Minyu [2 ]
Gao, Hongbo [2 ]
Yu, Dunji [1 ]
Xue, Fei [2 ]
Chen, Xu [1 ]
机构
[1] Tianjin Univ, Sch Chem Engn & Technol, Tianjin 300072, Peoples R China
[2] Suzhou Nucl Power Res Inst, Suzhou 215004, Peoples R China
基金
中国国家自然科学基金;
关键词
Long-term aging; Primary coolant piping; Spinodal decomposition; Fracture toughness; SZW; Critical crack size; STRETCH-ZONE; DUCTILE FRACTURE; STAINLESS-STEELS; BEHAVIOR; RESISTANCE; WELDS;
D O I
10.1016/j.nucengdes.2017.12.022
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
In this study, a series of accelerated thermal aging tests were performed on primary coolant piping materials (Z3CN20.09M) at 400 degrees C for 0, 2000, 5000 and 18,000 h to investigate the resulting microstructure change and fracture toughness. To further assess their fracture toughness, 0.2 mm offset line method and stretch zone width method were both employed to determine the fracture toughness. The results indicated that after long-term thermal aging, round shaped particles and characteristic morphology of spinodal decomposition were found in ferrite, thus resulting in the thermal aging embrittlement of Z3CN20.09M. Subsequently, the J-R curves and J-T curves all decreased significantly with the increasing thermal aging time. Furthermore, the fracture toughness parameters J(50), J(SZW(2D)), J(SZW(3D)) and dJ/d Delta a were first decreased rapidly and then slow saturated. In addition, the J(SZW(2D)) and J(SZW(3D)) values were significantly lower than J(Q) while the reduction of the critical crack size based on J(SZW(2D)) and J(SZW(3D)) parameters was about 30% compared with J(Q), and thus J(SZW) was relatively close to the onset of crack initiation.
引用
收藏
页码:150 / 160
页数:11
相关论文
共 50 条
  • [1] Fracture Toughness of Z3CN20.09M Cast Stainless Steel with Long-Term Thermal Aging
    Yu, Weiwei
    Yu, Dunji
    Gao, Hongbo
    Xue, Fei
    Chen, Xu
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (09) : 4442 - 4449
  • [2] Fracture Toughness of Z3CN20.09M Cast Stainless Steel with Long-Term Thermal Aging
    Weiwei Yu
    Dunji Yu
    Hongbo Gao
    Fei Xue
    Xu Chen
    Journal of Materials Engineering and Performance, 2017, 26 : 4442 - 4449
  • [3] The effect of constraint on fracture properties of Z3CN20.09M after accelerated thermal aging
    Yu, Weiwei
    Liu, Zheng
    Fan, Minyu
    Gao, Hongbo
    Liu, Erwei
    Chen, Mingya
    Xue, Fei
    Chen, Xu
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2021, 190
  • [4] Effect of multiple heat treatments on fracture property of centrifugal casting stainless steels Z3CN20.09M with long-term thermal aging degradation
    Fan, Min-yu
    Jia, Wen-qing
    Yu, Wei-wei
    Wang, Dong-ying
    Guan, Meng
    Cao, Yu
    Xue, Fei
    Liu, Yin-li
    Yao, Jing-wen
    Lin, Bin
    Yu, Ting
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2021, 28 (02) : 223 - 231
  • [5] Effect of multiple heat treatments on fracture property of centrifugal casting stainless steels Z3CN20.09M with long-term thermal aging degradation
    Min-yu Fan
    Wen-qing Jia
    Wei-wei Yu
    Dong-ying Wang
    Meng Guan
    Yu Cao
    Fei Xue
    Yin-li Liu
    Jing-wen Yao
    Bin Lin
    Ting Yu
    Journal of Iron and Steel Research International, 2021, 28 : 223 - 231
  • [6] Thermal aging effect on Z3CN20.09M Cast Duplex Stainless Steel
    Xue, Fei
    Wang, Zhao-Xi
    Shu, Guogang
    Yu, Weiwei
    Shi, Hui-Ji
    Ti, Wenxin
    NUCLEAR ENGINEERING AND DESIGN, 2009, 239 (11) : 2217 - 2223
  • [7] PRECIPITATION BEHAVIOR OF THE INTERMETALLIC PHASES IN Z3CN20.09M STAINLESS STEEL FOR PRIMARY COOLANT PIPES OF NUCLEAR POWER PLANT
    Wang Yongqiang
    Han Jun
    Yang Bin
    Wu Huanchun
    Wang Xitao
    ACTA METALLURGICA SINICA, 2013, 49 (04) : 415 - 420
  • [8] Pitting behavior of thermally aged Z3CN20.09M cast stainless steel for primary coolant pipe of nuclear power plant
    Chen, Yuefeng
    Chen, Bo
    Dong, Fang
    Yang, Bin
    Li, Shilei
    Yu, Xiaoyi
    ENGINEERING FAILURE ANALYSIS, 2018, 83 : 1 - 8
  • [9] EFFECT OF SIGMA PHASE PRECIPITATION ON THE MECHANICAL PROPERTIES OF Z3CN20.09M STAINLESS STEEL USED FOR PRIMARY COOLANT PIPES OF NUCLEAR POWER PLANT
    Yang, Bin
    Wang, Yongqiang
    Han, Jun
    Wu, Huanchun
    PROCEEDINGS OF THE 7TH INTERNATIONAL CONFERENCE ON MECHANICS AND MATERIALS IN DESIGN (M2D2017), 2017, : 1861 - 1862
  • [10] Effect of thermal aging on corrosion fatigue of Z3CN20.09M duplex stainless steel in high temperature water
    Wu, H. C.
    Yang, B.
    Wang, S. L.
    Zhang, M. X.
    Shi, Y. Z.
    Chen, Y. F.
    Sun, Y. H.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 655 : 183 - 192