Characterisation of pre-industrial hybrid cement and effect of pre-curing temperature

被引:48
|
作者
Qu, Bo [1 ,2 ]
Martin, A. [1 ]
Pastor, J. Y. [1 ]
Palomo, A. [2 ]
Fernandez-Jimenez, A. [2 ]
机构
[1] CIME Tech Univ Madrid, Dept Mat Sci, E-28040 Madrid, Spain
[2] Eduardo Torroja Inst Construct Sci CSIC, E-28033 Madrid, Spain
来源
关键词
Hybrid cements; Curing temperature; NMR; C-S-H; SILICATE HYDRATE PHASES; FLY-ASH; ALKALINE ACTIVATION; SLAG; STRENGTH; PASTES; AL-27; SI-29; GEL;
D O I
10.1016/j.cemconcomp.2016.07.019
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
This study aimed to determine the physical-mechanical, mineralogical and microstructural properties of a pre-industrially manufactured hybrid cement (HYC) containing 5% alkaline activator and less than 30% clinker. The effect of the initial curing temperature (25 +/- 1 or 85 degrees C for 20 h) on hydration kinetics and the development of compressive strength were also explored. The hydration products formed were characterised using XRD, SEM/EDX and Al-27 and Si-29 MAS-NMR The findings showed that pre-industrial hybrid cement sets when hydrated with water and hardens to a 28-day mechanical strength of 35 MPa. The main reaction product formed was a mix of cementitious gels: C-(A)-S-H and C-A-S-H. Curing at 85 degrees C for 20 h, shows a behaviour similar to OPC, inhibited ettringite formation and generated more polymerised gels, enhancing 3-day but not 28- or 90-day mechanical strength. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:281 / 288
页数:8
相关论文
共 50 条
  • [1] Effect of pre-curing on thermoplastic-thermoset interphases
    Fisher, Adam
    Radhakrishnan, Arjun
    Levy, Arthur
    Teuwen, Julie
    Kratz, James
    JOURNAL OF COMPOSITE MATERIALS, 2024,
  • [2] DENTIN BONDING - THE EFFECT OF PRE-CURING THE BONDING RESIN
    TODD, SRM
    BRITISH DENTAL JOURNAL, 1994, 177 (02) : 49 - 49
  • [3] DENTIN BONDING - THE EFFECT OF PRE-CURING THE BONDING RESIN
    MCCABE, JF
    RUSBY, S
    BRITISH DENTAL JOURNAL, 1994, 176 (09) : 333 - 336
  • [4] Exploring new pre-curing methods for carbonation curing of cement-based materials
    Liu, Pengfei
    Liu, Chuanbei
    Tang, Kaijing
    Guan, Sumin
    Luo, Xu
    Zhang, Lihua
    Liu, Laibao
    JOURNAL OF BUILDING ENGINEERING, 2025, 105
  • [5] Effects of pre-curing treatment and chemical accelerators on Portland cement mortars at low temperature (5 °C)
    Liu, Zhuangzhuang
    Lou, Baowen
    Barbieri, Diego Maria
    Sha, Aimin
    Ye, Tong
    Li, Yanlong
    CONSTRUCTION AND BUILDING MATERIALS, 2020, 240
  • [6] Effects of pre-curing treatment and chemical accelerators on Portland cement mortars at low temperature (5 °C)
    Liu, Zhuangzhuang
    Lou, Baowen
    Barbieri, Diego Maria
    Sha, Aimin
    Ye, Tong
    Li, Yanlong
    Construction and Building Materials, 2021, 240
  • [7] Properties and effective improvement approaches of basic magnesium sulfate cement under high-temperature pre-curing
    Wu, Chengyou
    Huang, Lei
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 411 (411)
  • [8] Mechanical properties of carbon nanotubes/epoxy nanocomposites: Pre-curing, curing temperature, and cooling rate
    Judawisastra, Hermawan
    Harito, Christian
    Anindyajati, Dika
    Purnama, Hengky
    Abdullah, Akbar Hanif Dawam
    HIGH PERFORMANCE POLYMERS, 2021, 33 (07) : 741 - 750
  • [9] THE PRE-INDUSTRIAL FAMILY
    HOULBROOKE, R
    HISTORY TODAY, 1986, 36 : 49 - 52
  • [10] Pre-Industrial Inequality
    Milanovic, Branko
    Lindert, Peter H.
    Williamson, Jeffrey G.
    ECONOMIC JOURNAL, 2011, 121 (551): : 255 - 272