摘要
The retention of nanometric microstructures is a challenge in any presureless sintering process. Grain size influences mechanical properties and grain coarsening retards densification upon sintering, thus resulting in the poor overall product properties. Hence, it is important to select, among others a suitable sintering regime which promotes densification and retards microstructure coarsening. In this work, Y-TZP ceramic bodies were fabricated under four different sintering regimes to investigate the governance of conventional Single-Stage Sintering (SSS) with 1 min and 2 h dwell time, and comparing their performance with bodies produced by Two-Stage Sintering (TSS). It was revealed that TSS sintered samples, yielded better properties than the SSS samples sintered at 1400 degrees C with a dwell time of 2 hours. In the hydrothermal ageing test, TSS samples did not undergo the low-temperature degradation via the martensitic phase transformation of tetragonal to monoclinic symmetry. Nevertheless, it was found by XRD analysis that Y-TZP ceramics sintered by the SSS method using a short dwell time of 1 minute was effective in maintaining the tetragonal phase stability after 50 hours of exposure in superheated steam conditions.
引用
收藏
页码:81 / 87
页数:7
相关论文
共 50 条
  • [1] EFFECT OF SINTERING PROFILES ON THE PROPERTIES AND AGEING RESISTANCE OF Y-TZP CERAMIC
    Sivakumar, S.
    Ramesh, S.
    Chin, K. L.
    Tan, C. Y.
    Teng, W. D.
    INTERNATIONAL JOURNAL OF AUTOMOTIVE AND MECHANICAL ENGINEERING, 2011, 4 : 405 - 413
  • [2] Ageing and electrical properties of Y-TZP based materials
    Cachadiña, I
    Solier, JD
    Domínguez-Rodríguez, A
    BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 2002, 41 (05): : 437 - 441
  • [3] Prediction of local sintering in laser beam machining of green Y-TZP ceramic
    Ducobu, Francois
    Riviere-Lorphevre, Edouard
    Demarbaix, Anthonin
    Lauwers, Bert
    CIRP ANNALS-MANUFACTURING TECHNOLOGY, 2020, 69 (01) : 225 - 228
  • [4] Adhesion to Y-TZP ceramic: Study of silica nanofilm coating on the surface of Y-TZP
    Druck, Carolina Ceolin
    Pozzobon, Joao Luiz
    Callegari, Gustavo Luiz
    Dorneles, Lucio Strazzabosco
    Valandro, Luiz Felipe
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2015, 103 (01) : 143 - 150
  • [5] Internal friction in Y-TZP ceramic
    Shepel, SV
    Drapkin, BM
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1998, 17 (23) : 1991 - 1993
  • [6] Effect of Air and Argon Sintering Atmospheres on Properties and Hydrothermal Aging Resistance of Y-TZP Ceramics
    Ubenthiran, Sutharsini
    Thanihaichelvan, Murugathas
    Singh, Ramesh
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (07) : 3574 - 3580
  • [7] Effect of Air and Argon Sintering Atmospheres on Properties and Hydrothermal Aging Resistance of Y-TZP Ceramics
    Sutharsini Ubenthiran
    Murugathas Thanihaichelvan
    Ramesh Singh
    Journal of Materials Engineering and Performance, 2018, 27 : 3574 - 3580
  • [8] HEATING AND SINTERING CHARACTERISTICS OF Y-TZP AND Y-TZP/Al2O3 BY MICROWAVE
    施剑林
    田永赉
    李包顺
    郭景坤
    严东生
    Science China Mathematics, 1992, (09) : 1144 - 1152
  • [9] HEATING AND SINTERING CHARACTERISTICS OF Y-TZP AND Y-TZP/AL2O3 BY MICROWAVE
    SHI, JL
    TIAN, YL
    LI, BS
    GUO, JK
    YAN, DS
    SCIENCE IN CHINA SERIES A-MATHEMATICS PHYSICS ASTRONOMY, 1992, 35 (09): : 1144 - 1152
  • [10] Increasing resistance to low temperature ageing degradation of Y-TZP by surface modification
    Feder, A
    Morcillo, P
    Anglada, MJ
    Active Materials, Nanoscale Materials, Composites, Glass and Fundamentals, 2005, 14 : 625 - 634