Fatigue design of welded joints from the wrought magnesium alloy AZ31 by the local stress concept with the fictitious notch radii of rf=1.0 and 0.05 mm

被引:69
|
作者
Karakas, O. [2 ]
Morgenstern, C. [3 ]
Sonsino, C. M. [1 ]
机构
[1] Fraunhofer Inst Struct Durabil & Syst Reliabil LB, D-64289 Darmstadt, Germany
[2] Univ Pamukkale, Fac Engn Sci, Denizli, Turkey
[3] Adam Opel GmbH, Russelsheim, Germany
关键词
Welded joints; Local stress concept; Fictitious radius; Magnesium; Aluminium; Steel;
D O I
10.1016/j.ijfatigue.2008.05.017
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Investigations were carried out with three different types of MIG- and TIG-welded joints of the magnesium alloy AZ31(ISO-MgAl3Zn1): fully or partially penetrated butt welds, transversal stiffeners. The evaluation of the results showed that the local stress concept using the fictitious notch radius of r(f) = 1.0 mm can be applied to magnesium welded joints from plates with thicknesses t >= 5 mm independently of the weld geometries. Design curves are proposed for different stress ratios, i.e. R = -1 as well as 0 and 0.5. which allow the consideration of residual stresses as well as load induced mean-stresses. The results also permit the suggestion of Delta sigma = 28 MPa for r(f) = 1.0 mm as FAT-value in the IIW-Fatigue Design Recommendations. Further, the FAT-value Delta sigma = 73 MPa is also derived for the fictitious radius of r(f) = 0.05 mm to be applied to welded thin magnesium joints (t < 5 mm). These FAT-values are compared with data already known for steel and aluminium joints. A linear relationship between the FAT-values and the Young's modulus is determined. (C) 2008 Elsevier Ltd. All rights reserved.