Inclusion Composition Control During LF Refining for SPCC Using FactSage Combined With Industrial Trials

被引:8
|
作者
Cheng Zi-jian [1 ,2 ]
Guo Jing [1 ]
Cheng Shu-sen [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Met & Ecol Engn, State Key Lab Adv Met, Beijing 100083, Peoples R China
[2] Hongxing Iron & Steel Co Ltd, Jiayuguan 735100, Gansu, Peoples R China
基金
中国国家自然科学基金;
关键词
LF refining; inclusion control; steel-inclusion equilibrium; FactSage; DEOXIDATION EQUILIBRIA;
D O I
10.1016/S1006-706X(13)60050-3
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Steel plate cold common (SPCC) is a Al-killed steel with Ca-treatment. The control of Al2O3 inclusion into low melting point liquid region is beneficial for inclusion removal, cast-ability promotion and defects reduction during rolling. Thus it is essential to understand steel-inclusion equilibrium since inclusion composition is determined by composition of liquid steel directly through steel-inclusion reaction. Thermodynamic calculation software FactSage is performed to understand how to control inclusion composition during ladle furnace (LF) refining, and industrial trials are carried out to verify calculated results. Firstly, target region for controlling CaO-Al2O3-MgO ternary inclusion is analyzed on the basis of the ternary phase diagram and the relationship between activities related to pure solid and activities related to pure liquid was fixed by thermodynamic analysis in order to obtain reliable activities for components of inclusions in the target region by FactSage. In addition, inclusions in steel samples are detected by scanning electron microscopy (SEM) combined with energy dispersive spectroscopy (EDS). It is found that most of Al2O3 inclusions are modified into lower melting point region but a number of them are still located in high melting point region at the end of LF refining after Ca-treatment. Moreover, the composition of liquid steel equilibrating with liquid CaO-Al2O3-MgO inclusion is obtained by steel-inclusion equilibrium calculation when w([Al]s) is approximating 0.03% as: a([O]) is 1. 0 x 10(-6) to 4. 0 x 10(-6), w([Ca]) is 20 x 10(-6) to 50 x 10(-6) and w([Mg]) is 0. 1 x 10(-6) to 3. 0 x 10(-6). At last, stability diagrams of various calcium aluminates and CaS are established and they show that liquid calcium aluminate inclusions form when w([Ca]) is more than 20 x 10(-6), but CaS precipitation is difficult to prevent because sufficiently low w([S]) (<0. 003%) is required.
引用
收藏
页码:14 / 20
页数:7
相关论文
共 40 条
  • [1] Inclusion Composition Control During LF Refining for SPCC Using FactSage Combined With Industrial Trials
    Zi-jian Cheng
    Jing Guo
    Shu-sen Cheng
    Journal of Iron and Steel Research International, 2013, 20 : 14 - 20
  • [2] Inclusion Composition Control During LF Refining for SPCC Using FactSage Combined With Industrial Trials
    CHENG Zi-jian
    GUO Jing
    CHENG Shu-sen
    Journal of Iron and Steel Research(International), 2013, 20 (02) : 14 - 20
  • [3] Modeling Manganese Silicate Inclusion Composition Changes during Ladle Treatment Using FactSage Macros
    Stephano P.T. Piva
    Deepoo Kumar
    P. Chris Pistorius
    Metallurgical and Materials Transactions B, 2017, 48 : 37 - 45
  • [4] Modeling Manganese Silicate Inclusion Composition Changes during Ladle Treatment Using FactSage Macros
    Piva, Stephano P. T.
    Kumar, Deepoo
    Chris Pistorius, P.
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2017, 48 (01): : 37 - 45
  • [5] Effects of Slag Composition and Impurities of Alloys on the Inclusion Transformation during Industrial Ladle Furnace Refining
    Liu, Chunyang
    Jia, Yi
    Hao, Lixia
    Han, Shaowei
    Huang, Fuxiang
    Yu, Huixiang
    Gao, Xu
    Ueda, Shigeru
    Kitamura, Shin-ya
    METALS, 2021, 11 (05)
  • [6] Decarburization treatment and inclusion control during RH refining
    Sun, Qun
    Lin, Yang
    Li, Wei-Dong
    Beijing Keji Daxue Xuebao/Journal of University of Science and Technology Beijing, 2011, 33 (SUPPL. 1): : 142 - 146
  • [7] Inclusion composition control in tyre cord steel by top slag refining
    He, X. F.
    Wang, X. H.
    Chen, S. H.
    Jiang, M.
    Huang, F. X.
    Wang, W. J.
    IRONMAKING & STEELMAKING, 2014, 41 (09) : 676 - 684
  • [9] Top slag refining for inclusion composition transform control in tire cord steel
    Chen, Shu-hao
    Jiang, Min
    He, Xiao-fei
    Wang, Xin-hua
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2012, 19 (06) : 490 - 498
  • [10] Top slag refining for inclusion composition transform control in tire cord steel
    Shu-hao Chen
    Min Jiang
    Xiao-fei He
    Xin-hua Wang
    International Journal of Minerals, Metallurgy, and Materials, 2012, 19 : 490 - 498