Effects of microstructure in high temperature fatigue: Lifetime to crack initiation of a single crystal superalloy in high temperature low cycle fatigue

被引:38
|
作者
Remy, L. [1 ]
Geuffrard, M. [1 ]
Alam, A. [1 ]
Koester, A. [1 ]
Fleury, E. [1 ]
机构
[1] Mines ParisTech, Ctr Mat, CNRS UMR 7633, Evry, France
关键词
High temperature low cycle fatigue; Single crystal superalloy; Damage model; Micro-crack growth; Casting pores; NICKEL-BASE SUPERALLOYS; THERMAL FATIGUE; OXIDATION INTERACTION; IN-100; SUPERALLOY; BEHAVIOR; GROWTH; DAMAGE; ORIENTATION; ALLOY; CREEP;
D O I
10.1016/j.ijfatigue.2012.10.013
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Single crystal superalloys are now the best alloys to make blades and vanes in aero-engines and gas turbines due to their temperature capability, their creep and fatigue resistance. Their composition and microstructure are optimised by heat treatments but low cycle fatigue resistance is mostly controlled by the initiation and early growth of micro-cracks at casting pores. An enriched engineering damage model is proposed to describe micro-crack growth from pores with a process zone concept. Damage equations use summation of contributions on all slip systems as the constitutive model. Oxidation can play a significant role that can be described through embrittled material ahead of micro-crack tip. To investigate the behaviour under small scale yielding at finer scale, experiments were carried out using sharp notches. Early growth of cracks in the notch vicinity was studied at two temperatures 650 degrees C and 950 degrees C. While at the lower temperature the notch can be analysed as a crack, anomalous crack growth rates are observed at the higher temperature. Using finite element computations and a damage model, this behaviour is attributed to local viscoplastic strain concentrations, and oxidation effects. Effects of strain concentration are attenuated since only a small volume of material is highly strained at the notch vicinity. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:37 / 49
页数:13
相关论文
共 50 条
  • [1] Simulation of crack growth under low cycle fatigue at high temperature in a single crystal superalloy
    Kiyak, Y.
    Fedelich, B.
    May, T.
    Pfennig, A.
    [J]. ENGINEERING FRACTURE MECHANICS, 2008, 75 (08) : 2418 - 2443
  • [2] Low-Cycle Fatigue Behavior of a Nickel Base Single Crystal Superalloy at High Temperature
    Shui Li
    Liu Ping
    [J]. RARE METAL MATERIALS AND ENGINEERING, 2015, 44 (02) : 288 - 292
  • [3] High cycle fatigue in a single crystal superalloy: Time dependence at elevated temperature
    Wright, PK
    Jain, M
    Cameron, D
    [J]. Superalloys 2004, 2004, : 657 - 666
  • [4] High-temperature fatigue-creep crack initiation and propagation of a single crystal nickel base superalloy
    Li, SX
    Smith, DJ
    [J]. SIXTH INTERNATIONAL CONFERENCE ON CREEP AND FATIGUE: DESIGN AND LIFE ASSESSMENT AT HIGH TEMPERATURE, 1996, 1996 (02): : 279 - 288
  • [5] Simulation of deformation and lifetime behavior of a fcc single crystal superalloy at high temperature under low-cycle fatigue loading
    Levkovitch, Vladislav
    Sievert, Rainer
    Svendsen, Bob
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2006, 28 (12) : 1791 - 1802
  • [6] Low cycle fatigue behavior of single crystal superalloy with temperature gradient
    Hou, N. X.
    Yu, Q. M.
    Wen, Z. X.
    Yue, Z. F.
    [J]. EUROPEAN JOURNAL OF MECHANICS A-SOLIDS, 2010, 29 (04) : 611 - 618
  • [7] Effects of yttrium on microstructure and low cycle fatigue properties of superalloy IN713C at high temperature
    Li, Qingling
    Zhang, Huarui
    Cheng, Ying
    Sun, Yanyun
    Wang, Fuwei
    Zha, Zichen
    Lin, Junpin
    Zhang, Hu
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2024, 189
  • [8] Crack initiation studies of MA 760 during high temperature low cycle fatigue
    Hynnä, A
    Kuokkala, VT
    Kettunen, P
    [J]. SUPERALLOYS 1996, 1996, : 369 - 374
  • [9] Crack initiation mechanisms during very high cycle fatigue of Ni-based single crystal superalloys at high temperature
    Cervellon, A.
    Hemery, S.
    Kuernsteiner, P.
    Gault, B.
    Kontis, P.
    Cormier, J.
    [J]. ACTA MATERIALIA, 2020, 188 (188) : 131 - 144
  • [10] Effects of secondary orientation on fatigue crack initiation in a single crystal superalloy
    He, Z.
    Qiu, W.
    Fan, Y. -N.
    Han, Q. -N.
    Shi, H. -J.
    Ma, X.
    [J]. FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2018, 41 (04) : 935 - 948