Ceramic firing protocols and thermocycling: effects on the load-bearing capacity under fatigue of a bonded zirconia lithium silicate glass-ceramic

被引:5
|
作者
Diniz, Vandeberg [1 ]
Conde Oliveira Prado, Pedro Henrique [1 ]
Meireles Rodrigues, Jonas Vinicius [1 ]
Monteiro, Jaiane Bandoli [1 ]
Zucuni, Camila [2 ]
Valandro, Luiz Felipe [2 ]
Melo, Renata M. [1 ]
机构
[1] Sao Paulo State Univ UNESP, Inst Sci & Technol, Div Prosthodont, Restorat Dent, Sao Jose Dos Campos, Brazil
[2] Univ Fed Santa Maria, Fac Odontol, Div Prosthodont, Oral Sci, Santa Maria, RS, Brazil
关键词
Glass ceramics; Crystallization; Aging; Fatigue; MECHANICAL-PROPERTIES; LUTING AGENT; Y-TZP; STRENGTH; SURFACE; RESIN; RESTORATIONS; DISILICATE; LEUCITE; IMPACT;
D O I
10.1016/j.jmbbm.2020.103963
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
This study evaluated the effect of different firing processes (without firing, additional crystallization and glaze firing) and thermal-cycling (with or without) on the fatigue behavior of simplified zirconia-lithium silicate (ZLS) glass ceramic restorations cemented to a dentin-like material. Materials and Methods. One hundred twenty-nine (129) discs (diameter = 12 mm and thickness = 1.2 mm) of ZLS (Celtra Duo, Dentsply Sirona) and fiber reinforced epoxy resin (diameter = 12 mm and thickness = 2.3 mm) were produced and tested under fatigue according to 2 study factors: a firing protocol with 3 levels (without firing, additional crystallization and glaze firing) and thermocycling of 2 levels (absence/presence), composing 6 study groups. Ceramic and epoxy resin discs had their surfaces treated and adhesive cementation was performed (Multilink N, Ivoclar). Half of the samples were immediately tested; the other half were subjected to thermal-cycling (10,000 cycles in water; 5-55 degrees C). The staircase method determined the fatigue failure load (100,000 cycles at a frequency of 20 Hz). The fatigue data (in N) were submitted to 2-way ANOVA and Bonferroni test (p < 0.05). Fractographic analyses were also carried out. Thermocycling decreased the fatigue failure load (FFL) of all groups when compared to those without aging. Bonferroni's test indicated that the groups with crystallization/glazing process behaved better in terms of FFL than those without firing in the same storage condition. All the samples had radial cracks and all fractures originated from defects on the cementation surface of the ceramic discs. Crystallization and glaze firing had a positive effect on the fatigue failure load of adhesively cemented ZLS glass ceramic compared to the group without crystallization firing, in both storage conditions (with or without thermocycling).
引用
收藏
页数:6
相关论文
共 50 条
  • [1] Adhesive application after ceramic surface treatment is detrimental to load-bearing capacity under fatigue of a lithium disilicate glass-ceramic
    Velho, Helder Callegaro
    da Rosa, Lucas Saldanha
    Temp, Renatta Wrasse
    Cocco, Fernanda Maidana
    Pereira, Gabriel Kalil Rocha
    May, Liliana Gressler
    Valandro, Luiz Felipe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2022, 135
  • [2] Grinding and polishing of the inner surface of monolithic simplified restorations made of zirconia polycrystals and lithium disilicate glass-ceramic: Effects on the load-bearing capacity under fatigue of the bonded restorations
    Cadore-Rodrigues, Ana Carolina
    Machry, Renan Vaz
    Zucuni, Camila Pauleski
    Pereira, Gabriel Kalil Rocha
    Valandro, Luiz Felipe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2021, 124
  • [3] Weak adhesion between ceramic and resin cement impairs the load-bearing capacity under fatigue of lithium disilicate glass-ceramic crowns
    da Rosa, Lucas Saldanha
    Velho, Helder Callegaro
    Tribst, Joao Paulo Mendes
    Valandro, Luiz Felipe
    Kleverlaan, Cornelis Johannes
    Pereira, Gabriel Kalil Rocha
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2023, 138
  • [4] Mechanical properties of zirconia reinforced lithium silicate glass-ceramic
    Elsaka, Shaymaa E.
    Elnaghy, Amr M.
    DENTAL MATERIALS, 2016, 32 (07) : 908 - 914
  • [5] One-step ceramic primer as surface conditioner: Effect on the load-bearing capacity under fatigue of bonded lithium disilicate ceramic simplified restorations
    Dapieve, Kiara Serafini
    Machry, Renan Vaz
    Pilecco, Rafaela Oliveira
    Kleverlaan, Cornelis Johannes
    Rocha Pereira, Gabriel Kalil
    Venturini, Andressa Bonin
    Valandro, Luiz Felipe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2020, 104
  • [6] CRYSTALLIZATION OF A LITHIUM SILICATE GLASS-CERAMIC UNDER PRESSURE
    JOHNSON, SM
    LAMOREAU, RH
    LOEHMAN, RE
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1995, 78 (04) : 1115 - 1117
  • [7] Ceramic surface conditioning, resin cement viscosity, and aging relationships affect the load-bearing capacity under fatigue of bonded glass-ceramics
    Dapieve, Kiara Serafini
    Velho, Helder Callegaro
    da Rosa, Lucas Saldanha
    Pivetta, Jordana Pavanelo
    Maidana, Fernanda Cocco
    Venturini, Andressa Borin
    Kleverlaan, Cornelis Johannes
    Pereira, Gabriel Kalil Rocha
    Valandro, Luiz Felipe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2023, 139
  • [8] Fatigue Failure Load of Resin-bonded Simplified Lithium Disilicate Glass-Ceramic Restorations: Effect of Ceramic Conditioning Methods
    Mendes Tribst, Joao Paulo
    Monteiro, Jaiane Bandoli
    Venturini, Andressa Borin
    Rocha Pereira, Gabriel Kalil
    Bottino, Marco Antonio
    de Melo, Renata Marques
    Valandro, Luiz Felipe
    JOURNAL OF ADHESIVE DENTISTRY, 2019, 21 (04): : 373 - 381
  • [9] Effects of contact-stress on wear behavior of zirconia-reinforced lithium silicate glass-ceramic
    Yilmaz, Efe Cetin
    Sadeler, Recep
    BIOMEDICAL AND BIOTECHNOLOGY RESEARCH JOURNAL, 2020, 4 (01): : 51 - 54
  • [10] Fatigue failure load of two resin-bonded zirconia-reinforced lithium silicate glass-ceramics: Effect of ceramic thickness
    Monteiro, Jaiane Bandoli
    Riquieri, Hilton
    Prochnow, Catina
    Guilardi, Luis Felipe
    Rocha Pereira, Gabriel Kalil
    Souto Borges, Alexandre Luiz
    de Melo, Renata Marques
    Valandro, Luiz Felipe
    DENTAL MATERIALS, 2018, 34 (06) : 891 - 900