Optical properties of gold-dispersed barium titanate thin films prepared by sol-gel processing

被引:25
|
作者
Otsuki, S [1 ]
Nishio, K
Kineri, T
Watanabe, Y
Tsuchiya, T
机构
[1] Sci Univ Tokyo, Dept Mat Sci & Technol, Noda, Chiba 278, Japan
[2] TDK Corp, R&D Ctr, Ichikawashi, Chiba 272, Japan
关键词
D O I
10.1111/j.1151-2916.1999.tb01985.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Gold-dispersed BaTiO3 thin films were prepared by the sol-gel process using spin coating, after which the effects of the gold particle size and shape on nonlinear optical properties were investigated. The BaTiO3 matrix was amorphous up to 500 degrees C. Polycrystalline BaTiO3 thin films were obtained by heating at 650 degrees C for 1 h, The mean gold particle size, which was calculated from the Au(111) diffraction peak according to Scherrer's formula, was similar to 8-10 nm in the range of 300 degrees to 550 degrees C, but rapidly increased thereafter with increasing temperature up to 650 degrees C. From 650 degrees to 800 degrees C, however, particle size was almost constant at similar to 16 nm, For those gold particles heated to 500 degrees C, the particlesize distribution was small and centered at similar to 10 nm, However, for gold particles heated at 650 degrees C, a broad particlesize distribution ranging from 10 to 100 nm could he observed in the BaTiO3 thin films from TEM observation. The peak position of the surface plasmon resonance of the gold particles shifted to a longer wavelength as temperature increased, An absorption peak position was calculated that was In very good agreement with Maxwell-Garnet (MG) theory, using the dielectric constant of the gold particles by Kreibig theory to calculate the absorption coefficient, a, of each distribution teach 2.5 nm) of the gold particle size, and these values were then averaged. BaTiO3 thin films heat-treated at 650 degrees C for 1 h exhibited third-order optical nonlinear susceptibility values (chi((3))) Of 1.09 x 10(-6) esu and chi((3))/alpha = 4.31 x 10(-11) esu cm at a wavelength of 532 nm, The values of chi((3))/alpha of gold-dispersed BaTiO3 thin films were 10 times larger than those of gold-dispersed SiO2 thin films.
引用
收藏
页码:1676 / 1680
页数:5
相关论文
共 50 条
  • [1] Preparation and optical properties of gold-dispersed (Pb, La)TiO3 thin films by sol-gel process
    Sei, T
    Takatou, N
    Kineri, T
    Tsuchiya, T
    MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 1997, 49 (01): : 61 - 65
  • [2] Study on microstructure and ferroelectricity of strontium barium titanate thin films prepared by Sol-Gel processing
    Shan, Lian-wei
    Wang, Lai-guo
    Li, Wei
    Dong, Li-min
    Han, Zhi-dong
    Wu, Ze
    Fu, Xing-hua
    Hou, Wen-ping
    CHINA FUNCTIONAL MATERIALS TECHNOLOGY AND INDUSTRY FORUM, 2013, 320 : 202 - +
  • [3] Sol-gel processing and properties of cerium doped barium strontium titanate thin films
    Sedlar, M
    Sayer, M
    Weaver, L
    JOURNAL OF SOL-GEL SCIENCE AND TECHNOLOGY, 1995, 5 (03) : 201 - 210
  • [4] Processing and dielectric property evaluation of barium strontium titanate thin films prepared by a sol-gel technique
    Tahan, DM
    Klein, LC
    Safari, A
    ISAF '96 - PROCEEDINGS OF THE TENTH IEEE INTERNATIONAL SYMPOSIUM ON APPLICATIONS OF FERROELECTRICS, VOLS 1 AND 2, 1996, : 483 - 486
  • [5] Sol-gel processed barium titanate thin films
    Sharma, HB
    Mansingh, A
    FERROELECTRICS LETTERS SECTION, 1997, 22 (3-4) : 75 - 82
  • [6] Effects of Nd-doping on optical and photovoltaic properties of barium titanate thin films prepared by sol-gel method
    Jiang, Weihai
    Cai, Wei
    Lin, Zebin
    Fu, Chunlin
    MATERIALS RESEARCH BULLETIN, 2013, 48 (09) : 3092 - 3097
  • [7] Hydrothermal processing of barium strontium titanate sol-gel composite thin films
    Zelonka, K.
    Sayer, M.
    Freundorfer, A. P.
    Hadermann, J.
    JOURNAL OF MATERIALS SCIENCE, 2006, 41 (12) : 3885 - 3897
  • [8] STRONTIUM-BARIUM-TITANATE THIN-FILMS BY SOL-GEL PROCESSING
    NAZERI, A
    KAHN, M
    KIDD, T
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1995, 14 (15) : 1085 - 1088
  • [9] Hydrothermal processing of barium strontium titanate sol-gel composite thin films
    K. Zelonka
    M. Sayer
    A. P. Freundorfer
    J. Hadermann
    Journal of Materials Science, 2006, 41 : 3885 - 3897
  • [10] Gold-particle-enhanced crystallite growth of thin films of barium titanate prepared by the sol-gel process
    Masaki, Y
    Koutzarov, IP
    Ruda, HE
    Farrell, M
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1998, 81 (04) : 1074 - 1076