Investigation of intergranular penetration behavior in CrMnFeCoNi HEA/304 SS dissimilar brazing joints

被引:25
|
作者
Wang, Ge [1 ]
Sheng, Guangmin [1 ]
Yu, Qili [1 ]
Yuan, Xinjian [1 ]
Sun, Jianchun [2 ]
Jiao, Yingjun [1 ]
Zhang, Yuntao [1 ]
机构
[1] Chongqing Univ, Coll Mat Sci & Engn, 174 Shazheng St, Chongqing 400044, Peoples R China
[2] Chongqing Univ Sci & Technol, Coll Mat Sci & Engn, 20 Daxuechengdong Rd, Chongqing 401331, Peoples R China
关键词
Brazing; Diffusion; Dissimilar joint; High-entropy alloy; Intergranular penetration; Stainless steel; HIGH-ENTROPY ALLOY; MECHANICAL-PROPERTIES; STAINLESS-STEEL; MICROSTRUCTURE; EVOLUTION; DIFFUSION; WELDABILITY; STABILITY; STRENGTH; TITANIUM;
D O I
10.1016/j.intermet.2020.106940
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
As-rolled and annealed CrMnFeCoNi high-entropy alloys (HEAs) were selected to braze 304 SS by using Ag50Cu as the filler metal (FM) in a vacuum furnace. Intergranular penetration was detected in each joint. To explore the evolvement mechanism of microstructure and performance, three different series of dissimilar joints were prepared and the microstructure and mechanical properties of the dissimilar joints were observed and tested. The penetration of liquid FM into the grain boundaries (GBs) of HEA was attributed to the imbalance between GB energy and solid-liquid interface energy. Intergranular penetration accelerated interdiffusion between FM and HEA, and diffusion induced further penetration. The mechanism of interdiffusion was studied, and the effects of brazing temperature, Ag50Cu content and Mn concentration in HEA on atomic immigration during brazing were discussed. Intergranular penetration inhibited grain growth in the penetration zone (PZ) of HEA. The physical difference between HEA and penetration phase generated residual stress. A layer of sigma (Cr, Fe) phase formed at the 304 SS/FM interfaces, and increased the embrittlement of the dissimilar joints brazed at high temperatures. However, the tensile strength of the joints is improved by the immigration of a huge amount of Mn (a solution-strengthened element of Ag-Cu alloy) into FM and the increasing contact area induced by penetration. The tensile strength of 304 SS and the as-rolled HEA reached 434.7 MPa, which is higher than that of the joint brazed using BNi2. The annealed HEA processed low GB density and low driving force for grain growth, decreasing the difference in grain sizes in PZ, reducing penetration and ensuring interdiffusion between HEA and FM. The tensile strength of the joint of annealed HEA reached 487.1 MPa, indicating that controlling parameters of brazing and changing conditions of HEA are effective to reduce penetration.
引用
收藏
页数:12
相关论文
共 50 条
  • [1] Mechanical properties and microstructure evolution of CrMnFeCoNi HEA/304 SS dissimilar brazing joints
    Wang, Ge
    Sheng, Guangmin
    Sun, Jianchun
    Wei, Yu
    Gao, Xianhui
    Yu, Zhe
    Yuan, Xinjian
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 829
  • [2] Numerical modelling and experimental investigation of diffusion brazing SS304/BNi-2/SS304 joint
    Chen, H.
    Gong, J-M.
    Tu, S-T.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2009, 14 (01) : 32 - 41
  • [3] Investigation of mechanical properties of microwave welded SS304-SS202 lap joints
    Samyal, Rahul
    Bedi, Raman
    Bagha, Ashok Kumar
    PHYSICA SCRIPTA, 2023, 98 (02)
  • [4] Investigation on regulating inter-granular penetration in CoCrMnFeNi high-entropy alloy and 304 stainless steel dissimilar joints
    Wang, Ge
    Sheng, Guangmin
    Yu, Qili
    Sun, Jianchun
    Li, Rui
    Yuan, Xinjian
    Zhang, Yuntao
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 800
  • [5] Optimization and influence of process parameters of dissimilar SS304L-SS430 joints produced by Robotic TIG welding
    Ramana, M. Venkata
    Kumar, B. V. R. Ravi
    Krishna, M.
    Rao, M. Venkateshwar
    Kumar, V. S.
    MATERIALS TODAY-PROCEEDINGS, 2020, 23 : 479 - 482
  • [6] Microstructure investigation and fracture mechanism of TC4-304L dissimilar joints fabricated by the cold metal transfer arc-brazing method
    Mou, Gang
    Zheng, Kaikui
    Shen, Chen
    Xiang, Hongliang
    Hua, Xueming
    He, Lun
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 15 : 6758 - 6768
  • [7] Study on the microstructure optimization and mechanical properties of dissimilar TC4-304L arc-brazing joints
    Mou, Gang
    Hua, Xueming
    Huang, Ye
    Shen, Chen
    Wang, Min
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 788 (788):
  • [8] Investigation on mechanical behavior of clinched joints produced with dissimilar dies
    Ren, Xiaoqiang
    Chen, Chao
    Peng, Hao
    Zhang, Huiyang
    Li, Haijun
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART B-JOURNAL OF ENGINEERING MANUFACTURE, 2023, 237 (1-2) : 31 - 42
  • [9] Microstructure evolution and corrosion behavior of dissimilar 304/430 stainless steel welded joints
    Wang, Caimei
    Yu, Yang
    Yu, Jianxing
    Zhang, Yu
    Zhao, Yan
    Yuan, Qiwei
    JOURNAL OF MANUFACTURING PROCESSES, 2020, 50 (50) : 183 - 191
  • [10] Investigating on the macroscopic morphology, microstructure and mechanical properties of Al0.3CoCrFeNi-HEA/304 stainless steel dissimilar welded joints
    Sui, Xinchen
    Zhao, Xiaohui
    Ren, Boqiao
    Chen, Yunhao
    Gao, Yihao
    Chen, Chao
    Hu, Chunhua
    CIRP JOURNAL OF MANUFACTURING SCIENCE AND TECHNOLOGY, 2024, 52 : 86 - 99