摘要
Considerable improvement in the impact toughness of an annealed polypropylene (PP) nanocomposite containing CaCO3 nanoparticles was achieved and its toughening mechanism was investigated. The nanocomposite was prepared by melt-blending PP and CaCO3 nanoparticles in a batch mixer. Injection-modeled impact and tensile bars were annealed at 150 degrees C for 2 h prior to the impact and tensile tests. The Young modulus and yield stress of the nanocomposite were found to increase after annealing. What is more, the annealed nanocomposite had much higher impact toughness than its unannealed counterpart. The average Izod impact strength of the 150 degrees C-annealed nanocomposite, containing 20 wt % (7.8 vol %) CaCO3 nanoparticles coated with 6 wt % stearic acid, was 168 J/m, which was 3.5 times higher than that of neat PP. Experiments, including X-ray diffraction, differential scanning calorimetry, scanning electron microscopy (SEM) and the instrumented falling-weight impact test, were performed to study the toughening mechanism of the annealed nanocomposite. SEM micrographs of the impact fracture surface and bulk morphology underneath the fracture surface of the broken Izod samples and the results of the instrumented failing-weight impact test suggested that the plastic deformation zone that formed in the crack-initiation stage was responsible for the high impact toughness of the annealed nanocomposite. The micromorphology ahead of the arrested crack tip of the annealed nanocomposite showed that the propagation of the crack occurred through shear-to-rupture of the ligaments at the crack opening. The size of the plastic deformation zone and the fracture energy were likely related to the increased matrix ligament strength after annealing. In summary, the annealing-rein forced ligaments were proposed to be responsible for the high impact toughness of the annealed nanocomposite.
引用
收藏
页码:9204 / 9213
页数:10
相关论文
共 50 条
  • [1] Annealing-induced high impact toughness of polypropylene/CaCO3 nanocomposites
    Lin, Yong
    Chen, Haibin
    Chan, Chi-Ming
    Wu, Jingshen
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2012, 124 (01) : 77 - 86
  • [2] Effects of surface modification of the filler on the impact toughness of polypropylene/CaCO3 nanocomposites
    Yong, Lin
    Chen, Haibin
    Chan, Chi-Ming
    Wu, Jingshen
    [J]. ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2009, 237
  • [3] Effects of coating amount and particle concentration on the impact toughness of polypropylene/CaCO3 nanocomposites
    Lin, Yong
    Chen, Haibin
    Chan, Chi-Ming
    Wu, Jingshen
    [J]. EUROPEAN POLYMER JOURNAL, 2011, 47 (03) : 294 - 304
  • [4] Toughening of isotactic polypropylene with CaCO3 particles
    Thio, YS
    Argon, AS
    Cohen, RE
    Weinberg, M
    [J]. POLYMER, 2002, 43 (13) : 3661 - 3674
  • [5] Influence of Strain Rate on the Toughening Effect of CaCO3 in Polypropylene/CaCO3 Composites
    Zebarjad, Seyyed Mojtaba
    Golmakaniyoon, Sahar
    [J]. JOURNAL OF VINYL & ADDITIVE TECHNOLOGY, 2013, 19 (04): : 271 - 275
  • [6] Crystallization and impact energy of polypropylene/CaCO3 nanocomposites with nonionic modifier
    Zhang, QX
    Yu, ZZ
    Xie, XL
    Mai, YW
    [J]. POLYMER, 2004, 45 (17) : 5985 - 5994
  • [7] Thermomechanical Properties of Virgin and Recycled Polypropylene Impact Copolymer/CaCO3 Nanocomposites
    Elloumi, A.
    Pimbert, S.
    Bourmaud, A.
    Bradai, C.
    [J]. POLYMER ENGINEERING AND SCIENCE, 2010, 50 (10): : 1904 - 1913
  • [8] Synergistic effects of toughening of nano-CaCO3 and toughness of β-polypropylene
    Zhang, Zishou
    Wang, Chunguang
    Meng, Yuezhong
    Mai, Kancheng
    [J]. COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2012, 43 (01) : 189 - 197
  • [9] Sequences of Fracture Toughness Micromechanisms in PP/CaCO3 Nanocomposites
    Khosh, R. Lesan
    Bagheri, R.
    Zokaei, S.
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2008, 110 (06) : 4040 - 4048
  • [10] Crystallization, shrinkage and mechanical characteristics of polypropylene/CaCO3 nanocomposites
    Shelesh-Nezhad, Karim
    Orang, Hamed
    Motallebi, Mahdi
    [J]. JOURNAL OF THERMOPLASTIC COMPOSITE MATERIALS, 2013, 26 (04) : 544 - 554