Ambient curable latex films and adhesives based on natural rubber bearing Acetoacetoxy functionality

被引:10
|
作者
Ninjan, Rattanawadee [1 ]
Thongnuanchan, Bencha [1 ]
Lopattananon, Natinee [1 ]
Thitithammawong, Anoma [1 ]
Nakason, Charoen [2 ]
机构
[1] Prince Songkla Univ, Fac Sci & Technol, Dept Rubber Technol & Polymer Sci, Pattani 94000, Thailand
[2] Prince Songkla Univ, Fac Sci & Ind Technol, Surat Thani, Thailand
关键词
acetoacetoxyethyl methacrylate; adhesive; graft copolymers; natural rubber; CROSS-LINKING;
D O I
10.1002/pat.4496
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The study described in this paper first demonstrates that a newly modified form of natural rubber, namely graft copolymers of natural rubber with poly (acetoacetoxyethyl methacrylate), NR-g-PAAEM, is able to undergo a cross-linking reaction at room temperature by reaction with a water dispersible polyisocyanate based on hexamethylene diisocyanate (poly-HDI). Attenuated total reflectance Fourier transform infrared (ATR-FTIR) analysis indicated that amide groups were formed by the reaction of the acetoacetyl groups (AcAc) present in the grafted poly (acetoacetoxyethyl methacrylate) (PAAEM) chains with the poly-HDI. This observation was accompanied by a noticeable increase in the tensile strength of the NR-g-PAAEM latex films when adding poly-HDI to the latex prior to film formation. DMTA analyses also revealed a shift in the tan delta peaks, corresponding to the transitions of both NR-g-PAAEM and free PAAEM phases, to higher temperatures. These results provide firm evidence of cross-linking between NR-g-PAAEM chains by reaction with poly-HDI during film formation under ambient conditions. Adhesives for bonding wood to wood based on the NR-g-PAAEM latex were then prepared, using poly-HDI as the cross-linker. The lap shear strength of the resulting adhesives exhibited a maximum value of 2657 KPa when a poly-HDI:AAEM molar ratio of 3:1 was employed. It was also observed that the adhesive attained about approximately 89% of the highest lap shear strength after it was allowed to set at 30 degrees C for 24 hours. Hence, the use of poly-HDI in cross-linking NR particles bearing grafted PAAEM offers great potential for developing latex adhesives and coatings capable of curing under ambient conditions.
引用
收藏
页码:598 / 607
页数:10
相关论文
共 50 条
  • [1] Acetoacetoxy functionalized natural rubber latex capable of forming cross-linkable film under ambient conditions
    Thongnuanchan, Bencha
    Ninjan, Rattanawadee
    Nakason, Charoen
    IRANIAN POLYMER JOURNAL, 2017, 26 (01) : 41 - 53
  • [2] Acetoacetoxy functionalized natural rubber latex capable of forming cross-linkable film under ambient conditions
    Bencha Thongnuanchan
    Rattanawadee Ninjan
    Charoen Nakason
    Iranian Polymer Journal, 2017, 26 : 41 - 53
  • [3] Natural rubber latex-based adhesives: role of nanofillers
    Shybi, A. A.
    Varghese, Siby
    Thomas, Sabu
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2021, 35 (04) : 406 - 418
  • [4] Ambient curable natural rubber latex adhesive cross-linked with polymeric isocyanate for bonding wood
    Muhammad Adly Rahandi Lubis
    Fahriya Puspita Sari
    Raden Permana Budi Laksana
    Widya Fatriasari
    Euis Hermiati
    Polymer Bulletin, 2022, 79 : 6745 - 6757
  • [5] Ambient curable natural rubber latex adhesive cross-linked with polymeric isocyanate for bonding wood
    Lubis, Muhammad Adly Rahandi
    Sari, Fahriya Puspita
    Laksana, Raden Permana Budi
    Fatriasari, Widya
    Hermiati, Euis
    POLYMER BULLETIN, 2022, 79 (08) : 6745 - 6757
  • [6] Physical-Mechanical Characterization of Epoxidized Natural Rubber Films Curable at Ambient Temperature
    Jorge, Rosane M.
    Ferreira, Marcos T.
    Picciani, Paulo H. S.
    Gomes, Ailton S.
    Nunes, Regina C. R.
    POLIMEROS-CIENCIA E TECNOLOGIA, 2009, 19 (04): : 329 - 335
  • [7] Studies on wood-to-wood bonding adhesives based on natural rubber latex
    John, N
    Joseph, R
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 1997, 11 (02) : 225 - 232
  • [8] Formation and crosslinking of latex films through the reaction of acetoacetoxy groups with diamines under ambient conditions
    Feng, JR
    Pham, H
    Macdonald, P
    Winnik, MA
    Geurts, JM
    Zirkzee, H
    van Es, S
    German, AL
    JOURNAL OF COATINGS TECHNOLOGY, 1998, 70 (881): : 57 - 68
  • [9] The microstructure of natural rubber latex films
    Cook, S
    Cudby, PEF
    Davies, RT
    Morris, MD
    RUBBER CHEMISTRY AND TECHNOLOGY, 1997, 70 (04): : 549 - 559
  • [10] Studies on the ambient temperature crosslinking of latex films based on natural rubber grafted with poly(diacetone acrylamide) using DMTA
    Bencha Thongnuanchan
    Rattanawadee Ninjan
    Azizon Kaesaman
    Charoen Nakason
    Journal of Polymer Research, 2015, 22