Pyrolysis of wood-PVC mixtures. Formation of chloromethane from lignocellulosic materials in the presence of PVC

被引:43
|
作者
Czegeny, Zsuzsanna [1 ]
Jakab, Emma [1 ]
Bozi, Janos [1 ]
Blazso, Marianne [1 ]
机构
[1] Hungarian Acad Sci, Inst Mat & Environm Chem, Res Ctr Nat Sci, H-1117 Budapest, Hungary
关键词
Pyrolysis; PVC; Biomass; Chloromethane; THERMAL-DECOMPOSITION; CO-PYROLYSIS; POLY(VINYL CHLORIDE); CELLULOSE; PRODUCTS; DEGRADATION;
D O I
10.1016/j.jaap.2014.11.016
中图分类号
O65 [分析化学];
学科分类号
070302 ; 081704 ;
摘要
Thermal decomposition of polyvinylchloride (PVC)-wood and wood component mixtures were examined under slow and fast heating by pyrolysis-gas chromatography/mass spectrometry (Py-GC/MS) and thermogravimetry/mass spectrometry(TG/MS) techniques in order to clarify the chemical interaction of biomass materials and PVC during thermal decomposition. A hardwood and a softwood (beech and pine), their lignin and two types of cellulose (Avicel and Whatman) were chosen as natural polymer components. Comparing the gaseous and liquid pyrolysis products of pure samples to those of mixtures it was found that considerably lower amount of several reactive compounds have been produced when the biomass sample was mixed with PVC. On the other hand significant amount of chloromethane appeared in the pyrolysate of wood and lignin samples mixed with PVC under fast and slow pyrolysis conditions as well, but only in traces of chlorinated organic compounds were detected from cellulose mixtures. It was concluded that the methoxy groups at phenolic rings in lignin are the methyl source of chloromethane formation, and this reaction consumed most of the HCl evolved from PVC. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:123 / 132
页数:10
相关论文
共 7 条
  • [1] Pyrolysis of wood and PVC mixtures: thermal behaviour and kinetic modelling
    Ephraim, Augustina
    Pozzobon, Victor
    Lebonnois, Damien
    Peregrina, Carlos
    Sharrock, Patrick
    Nzihou, Ange
    Minh, Doan Pham
    BIOMASS CONVERSION AND BIOREFINERY, 2023, 13 (10) : 8669 - 8683
  • [2] Pyrolysis of wood and PVC mixtures: thermal behaviour and kinetic modelling
    Augustina Ephraim
    Victor Pozzobon
    Damien Lebonnois
    Carlos Peregrina
    Patrick Sharrock
    Ange Nzihou
    Doan Pham Minh
    Biomass Conversion and Biorefinery, 2023, 13 : 8669 - 8683
  • [3] Pyrolysis and combustion of PVC, PVC-wood and PVC-coal mixtures in a two-stage fluidized bed process
    Saeed, L
    Tohka, A
    Haapala, M
    Zevenhoven, R
    FUEL PROCESSING TECHNOLOGY, 2004, 85 (14) : 1565 - 1583
  • [4] Formation of aromatics during pyrolysis of PVC in the presence of metal chlorides
    Muller, J
    Dongmann, G
    JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 1998, 45 (01) : 59 - 74
  • [5] PVC-alkaline earth metal carbonates mixtures. I. PVC thermodegradation in the presence of alkaline earth metal carbonates
    Cailean, A
    Rosca, I
    Sutiman, D
    Cretescu, I
    Vizitiu, M
    Sibiescu, D
    MATERIALE PLASTICE, 2001, 38 (01) : 45 - 51
  • [6] Effects of torrefaction on the formation and distribution of dioxins during wood and PVC pyrolysis: An experimental and mechanistic study
    Han, Zixi
    Li, Jian
    Gu, Tianbao
    Yang, Ruilei
    Fu, Zhufu
    Yan, Beibei
    Chen, Guanyi
    JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2021, 157
  • [7] FORMATION OF MONO(ETHYLHEXYL)PHTHALATE FROM DI(ETHYLHEXYL)PHTHALATE IN HUMAN-PLASMA STORED IN PVC BAGS AND ITS PRESENCE IN FRACTIONATED PLASMA-PROTEINS
    VESSMAN, J
    RIETZ, G
    VOX SANGUINIS, 1978, 35 (1-2) : 75 - 80