Effect of joining temperature and holding time on microstructure and shear strength of Ti2AlC/Cu joints brazed using Ag-Cu filler alloy

被引:26
|
作者
Zhang, J. [1 ]
Wang, G. C. [1 ]
Hea, Y. M. [1 ]
Sun, Y. [1 ]
He, X. D. [2 ]
机构
[1] Harbin Inst Technol, State Key Lab Adv Welding & Joining, Harbin 150001, Peoples R China
[2] Harbin Inst Technol, Ctr Composite Mat & Struct, Harbin 150080, Peoples R China
关键词
Ti2AlC ceramic; Copper; brazing; Shear strength; TIAL-BASED INTERMETALLICS; INTERFACIAL MICROSTRUCTURE; MECHANICAL-PROPERTIES; STEEL; 35CRMO; INTERLAYER; OXIDATION; CERAMICS; TI3ALC2; PHASES; METAL;
D O I
10.1016/j.msea.2012.12.037
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The present study investigated the effect of brazing temperature and holding time on the microstructure and mechanical properties of Ti2AlC-copper joints brazed with Ag-Cu filler alloy at 800-900 degrees C for 10 min and held for different times at 850 degrees C. The representative structure of the joints was Ti2AlC/interaction area in the Ti2AlC substrate/brazing layer/diffusion area of the copper substrates/Cu. The brazing layer was composed of Cu-rich phases, AlCu2Ti intermetallic compounds and Ag[Cu] solid solutions. With increasing brazing temperature, more filler alloy was infiltrated into the ceramic substrate and reacted with Ti2AlC, accelerating the decomposition of Ti2AlC and the formation of Ti3AlC2, TiC and AlCu2Ti reaction phases. Moreover, more copper substrate was dissolved into the filler alloy; thus, more Cu-rich phase and AlCu2Ti were produced in the brazing layer. Moreover, the width of the brazing layer was reduced, while the widths of both the interaction area and diffusion area increased. As the brazing temperature was increased, the shear joint strength increased and then decreased. By prolonging the holding time, the widths of both the interaction area and the diffusion area were increased, while the width of the brazing layer was held constant at approximately 50 mu m. Neither the structure nor the shear strength of the joints was influenced by the holding time. The optimum brazing parameters for joining Ti2AlC ceramic to copper with Ag-Cu filler alloy were 850 degrees C for 40 min. The joints obtained exhibit a maximum shear strength of 203.3 MPa. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:58 / 64
页数:7
相关论文
共 50 条
  • [1] Characterizing the Decomposition of Ti2AlC during its Brazing with Cu by Using Ag-Cu Filler Alloy
    Wang, Guochao
    Zhang, Jie
    Liu, Xiaowen
    PHYSICAL AND NUMERICAL SIMULATION OF MATERIALS PROCESSING VII, 2013, 762 : 607 - +
  • [2] Effect of Sn Content on the Microstructure, Mechanical and Electrical Properties of Ti2AlC/Cu Joints Brazed with Cu-Sn-Ti Filler Alloy
    Zhang, Jie
    Wang, Guochao
    Zheng, Yi
    PHYSICAL AND NUMERICAL SIMULATION OF MATERIALS PROCESSING VII, 2013, 762 : 602 - +
  • [3] Effect of holding time on microstructure and mechanical properties of ZrO2/TiAl joints brazed by Ag-Cu filler metal
    Dai, Xiangyu
    Cao, Jian
    Liu, Jiakun
    Su, Shuai
    Feng, Jicai
    MATERIALS & DESIGN, 2015, 87 : 53 - 59
  • [4] Microstructure of reaction layer and its effect on the joining strength of SiC/SiC joints brazed using Ag-Cu-In-Ti alloy
    Liu, Yan
    Zhu, Yunzhou
    Yang, Yong
    Liu, Xuejian
    Huang, Zhengren
    JOURNAL OF ADVANCED CERAMICS, 2014, 3 (01) : 71 - 75
  • [5] Microstructure evolution and joining strength of diamond brazed on Ti-6Al-4V substrates using Ti-free eutectic Ag-Cu filler alloy
    Liao, Xinjiang
    Liu, Zhuo
    Liu, Ruixiang
    Mu, Dekui
    DIAMOND AND RELATED MATERIALS, 2022, 127
  • [6] Microstructure evolution and mechanical properties of Ti2AlNb-C/C joints brazed with Ag-Cu filler
    Xu, Jingxin
    Zhou, Wenlong
    Song, Xiaoguo
    Fu, Wei
    Song, Yanyu
    Long, Fei
    Hu, Shengpeng
    MATERIALS TODAY COMMUNICATIONS, 2025, 43
  • [7] Joining of TiAl Alloy Using Novel Ag-Cu Sputtered Coated Ti Brazing Filler
    Simoes, Sonia
    Soares, Ana
    Tavares, Carlos Jose
    Guedes, Anibal
    MICROSCOPY AND MICROANALYSIS, 2019, 25 (01) : 192 - 195
  • [9] Microstructure and shear strength of brazed joints between Ti(C,N)-based cermet and steel with Cu-Ag-Ti filler metal
    Jing, Yong
    Yang, Qingqing
    Xiong, Weihao
    Huang, Bin
    Li, Baolong
    Zhang, Man
    JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 682 : 525 - 530
  • [10] Comparative study on microstructure and strength of TiAl/steel joints brazed with Ag-Cu-Ti and Ag-Cu-Zn filler metals
    Liu, HJ
    Feng, JC
    NEW FRONTIERS OF PROCESSING AND ENGINEERING IN ADVANCED MATERIALS, 2005, 502 : 467 - 472