Development of suicide coatings to ensure the protection of Nb and suicide composites against high temperature oxidation

被引:64
|
作者
Knittel, S. [1 ]
Mathieu, S. [2 ]
Portebois, L. [2 ]
Drawin, S. [3 ]
Vilasi, M. [2 ]
机构
[1] SNECMA, F-91003 Evry, France
[2] Univ Lorraine, Inst Jean Lamour, UMR7198, F-54506 Vandoeuvre Les Nancy, France
[3] Onera French Aerosp Lab, F-92322 Chatillon, France
来源
关键词
Diffusion coating; Pack cementation; Niobium silicide composites; Oxidation; ISOTHERMAL SECTION; SILICIDES; KINETICS; ALLOYS;
D O I
10.1016/j.surfcoat.2013.07.053
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this work, we describe the fabrication of coatings containing (TiNbXCr)(7)Si-6 silicide (with X = Fe, Co and Ni) by halide-activated pack-cementation on Nb and silicide composites. The coating oxidation performance is evaluated isothermally at temperatures ranging from 1100 degrees C to 1300 degrees C and cyclically at 1100 degrees C In all the coating systems examined, the M7Si6 suicide formed in the protective coating and constituted the outmost layer for coatings containing Co, whereas M6Si5 and a Cr-rich suicide constituted the outmost compounds for Fe and Ni coatings, respectively. The results of isothermal oxidation tests show that all these compounds form protective oxide layers leading to very low mass gains, both at 1100 degrees C and 1200 degrees C. Under cyclic conditions at 1100 degrees C, coatings containing Co and Ni exhibited very long lifetimes, exceeding 2600 1-hour cycles. The beneficial effect of Ni and Co diminished at 1300 degrees C, due to rapid interdiffusion between substrate and coating in comparison to that found in the Fe containing coating. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:401 / 406
页数:6
相关论文
共 50 条
  • [1] Nb4Fe4Si7 coatings to protect niobium and niobium suicide composites against high temperature oxidation
    Knittel, S.
    Mathieu, S.
    Vilasi, M.
    SURFACE & COATINGS TECHNOLOGY, 2013, 235 : 144 - 154
  • [2] Development of suicide coatings over Nb-NbCr2 alloy and their oxidation behavior at 1250 °C
    Qiao, Yanqiang
    Li, Maoyuan
    Guo, Xiping
    SURFACE & COATINGS TECHNOLOGY, 2014, 258 : 921 - 930
  • [3] COMPOSITE COATINGS OF CHROMIUM AND NICKEL FOR THE PROTECTION OF MOLYBDENUM AGAINST HIGH TEMPERATURE OXIDATION
    TAYLOR, JK
    SHAPIRO, H
    BRENNER, A
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1955, 102 (09) : C224 - C224
  • [4] Coatings with particulate dispersions for high temperature oxidation protection of carbon and C/C composites
    Joshi, A
    Lee, JS
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1997, 28 (02) : 181 - 189
  • [5] VACUUM-ARC CHROMIUM COATINGS FOR Zr-1Nb ALLOY PROTECTION AGAINST HIGH-TEMPERATURE OXIDATION IN AIR
    Kuprin, A. S.
    Belous, V. A.
    Bryk, V. V.
    Vasilenko, R. L.
    Voyevodin, V. N.
    Ovcharenko, V. D.
    Tolmachova, G. N.
    Kolodiy, I. V.
    Lunyov, V. M.
    Klimenko, I. O.
    PROBLEMS OF ATOMIC SCIENCE AND TECHNOLOGY, 2015, (02): : 111 - 118
  • [6] Ultra-high-temperature ceramic coatings for oxidation protection of carbon-carbon composites
    Corral, Erica L.
    Loehman, Ronald E.
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2008, 91 (05) : 1495 - 1502
  • [7] DEVELOPMENT OF ADVANCED VITREOUS COATINGS FOR HIGH-TEMPERATURE OXIDATION PROTECTION OF COMBUSTION LINERS
    HSU, L
    STETSON, AR
    JOURNAL OF METALS, 1982, 35 (12): : A25 - A25
  • [8] PROTECTION OF PURE IRON AGAINST HIGH-TEMPERATURE OXIDATION USING METABORATE AND METASILICATE COATINGS
    HUSAIN, Z
    CORROSION, 1993, 49 (04) : 290 - 293
  • [9] Fe-Al-Si coatings for the protection of steel against high-temperature oxidation
    Novák P.
    Lamchaouri A.
    Nová K.
    Průša F.
    Manufacturing Technology, 2019, 19 (04): : 660 - 663
  • [10] High temperature oxidation protection coatings for monolithic or composite ceeramics
    Desmaison, J.
    Werkstoffe und Korrosion, 1990, 41 (12): : 749 - 750