摘要
Fine and uniform powder of beta-silicon nitride was liquid phase sintered by hot-pressing at 1700 degrees C. Deformation behavior was investigated under compressive stress at 1500 - 1600 OC. The material deformed at a strain rate, 1-7 x 10(-4) /s, under a pressure of 10-100 MPa at 1550 degrees C. Strain hardening was not observed even at slow deformation rate because of the absence of appreciable dynamic grain growth. The strength and fracture toughness of as-hot-pressed materials was 793 MPa and 2.8 MPa(.)m(1/2), respectively.The properties were improved by the deformation to 912 MPa and 3.5 MPa(.)m(1/2), rtspectively. Further Improvement was achieved by the annealing at 1700 degrees C for 30 min. The bending strength and fracture toughness increased to 982 MPa and 3.7 MPa(.)m(1/2), respectively, by slight grain growth. Present work provides a process to produce complex-shaped components by superplastic deformation at low temperatures and to improve the mechanical properties by further heat treatment.
引用
收藏
页码:477 / 482
页数:6
相关论文
共 50 条
  • [1] Microstructures and mechanical properties of anisotropic silicon nitride produced by superplastic deformation
    Kondo, N
    Ohji, T
    Sato, E
    Wakai, F
    [J]. SCIENCE OF ENGINEERING CERAMICS II, 1999, 2 : 555 - 558
  • [2] Superplastic deformation of silicon nitride ceramics
    Kondo, N
    [J]. TIME DEPENDENT MECHANICAL RESPONSE OF ENGINEERING CERAMICS: FROM PICO-SECOND TO MILLION YEARS, 1999, 4 : 109 - 116
  • [3] Strengthening and toughening of silicon nitride by superplastic deformation
    Kondo, N
    Ohji, T
    Wakai, F
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1998, 81 (03) : 713 - 716
  • [4] Improvement in the Mechanical Properties of Silicon Nitride Ceramic in High-Temperature Deformation Processes
    I. D. Gnilitsa
    Ya. A. Kril'
    [J]. Powder Metallurgy and Metal Ceramics, 2005, 44 : 441 - 445
  • [5] Improvement in the mechanical properties of silicon nitride ceramic in high-temperature deformation processes
    Gnilitsa, ID
    Kril, YA
    [J]. POWDER METALLURGY AND METAL CERAMICS, 2005, 44 (9-10) : 441 - 445
  • [6] Superplastic deformation in silicon nitride-silicon oxynitride in situ composites
    Xie, RJ
    Mitomo, M
    Zhan, GD
    Emoto, H
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2000, 83 (10) : 2529 - 2535
  • [7] Creep deformation effects on the mechanical properties of a silicon nitride ceramic
    Tenore, D
    Melandri, C
    Guicciardi, S
    [J]. JOURNAL OF MATERIALS SCIENCE LETTERS, 2000, 19 (16) : 1427 - 1429
  • [8] SPS processing and superplastic deformation of silicon nitride based ceramics
    Peng, H
    Shen, ZJ
    Nygren, M
    [J]. ADVANCED SI-BASED CERAMICS AND COMPOSITES, 2005, 287 : 146 - 155
  • [9] Superplastic deformation of silicon nitride nanocompositee at high strain rates
    Chihara, Kentarou
    Shinoda, Yutaka
    Akatsu, Takashi
    Wakai, Fumihiro
    [J]. SCIENCE OF ENGINEERING CERAMICS III, 2006, 317-318 : 403 - 406
  • [10] Superplastic deformation of nano-sized silicon nitride ceramics
    Xu, X
    Nishimura, T
    Hirosaki, N
    Xie, RJ
    Yamamoto, Y
    Tanaka, H
    [J]. ACTA MATERIALIA, 2006, 54 (01) : 255 - 262