Effect of Process Parameters on Defects, Melt Pool Shape, Microstructure, and Tensile Behavior of 316L Stainless Steel Produced by Selective Laser Melting

被引:3
|
作者
Jiang, Hua-Zhen [1 ,2 ]
Li, Zheng-Yang [2 ]
Feng, Tao [3 ]
Wu, Peng-Yue [3 ]
Chen, Qi-Sheng [1 ,2 ]
Feng, Yun-Long [3 ]
Chen, Long-Fei [3 ]
Hou, Jing-Yu [1 ,2 ]
Xu, He-Jian [2 ]
机构
[1] Univ Chinese Acad Sci, Sch Engn Sci, Beijing 100190, Peoples R China
[2] Chinese Acad Sci, Inst Mech, Beijing 100190, Peoples R China
[3] Beijing E Plus 3D Technol Co LTD, Beijing 102299, Peoples R China
基金
中国国家自然科学基金; 国家重点研发计划;
关键词
Selective laser melting; Defects; Melt pool shape; Primary dendrite spacing; Mechanical properties; 316L stainless steel; POWDER-BED FUSION; HIGH-STRENGTH; DENSITY; DENSIFICATION; PERFORMANCE; DEPENDENCE; AUSTENITE; MECHANISM; DUCTILITY; DIAGRAMS;
D O I
10.1007/s40195-020-01157-2
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Previous studies have revealed that laser power and energy density are significant factors affecting the quality of parts manufactured by selective laser melting (SLM). The normalized equivalent densityE(0)* and dimensionless laser powerq*, which can be regarded as a progress on the understanding of the corresponding dimensional quantities, are adopted in this study to examine the defects, melt pool shape, and primary dendrite spacing of the SLM-manufactured 316L stainless steel, because it reflects the combined effect of process parameters and material features. It is found that the number of large defects decreases with increasingE(0)* due to enough heat input during the SLM process, but it will show an increasing trend when excessive heat input (i.e., utilizing a highE(0)*) is imported into the powder bed. Theq* plays an important role in controlling maximum temperature rising in the SLM process, and in turn, it affects the number of large defects. A largeq* value results in a low value of absolute frequency of large defects, whereas a maximum value of absolute frequency of large defects is achieved at a lowq* even ifE(0)* is very high. The density of the built parts is greater at a higherq* whenE(0)* remains constant. Increasing the melt pool depth at relatively low value ofE(0)* enhances the relative density of the parts. A narrow, deep melt pool can be easily generated at a highq* whenE(0)* is sufficiently high, but it may increase melt pool instability and cause keyhole defects. It is revealed that a lowE(0)* can lead to a high cooling rate, which results in a refined primary dendrite spacing. Relatively lowE(0)* is emphasized in selecting the process parameters for the tensile test sample fabrication. It shows that excellent tensile properties, namely ultimate tensile strength, yield strength, and elongation to failure of 773 MPa, 584 MPa, and 46%, respectively, can be achieved at a relatively lowE(0)* without heat treatment.
引用
收藏
页码:495 / 510
页数:16
相关论文
共 50 条
  • [1] Effect of Process Parameters on Defects, Melt Pool Shape, Microstructure, and Tensile Behavior of 316L Stainless Steel Produced by Selective Laser Melting
    Hua-Zhen Jiang
    Zheng-Yang Li
    Tao Feng
    Peng-Yue Wu
    Qi-Sheng Chen
    Yun-Long Feng
    Long-Fei Chen
    Jing-Yu Hou
    He-Jian Xu
    ActaMetallurgicaSinica(EnglishLetters), 2021, 34 (04) : 495 - 510
  • [2] Effect of Process Parameters on Defects, Melt Pool Shape, Microstructure, and Tensile Behavior of 316L Stainless Steel Produced by Selective Laser Melting
    Hua-Zhen Jiang
    Zheng-Yang Li
    Tao Feng
    Peng-Yue Wu
    Qi-Sheng Chen
    Yun-Long Feng
    Long-Fei Chen
    Jing-Yu Hou
    He-Jian Xu
    Acta Metallurgica Sinica (English Letters), 2021, 34 : 495 - 510
  • [3] Microstructure and Fracture Behavior of 316L Austenitic Stainless Steel Produced by Selective Laser Melting
    R.Casati
    J.Lemke
    M.Vedani
    JournalofMaterialsScience&Technology, 2016, 32 (08) : 738 - 744
  • [4] Microstructure and Fracture Behavior of 316L Austenitic Stainless Steel Produced by Selective Laser Melting
    Casati, R.
    Lemke, J.
    Vedani, M.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2016, 32 (08) : 738 - 744
  • [5] Effect of Process Parameters on Defect in Selective Laser Melting of 316L Stainless Steel
    Wang Lei
    Guo Kai
    Cong Jiaqi
    Bai Huiyi
    Kang Xueliang
    Ji Yunping
    Li Yiming
    Ren Huiping
    LASER & OPTOELECTRONICS PROGRESS, 2023, 60 (05)
  • [6] Microstructure and Mechanical Properties of 316L Stainless Steel Produced by Selective Laser Melting
    Qi, Xiaotong
    Feng, Haoming
    Liu, Lin
    MATERIALS SCIENCE, ENERGY TECHNOLOGY AND POWER ENGINEERING III (MEP 2019), 2019, 2154
  • [7] Biaxial tensile behavior of stainless steel 316L manufactured by selective laser melting
    Wang, Hao
    Shu, Xiaoyong
    Zhao, Jianping
    Alexandrov, I. V.
    SCIENTIFIC REPORTS, 2023, 13 (01)
  • [8] Biaxial tensile behavior of stainless steel 316L manufactured by selective laser melting
    Hao Wang
    Xiaoyong Shu
    Jianping Zhao
    I. V. Alexandrov
    Scientific Reports, 13
  • [9] Microstructure and properties of 316L stainless steel by selective laser melting under various process parameters
    Hsueh-Chuan Hsu
    Ka-Kin Wong
    Shih-Ching Wu
    Po-Jen Hou
    Wen-Fu Ho
    MRS Communications, 2022, 12 : 768 - 772
  • [10] Microstructure and properties of 316L stainless steel by selective laser melting under various process parameters
    Hsu, Hsueh-Chuan
    Wong, Ka-Kin
    Wu, Shih-Ching
    Hou, Po-Jen
    Ho, Wen-Fu
    MRS COMMUNICATIONS, 2022, 12 (05) : 768 - 772