Microcrack formation under normal and dwell fatigue of IMI 834

被引:11
|
作者
Yazar, K. U. [1 ]
Bahl, S. [1 ]
Mishra, S. [1 ]
Sahu, V. K. [2 ]
Bhattacharjee, A. [3 ]
Banerjee, D. [1 ]
Suwas, S. [1 ]
机构
[1] Indian Inst Sci, Dept Mat Engn, Bangalore 560012, India
[2] Indian Inst Technol Kanpur, Dept Mat Sci & Engn, Kanpur 208016, India
[3] Titanium Alloys Grp, Def Met Res Lab, Hyderabad 500066, India
关键词
Near alpha titanium alloy; Dwell fatigue; Microcracks; Facets; Pileup; HIGH-CYCLE FATIGUE; CRYSTAL PLASTICITY; CRACK NUCLEATION; SENSITIVE FATIGUE; TITANIUM-ALLOY; CRYSTALLOGRAPHIC ORIENTATION; TEXTURE HETEROGENEITIES; TEMPERATURE CREEP; BETA-PHASE; MICROSTRUCTURE;
D O I
10.1016/j.ijfatigue.2023.107724
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Dwell sensitivity of titanium alloys at ambient temperature (-25 degrees C) is a well-reported phenomenon, although the question about the phenomena of crack initiation remains open. In this work, the normal and dwell fatigue response of a near alpha titanium alloy is studied. A dwell fatigue debit (number of continuous cycles to failure to number of cycles to failure with a dwell period) of up to 2 and 10 were observed at two different load levels. Analysis using scanning electron microscopy, electron back scattered diffraction and transmission electron microscope-based orientation imaging microscopy (TEM-OIM) revealed that the formation of microcracks at very early stages of dwell fatigue loading was the major reason for this decreased life. The initiation of these cracks was observed to be a strong function of the local crystallography of the constituent grains. A modified pile up model in which the shear stress on the pile up plane is calculated using stress redistribution at the grain level is used to explain the micromechanisms of crack nucleation in dwell fatigue. The elastic and plastic anisotropy of the hexagonal crystal, the microtextural characteristics and strong stress redistributions at the grain level results in the nucleation and propagation of these microcracks.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] Bimodal dwell-fatigue Weibull distribution of forged titanium IMI 834
    Toubal, Lotfi
    Bocher, Philippe
    Moreau, Andre
    INTERNATIONAL JOURNAL OF DAMAGE MECHANICS, 2015, 24 (05) : 629 - 645
  • [2] Influence of Hold Time on Dwell Fatigue Behavior in IMI834 Disc Forging
    Ruyue You
    Mengmeng Zhang
    Jianke Qiu
    Chao Fang
    Chunling Zhao
    Bo Lu
    Haibin Ji
    Yingjie Ma
    Jiafeng Lei
    Rui Yang
    JOM, 2022, 74 : 3733 - 3744
  • [3] Influence of Hold Time on Dwell Fatigue Behavior in IMI834 Disc Forging
    You, Ruyue
    Zhang, Mengmeng
    Qiu, Jianke
    Fang, Chao
    Zhao, Chunling
    Lu, Bo
    Ji, Haibin
    Ma, Yingjie
    Lei, Jiafeng
    Yang, Rui
    JOM, 2022, 74 (10) : 3733 - 3744
  • [4] Effect of Thermomechanical Processing on the Dwell Fatigue Behaviour of Near Alpha Titanium Alloy IMI 834
    K. U. Yazar
    Amit Bhattacharjee
    Satyam Suwas
    JOM, 2023, 75 : 218 - 231
  • [5] Effect of Thermomechanical Processing on the Dwell Fatigue Behaviour of Near Alpha Titanium Alloy IMI 834
    Yazar, K. U.
    Bhattacharjee, Amit
    Suwas, Satyam
    JOM, 2023, 75 (01) : 218 - 231
  • [6] How Texture and Microtexture Influence Dwell Fatigue Lifetime in Forged IMI834 Titanium Alloys
    Gey, N.
    Bocher, P.
    Uta, E.
    Humbert, M.
    Gilgert, J.
    TI-2011: PROCEEDINGS OF THE 12TH WORLD CONFERENCE ON TITANIUM, VOL II, 2012, : 879 - 882
  • [7] Effect of environment on high-temperature fatigue of IMI 834
    Schauerte, O
    Gysler, A
    Lütjering, G
    Mailly, S
    Chabanne, Y
    Sarrazin-Baudoux, C
    Mendez, J
    Petit, J
    FATIGUE BEHAVIOR OF TITANIUM ALLOYS, 1999, : 191 - 202
  • [8] Formation of interface phases in the titanium alloy IMI 834
    Baxter, GJ
    Rainforth, WM
    Grabowski, L
    JOURNAL OF MATERIALS SCIENCE, 1996, 31 (05) : 1205 - 1211
  • [9] High Temperature Fretting Fatigue Behavior of IMI 834 Titanium Alloy
    M. Jayaprakash
    D. Komatsu
    M. Okazaki
    Y. Miyashita
    Y. Otsuka
    Y. Mutoh
    Transactions of the Indian Institute of Metals, 2016, 69 : 439 - 444
  • [10] Life prediction for the titanium alloy IMI 834 under high temperature creep-fatigue loadings
    Kordisch, T.
    Nowack, H.
    Fatigue and Fracture of Engineering Materials and Structures, 1998, 21 (01): : 47 - 63