The Effect of Brushing on Residual Stress and Surface Roughness of EN AW-2024-T3 Aluminum Alloy Joints Welded Using the FSW Method

被引:3
|
作者
Bucior, Magdalena [1 ]
Kluz, Rafal [1 ]
Kubit, Andrzej [1 ]
Ochal, Kamil [2 ]
机构
[1] Rzeszow Univ Technol, Dept Mfg Proc & Prod Engn, al Powstancow Warszawy 8, PL-35959 Rzeszow, Poland
[2] Rzeszow Univ Technol, Dept Mat Sci, al Powstancow Warszawy 8, PL-35959 Rzeszow, Poland
关键词
brushing; aluminum alloy; friction stir welding; surface roughness; residual stress; MECHANICAL-PROPERTIES; FRICTION; MICROSTRUCTURE; PARAMETERS;
D O I
10.12913/22998624/156943
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This article presents the influence of the brushing process on residual stress and surface roughness of EN AW-2024-T3 aluminum alloy joints welded using the Friction Stir Welding (FSW) method. Butt joints with thicknesses of 2 mm were brushing with using ceramic brush. The aim of the study was to find optimal parameters of the brush-ing process, which would significantly improve the functional properties of welded joints. The experiments were carried out in two steps. In the first stage of the research, the feed rate was changed in the range f = 40 divided by 120 mm/min with a constant brushing depth d = 0.5 mm. The roughness decreased from Sa = 5.285 mu m for the specimen after welding to Sa = 2.460 mu m for the f = 120 mm/min and d = 0.5 mm. The change in the parameters of the brushing process did not have a significant impact on the state of residual stresses. Hence, in the second step, the brushing depth was increased in steps of 0.1 mm. The best properties were obtained for f = 120 mm/min and d = 0.6 mm (variant 6A), where roughness was Sa = 0.443 mu m and compressive stresses sigma =-118 MPa.
引用
收藏
页码:86 / 93
页数:8
相关论文
共 50 条
  • [1] Effect of Diamond Burnishing on the Properties of FSW Joints of EN AW-2024 Aluminum Alloys
    Kluz, Rafal
    Bucior, Magdalena
    Dzierwa, Andrzej
    Antosz, Katarzyna
    Bochnowski, Wojciech
    Ochal, Kamil
    APPLIED SCIENCES-BASEL, 2023, 13 (03):
  • [2] Effects of process parameters on dynamic and static load capacity of EN AW-2024-T3 aluminum alloy joints prepared by friction stir welding
    Andrzej Kubit
    Hamed Aghajani Derazkola
    Wojciech Jurczak
    Krzysztof Ochałek
    Piotr Myśliwiec
    Wojciech Macek
    Olga Łastowska
    Przemysław Podulka
    Ján Slota
    Archives of Civil and Mechanical Engineering, 25 (3)
  • [3] Multi-Criteria Optimisation of Friction Stir Welding Parameters for EN AW-2024-T3 Aluminium Alloy Joints
    Kubit, Andrzej
    Trzepiecinski, Tomasz
    Kluz, Rafal
    Ochalek, Krzysztof
    Slota, Jan
    MATERIALS, 2022, 15 (15)
  • [4] EFFECT OF HOLES IN OVERLAP ON THE LOAD CAPACITY OF THE SINGLE-LAP ADHESIVE JOINTS MADE OF EN AW-2024-T3 ALUMINIUM ALLOY
    Zielecki, Wladyslaw
    Burnat, Katarzyna
    Kubit, Andrzej
    Katrnak, Tomas
    ADVANCES IN MATERIALS SCIENCE, 2021, 21 (04): : 112 - 121
  • [5] Experimental and numerical investigation of the strength behavior of corroded aluminum alloy EN AW-2024-T3 under uniaxial loading
    Schmidl, E.
    Pippig, R.
    Lampke, T.
    18TH CHEMNITZ SEMINAR ON MATERIALS ENGINEERING, 2016, 118
  • [6] Experimental and numerical investigation of the residual yield strength of aluminium alloy EN AW-2024-T3 affected by artificially produced pitting corrosion
    Pippig, R.
    Schmidl, E.
    Steinert, P.
    Schubert, A.
    Lampke, T.
    19TH CHEMNITZ SEMINAR ON MATERIALS ENGINEERING, 2017, 181
  • [7] Effects of polymer sealant interlayer on quality of EN AW-2024-T3 aluminum alloy lap joint prepared by friction stir welding
    Kubit, Andrzej
    Derazkola, Hamed Aghajani
    Mysliwiec, Piotr
    Szawara, Paulina
    Slota, Jan
    Macek, Wojciech
    ARCHIVES OF CIVIL AND MECHANICAL ENGINEERING, 2024, 24 (04)
  • [8] Experimental study of the low-cycle fatigue life under multiaxial loading of aluminum alloy EN AW-2024-T3 at elevated temperatures
    Szusta, J.
    Seweryn, A.
    INTERNATIONAL JOURNAL OF FATIGUE, 2017, 96 : 28 - 42
  • [9] Study of thermal properties of the aluminum EN AW 2024-T3 alloy
    Manasijevic, Dragan
    Balanovic, Ljubisa
    Tadic, Nebojsa
    Radovic, Zarko
    Stamenkovic, Uros
    Gorgievski, Milan
    Markovic, Ivana
    KOVOVE MATERIALY-METALLIC MATERIALS, 2024, 62 (01): : 31 - 39
  • [10] Experimental Investigation of Load-Bearing Capacity in EN AW-2024-T3 Aluminum Alloy Sheets Strengthened by SPIF-Fabricated Stiffening Rib
    Khalaf, Hassanein I.
    Al-Sabur, Raheem
    Kubit, Andrzej
    Swiech, Lukasz
    Zaba, Krzysztof
    Novak, Vit
    MATERIALS, 2024, 17 (08)