Corrosion protection of magnesium alloys anode by cerium-based anodization coating in magnesium-air battery

被引:12
|
作者
You, Xiang [1 ]
Zhang, Xiaowei [2 ,3 ]
Yu, Chuang [2 ,3 ]
Chen, Yuanliang [1 ]
Li, Huiming [1 ]
Hou, Yanqing [1 ]
Tian, Lin [4 ]
Yang, Ni [4 ]
Xie, Gang [4 ]
机构
[1] Kunming Univ Sci & Technol, State Key Lab Complex Nonferrous Met Resources Cle, Kunming 650093, Peoples R China
[2] GRINM Grp Co Ltd, Natl Engn Res Ctr Rare Earth Mat, Beijing 100088, Peoples R China
[3] GRIREM Adv Mat Co Ltd, Beijing 100088, Peoples R China
[4] State Key Lab Pressure Hydromet Technol Associated, Kunming 650031, Peoples R China
基金
中国国家自然科学基金;
关键词
AZ31 magnesium alloy anode; Magnesium-air battery; Corrosion rate; Electrochemical; Rare earths; MG; MICROSTRUCTURE;
D O I
10.1016/j.jre.2022.04.011
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
CeN3O9.6H2O (0.5, 1.0, 1.5, and 2.0 g/L) was added into an 8.0% NaCl electrolyte solution to investigate this electrolyte for use in a Mg-air battery. The effects of the amount of CeN3O9.6H2O on the corrosion resistance of an AZ31 Mg alloy anode and battery performance were investigated using microstructure, electrochemical (dynamic potential polarization method and electrochemical impedance spectroscopy), and battery measurements. The results show that the addition of CeN3O9.6H2O to the electrolyte leads to the formation of a Ce(OH)3 protective film on the surface of the AZ31 Mg alloy that improves the corrosion resistance of the Mg alloy. An increase in the concentration of CeN3O9.6H2O results in a denser Ce(OH)3 protective film and decreases corrosion rate of the AZ31 Mg alloy. When the concentration of CeN3O9.6H2O is 1.0 g/L, the corrosion rate of the Mg alloy is the lowest with a corrosion inhibition rate of 70.4%. However, the corrosion rate increases due to the dissolution of the Ce(OH)3 protective film when the concentration of CeN3O9.6H2O is greater than 1.0 g/L. Immersing the Mg alloy in the electrolyte solution containing CeN3O9.6H2O for 50 h leads to the formation of the Ce(HO)3 protective film on its surface, which was confirmed by scanning electron microscopy of the AZ31 alloy. The Mg2 thorn charge transfer resistance increases by 69.5 U from the equivalent circuit diagram, which improves the corrosion resistance of the Mg alloy. The discharge performance of CeN3O9.6H2O improves according to a discharge test, and the discharge time increases by 40 min. (c) 2022 Chinese Society of Rare Earths. Published by Elsevier B.V. All rights reserved.
引用
收藏
页码:471 / 476
页数:6
相关论文
共 50 条
  • [1] Corrosion protection of magnesium alloys anode by cerium-based anodization coating in magnesium-ait battery
    Xiang You
    Xiaowei Zhang
    Chuang Yu
    Yuanliang Chen
    Huiming Li
    Yanqing Hou
    Lin Tian
    Ni Yang
    Gang Xie
    JournalofRareEarths, 2023, 41 (03) : 471 - 476
  • [2] Decyl glucoside as a corrosion inhibitor for magnesium-air battery
    Deyab, M. A.
    JOURNAL OF POWER SOURCES, 2016, 325 : 98 - 103
  • [3] Corrosion and discharge performance of a magnesium aluminum eutectic alloy as anode for magnesium-air batteries
    Ma, Jingling
    Zhang, Yi
    Ma, Mingsheng
    Qin, Conghui
    Ren, Fengzhang
    Wang, Guangxin
    CORROSION SCIENCE, 2020, 170 (170)
  • [4] Effect of HCl pre-treatment on corrosion resistance of cerium-based conversion coatings on magnesium and magnesium alloys
    Brunelli, K
    Dabalà, M
    Calliari, I
    Magrini, M
    CORROSION SCIENCE, 2005, 47 (04) : 989 - 1000
  • [5] Magnesium alloys as anodes for neutral aqueous magnesium-air batteries
    Tong, Fanglei
    Wei, Shanghai
    Chen, Xize
    Gao, Wei
    JOURNAL OF MAGNESIUM AND ALLOYS, 2021, 9 (06) : 1861 - 1883
  • [6] Magnesium alloys as anodes for neutral aqueous magnesium-air batteries
    Fanglei Tong
    Shanghai Wei
    Xize Chen
    Wei Gao
    Journal of Magnesium and Alloys, 2021, 9 (06) : 1861 - 1883
  • [7] Enhancing primary aqueous magnesium-air battery performance by tailoring anode texture
    Sha, Jianchun
    Liu, Zhoulin
    Bao, Jiaxin
    Li, Lianhui
    Qiao, Mingliang
    Jie, Tian
    Liu, Wenhong
    Zhang, Zhiqiang
    JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 2024, 964
  • [8] Magnesium alloys as anodes for neutral aqueous magnesium-air batteries
    Fanglei Tong
    Shanghai Wei
    Xize Chen
    Wei Gao
    Journal of Magnesium and Alloys, 2021, (06) : 1861 - 1883
  • [9] Current Progress on Rechargeable Magnesium-Air Battery
    Li, Chun-Sheng
    Sun, Yan
    Gebert, Florian
    Chou, Shu-Lei
    ADVANCED ENERGY MATERIALS, 2017, 7 (24)
  • [10] Microstructure and battery performance of Mg-Zn-Sn alloys as anodes for magnesium-air battery
    Fanglei Tong
    Xize Chen
    Shanghai Wei
    Jenny Malmstr^m
    Joseph Vella
    Wei Gao
    Journal of Magnesium and Alloys, 2021, (06) : 1967 - 1976