Microstructure Stabilities of Newly Developed Hot-Working Die Steel and H13 Steel at Elevated Temperature

被引:1
|
作者
Zhang, Cheng [1 ]
Cao, Yuqian [1 ]
Chen, Junyu [1 ]
Ye, Huanyu [2 ]
Zhao, Chao [3 ]
Huang, Jinfeng [1 ]
机构
[1] Univ Sci & Technol Beijing, State Key Lab Adv Met & Mat, Beijing 100083, Peoples R China
[2] Univ Sci & Technol Beijing, Sch Math & Phys, Beijing 100083, Peoples R China
[3] North Univ China, Coll Mechatron Engn, Taiyuan 030000, Peoples R China
基金
中国国家自然科学基金;
关键词
hot-working die steels; nano-carbides; recrystallization; thermal stability; CARBIDE PRECIPITATION; MECHANICAL-PROPERTIES; COARSENING BEHAVIOR; NB; MO; EVOLUTION; STRENGTH; CR; BOUNDARIES; AUSTENITE;
D O I
10.1002/srin.202200811
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Herein, the microstructure stability of a newly developed hot-working die (HWD700) steel at elevated temperatures up to 700 degrees C is investigated using transmission electron microscopy (TEM), selected-area electron diffraction, energy-dispersive spectrometer, and high-resolution transmission electron microscope. It is showed in the results that the HWD700 steel exhibits a higher thermal stability than the commercial H13 steel when the temperature is up to 700 degrees C. After quenching and tempering, high densities of intra-lath rodlike and inter-lath spherical MC nano-carbides and inter-lath strip-like M7C3 nano-carbides are observed in the HWD700 steel. These carbides remain nanoscale at temperatures up to 700 degrees C. For comparison, rod-shaped MC nano-carbides in the tempered H13 steel tend to coarsen and transform into larger M23C6 carbides at temperatures up to 650 degrees C. The TEM observation further reveals that the interface misfit between the MC nano-carbide and matrix in the HWD700 steel is as low as 0.88%, lower than that of 14.8% in the H13 steel. This can be the main reason for the improved stability of the HWD700 steel by pinning dislocations and grain boundaries and thereby hindering the recrystallization process at an elevated temperature.
引用
收藏
页数:12
相关论文
共 50 条
  • [1] Heat treatment of hot working die steel H13
    Li, Wenxue
    Wang, Yufeng
    Liu, Zongchang
    Teshugang/Special Steel, 1999, 20 (06): : 10 - 12
  • [2] Inclusion Variations of Hot Working Die Steel H13 in Refining Process
    Jian-hua Liu
    Guo-xuan Wang
    Yan-ping Bao
    Yan Yang
    Wei Yao
    Xiao-ning Cui
    Journal of Iron and Steel Research International, 2012, 19 : 1 - 7
  • [4] Inclusion Variations of Hot Working Die Steel H13 in Refining Process
    Liu Jian-hua
    Wang Guo-xuan
    Bao Yan-ping
    Yang Yan
    Yao Wei
    Cui Xiao-ning
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2012, 19 (11) : 1 - 7
  • [5] AN INVESTIGATION OF THE PROPERTIES AND WEAR BEHAVIOR OF PLASMA-NITRIDED HOT-WORKING STEEL (H13)
    KARAMIS, MB
    WEAR, 1991, 150 (1-2) : 331 - 342
  • [6] Comparative research on the elevated-temperature wear resistance of a cast hot-working die steel
    Wei, M. X.
    Wang, F.
    Wang, S. Q.
    Cui, X. H.
    MATERIALS & DESIGN, 2009, 30 (09) : 3608 - 3614
  • [7] Microstructure and Properties of Hot Working Die Steel H13MOD
    ZHOU Jian
    MA Dang-shen
    CHI Hong-xiao
    CHEN Zai-zhi
    LI Xiang-yang
    Journal of Iron and Steel Research(International), 2013, 20 (09) : 117 - 125
  • [8] Microstructure and Properties of Hot Working Die Steel H13MOD
    Zhou Jian
    Ma Dang-shen
    Chi Hong-xiao
    Chen Zai-zhi
    Li Xiang-yang
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2013, 20 (09) : 117 - 125
  • [9] Microstructure and Properties of Hot Working Die Steel H13MOD
    Jian Zhou
    Dang-shen Ma
    Hong-xiao Chi
    Zai-zhi Chen
    Xiang-yang Li
    Journal of Iron and Steel Research International, 2013, 20 : 117 - 125