Effect of mechanical stresses on degradation behavior of high-purity magnesium in bone environments

被引:1
|
作者
Yao, Yan [1 ]
Xia, Jie [1 ]
Wang, Lizhen [1 ]
Gao, Yuanming [1 ]
Ding, Xili [1 ]
Wang, Chao [1 ]
Fan, Yubo [1 ]
机构
[1] Beihang Univ, Beijing Adv Innovat Ctr Biomed Engn, Sch Biol Sci & Med Engn, Sch Engn Med,Key Lab Biomech & Mechanobiol,Minist, Beijing 100083, Peoples R China
来源
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY | 2024年 / 171卷
关键词
High-purity magnesium; Quantitative stresses; Degradation; Bone environments; In vivo and in vitro; IN-VITRO; CORROSION CRACKING; ALLOYS; MODEL; VIVO; MG; DEFORMATION; IMPLANTS; FRACTURE; DESIGN;
D O I
10.1016/j.jmst.2023.07.043
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
High-purity (HP) magnesium (Mg) has emerged as a promising biomaterial for supporting functional bone tissue. Our previous study found that mechanical stresses and the surrounding fibrotic tissue (subcutaneous) both play crucial roles in the degradation of HP Mg. However, due to challenges in the degradation and regeneration process in vivo, it remains unclear how stress affects HP Mg degradation in bone environments, limiting its further application. In this study, novel loading devices were designed and the effects of tensile and compressive stresses on HP Mg degradation in vivo and in vitro bone environments were quantitatively analyzed. In addition, bone osteointegration around HP Mg was explored preliminarily. Tensile stress increases the degradation rate of HP Mg in vivo and in vitro. HP Mg degradation in vivo is more sensitive to stress factors than in vitro, but the sensitivity decreases with corrosion time. The volume loss rate of HP Mg is multilinear with the applied stress and degradation time. The volume of bone tissue surrounding HP Mg is larger in the no-stress group compared to the stressed groups, which is more pronounced with increasing implantation time. These results provide valuable insights for optimizing the design of HP Mg-based implants considering load conditions. This will help to achieve a balance between the degradation rate of the implant and the regeneration rate of the surrounding bone.& COPY; 2023 Published by Elsevier Ltd on behalf of The editorial office of Journal of Materials Science & Technology.
引用
收藏
页码:252 / 261
页数:10
相关论文
共 50 条
  • [1] RELAXATION OF STRESSES IN IRON OF HIGH-PURITY
    KAMENETS.DS
    PILETSKA.IB
    SHIRYAEV, VI
    FIZIKA METALLOV I METALLOVEDENIE, 1973, 36 (03): : 605 - 609
  • [2] In vitro degradation and mineralization of high-purity magnesium in three physiological fluids
    Zuo, Minchao
    Wang, Wenhui
    Wu, Hongliu
    Yang, Linhua
    Yan, Jun
    Ni, Jiahua
    Zhang, Shaoxiang
    Song, Yang
    Wang, Jian
    Zhang, Xiaonong
    MATERIALS LETTERS, 2019, 240 : 279 - 283
  • [3] THE STRUCTURE AND MECHANICAL PROPERTIES OF HIGH-PURITY ALUMINIUM ZINC MAGNESIUM ALLOYS
    NUTTING, J
    THOMAS, G
    VARLEY, PC
    DAY, MKB
    SENDOREK, A
    JOURNAL OF THE INSTITUTE OF METALS, 1958, 86 (13): : 542 - 542
  • [4] THE STRUCTURE AND MECHANICAL PROPERTIES OF HIGH-PURITY ALUMINIUM ZINC MAGNESIUM ALLOYS
    VARLEY, PC
    DAY, MKB
    SENDOREK, A
    JOURNAL OF THE INSTITUTE OF METALS, 1958, 86 (08): : 337 - 351
  • [5] ANALYSIS FOR MAGNESIUM IN HIGH-PURITY ALUMINIUM
    YOUNGDAHL, CA
    DEBOER, FE
    NATURE, 1959, 184 (4679) : 54 - 55
  • [6] Effect of stress on corrosion of high-purity magnesium in vitro and in vivo
    Gao, Yuanming
    Wang, Lizhen
    Li, Linhao
    Gu, Xuenan
    Zhang, Kuo
    Xia, Jie
    Fan, Yubo
    ACTA BIOMATERIALIA, 2019, 83 : 477 - 486
  • [7] DEGRADATION OF HIGH-PURITY WATER ON STORAGE
    GABLER, R
    HEGDE, R
    HUGHES, D
    JOURNAL OF LIQUID CHROMATOGRAPHY, 1983, 6 (13): : 2565 - 2570
  • [8] BEHAVIOR OF THE BORDONI RELAXATION IN A HIGH-PURITY MAGNESIUM AFTER PLASTIC-DEFORMATION
    SEYEDREIHANI, SM
    FANTOZZI, G
    ESNOUF, C
    REVEL, G
    SCRIPTA METALLURGICA, 1979, 13 (11): : 1011 - 1015
  • [9] The Separation Behavior of Impurities in the Purification of High-Purity Magnesium via Vacuum Distillation
    Neng Xiong
    Semiramis Friedrich
    Seifeldin R. Mohamed
    Ivan Kirillov
    Xiaozhou Ye
    Yang Tian
    Bernd Friedrich
    Journal of Sustainable Metallurgy, 2022, 8 : 1561 - 1572
  • [10] The Separation Behavior of Impurities in the Purification of High-Purity Magnesium via Vacuum Distillation
    Xiong, Neng
    Friedrich, Semiramis
    Mohamed, Seifeldin R.
    Kirillov, Ivan
    Ye, Xiaozhou
    Tian, Yang
    Friedrich, Bernd
    JOURNAL OF SUSTAINABLE METALLURGY, 2022, 8 (04) : 1561 - 1572