Enhanced electrochemical redox kinetics of La0.6Sr0.4Co0.2Fe0.8O3 in reversible solid oxide cells

被引:13
|
作者
Li, Ping [1 ,2 ]
Liu, Fei [2 ]
Yang, Beibei [2 ]
Wei, Wei [2 ]
Ma, Xinyu [2 ]
Yan, Fei [1 ,2 ]
Gan, Tian [3 ]
Fu, Dong [1 ,2 ]
机构
[1] North China Elect Power Univ, Dept Environm Sci & Engn, Hebei Key Lab Power Plant Flue Gas Multipollutants, Baoding 071003, Peoples R China
[2] North China Elect Power Univ, Sch Environm Sci & Engn, Baoding 071003, Peoples R China
[3] Suzhou Univ Sci & Technol, Sch Chem & Life Sci, Jiangsu Key Lab Environm Funct Mat, Suzhou 215009, Peoples R China
关键词
Perovskite oxide; Reversible solid oxide cell; High-valence cations; Kinetic mechanism; Cell performance; FUEL-CELL; HIGH-PERFORMANCE; PEROVSKITE; ELECTRODE; CATHODE; COMPOSITE;
D O I
10.1016/j.electacta.2023.142069
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Due to its high conversion efficiency in fuel-to-power and power-to-fuel modes, reversible solid oxide cell (RSOC) is widely regarded as a promising device. In this study, La0.6Sr0.4Co0.2Fe0.7M0.1O3 (M=Fe, Mo, Nb) oxides are prepared and composited with Sm0.2Ce0.8O2-(Li0.67Na0.33)2CO3 to form reversible single component cell (RSCC). Among them, La0.6Sr0.4Co0.2Fe0.7Mo0.1O3 (LSCFM) shows the highest oxygen vacancy concentration, further promoting catalytic activity towards oxygen reduction reaction (ORR) and hydrogen oxidation reaction (HOR). Besides, Mo or Nb doping enhances the surface reaction rate constant (kchem) and oxygen chemical bulk diffusion coefficient (Dchem) at the temperature range of 550-700 degrees C. LSCFM shows the highest kchem of 39.3 x 10-5 cm s- 1 , approximate 3.5 times as 11.1 x 10-5 cm s- 1 for La0.6Sr0.4Co0.2Fe0.8O3 (LSCF), and Dchem for LSCFM is 31.1 x 10-6 cm2 s- 1 , approximate 2.5 times as 12.4 x 10-6 cm2 s- 1 for LSCF at 700 degrees C. Furthermore, the rate determining steps (RDS) of ORR and HOR for LSCFM-based cell are the reduction of oxygen atoms to O- and the charge transfer reaction, respectively. Under SOFC/SOEC reversible operation, the RSCC composed of LSCFM exhibits the best cell performance. In the solid oxide fuel cell mode, the maximum power density reaches 236.2 mW cm-2 and in the solid oxide electrolysis cell mode the current density at 1.3 V is-312.4 mA cm- 2.
引用
收藏
页数:10
相关论文
共 50 条
  • [1] IMMITTANCE RESPONSE OF LA0.6SR0.4CO0.2FE0.8O3 BASED ELECTROCHEMICAL-CELLS
    CHEN, CC
    NASRALLAH, MM
    ANDERSON, HU
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1995, 142 (02) : 491 - 496
  • [2] La0.6Sr0.4Co0.2Fe0.8O3 as the anode and cathode for intermediate temperature solid oxide fuel cells
    Hartley, A
    Sahibzada, M
    Weston, M
    Metcalfe, IS
    Mantzavinos, D
    CATALYSIS TODAY, 2000, 55 (1-2) : 197 - 204
  • [3] Moisture Effect on La0.8Sr0.2MnO3 and La0.6Sr0.4Co0.2Fe0.8O3 Cathode Behaviors in Solid Oxide Fuel Cells
    Shen, F.
    Lu, K.
    FUEL CELLS, 2015, 15 (01) : 105 - 114
  • [4] Long term behaviors of La0.8Sr0.2MnO3 and La0.6Sr0.4Co0.2Fe0.8O3 as cathodes for solid oxide fuel cells
    Lu, Kathy
    Shen, Fengyu
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2014, 39 (15) : 7963 - 7971
  • [5] Mechanism of La0.6Sr0.4Co0.2Fe0.8O3 cathode degradation
    Oh, Dongjo
    Gostovic, Danijel
    Wachsman, Eric D.
    JOURNAL OF MATERIALS RESEARCH, 2012, 27 (15) : 1992 - 1999
  • [6] Synthesis and characterization La0.6Sr0.4CoO3 and La0.6Sr0.4Co0.2Fe0.8O3 nanotubes for cathode of solid-oxide fuel cells
    Sacanell, J.
    Bellino, M. G.
    Lamas, D. G.
    Leyva, A. G.
    PHYSICA B-CONDENSED MATTER, 2007, 398 (02) : 341 - 343
  • [7] Mechanism of La0.6Sr0.4Co0.2Fe0.8O3 cathode degradation
    Dongjo Oh
    Danijel Gostovic
    Eric D. Wachsman
    Journal of Materials Research, 2012, 27 : 1992 - 1999
  • [8] Silver infiltrated La0.6Sr0.4Co0.2Fe0.8O3 cathodes for intermediate temperature solid oxide fuel cells
    Sakito, Y.
    Hirano, A.
    Imanishi, N.
    Takeda, Y.
    Yamamoto, O.
    Liu, Y.
    JOURNAL OF POWER SOURCES, 2008, 182 (02) : 476 - 481
  • [9] Cathode supported tubular solid oxide fuel cells with nanostructured La0.6Sr0.4Co0.2Fe0.8O3 electrocatalysts
    Wu, Liuer
    Zhao, Ling
    Zhan, Zhongliang
    Xia, Changrong
    JOURNAL OF POWER SOURCES, 2014, 266 : 268 - 274
  • [10] Influence of sulfur impurities on the stability of La0.6Sr0.4Co0.2Fe0.8O3 cathode for solid oxide fuel cells
    Xie, Jing
    Ju, Young-Wan
    Ishihara, Tatsumi
    SOLID STATE IONICS, 2013, 249 : 177 - 183