Preliminary study on Hot Isostatic Pressing diffusion bonding of Fe-Cr-Al and CLF-1 steel for preparation of tritium permeation barrier

被引:4
|
作者
Du, Pei-Song [1 ,2 ]
Wang, Wan-Jing [1 ,2 ]
Wang, Ji-Chao [3 ]
Xu, Hua-Qi [1 ,2 ]
Wang, Qiao-ling [1 ,2 ]
Xu, Yu-Ping [1 ,2 ]
Zhou, Hai-Shan [1 ,2 ]
Liu, Wei [4 ]
Luo, Guang-Nan [1 ,2 ]
机构
[1] Chinese Acad Sci, Inst Plasma Phys, Hefei 230031, Peoples R China
[2] Univ Sci & Technol China, Hefei 230026, Peoples R China
[3] Inst Energy, Hefei Comprehens Natl Sci Ctr, Hefei 230031, Anhui, Peoples R China
[4] Tsinghua Univ, Sch Mat Sci & Engn, Beijing, Peoples R China
关键词
Fe-Cr-Al ferritic steel; CLF-1; steel; Hot Isostatic Pressing; Ni interlayer; NixAly phase; DESIGN; MICROSTRUCTURE; ALUMINUM; COATINGS; ALLOYS; PRECIPITATION; RESISTANT; OXIDATION; BEHAVIOR;
D O I
10.1016/j.nme.2023.101426
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
In the internal cooling channel forming of the blanket component for fusion reactor, the combination of Fe-Cr-Al ferritic steel with RAFM steel (reduced activation ferritic/martensitic steel) can form alumina film and then be served as tritium permeation barrier (TPB), which can inhibit the penetration of tritium into structural materials. To realize reliable joining between the two materials, Hot Isostatic Pressing (HIP) diffusion bonding, which is considered as the most promising fabrication technique for blanket component was used. The microstructure and mechanical properties of the joints were analyzed, and the results showed that Fe-Cr-Al/CLF-1 steel interfaces generated some large-size AlN, and the interfacial microvoids are not totally eliminated. While adding Ni interlayer between Fe-Cr-Al/CLF-1 steel could significantly reduce the size of AlN and promote interfacial microvoids closure. Fine NiAl and Ni3Al phases, as the strengthening phases in Nickel-based superalloys, were formed due to atom interdiffusion across the interfaces. Fe-Cr-Al/Ni/CLF-1 joints exhibited average tensile strength of 636 and 529 MPa, and elongation rate of 3% and 15% when tested at 25 and 300 degrees C, respectively. Microhardness test demonstrated Fe-Cr-Al/Ni/CLF-1 steel joints could be enhanced by precipitation-hardening of NixAly phases. These preliminary studies have laid a foundation for the preparation of TPB in the cooling channel of blanket components.
引用
收藏
页数:9
相关论文
共 9 条
  • [1] Investigation on the suitability of plasma sprayed Fe-Cr-Al coatings as tritium permeation barrier
    Fazio, C
    Stein-Fechner, K
    Serra, E
    Glasbrenner, H
    Benamati, G
    JOURNAL OF NUCLEAR MATERIALS, 1999, 273 (03) : 233 - 238
  • [2] Diffusion bonding W and RAFM-steel with an Fe interlayer by hot isostatic pressing
    Huang, Pan
    Wang, Yiming
    Peng, Huabei
    Chen, Jiming
    Wang, Pinghuai
    FUSION ENGINEERING AND DESIGN, 2020, 158
  • [3] Preliminary experimental study on Hot Isostatic Pressing diffusion bonding for CLAM/CLAM
    Li, C.
    Huang, Q.
    Zhang, P.
    FUSION ENGINEERING AND DESIGN, 2007, 82 (15-24) : 2627 - 2633
  • [4] Verification of the effect of surface preparation on Hot Isostatic Pressing diffusion bonding joints of CLAM steel
    Zhao, Yanyun
    Li, Chunjing
    Huang, Bo
    Liu, Shaojun
    Huang, Qunying
    JOURNAL OF NUCLEAR MATERIALS, 2014, 455 (1-3) : 486 - 490
  • [5] Study on microstructure and properties between alloy steel and powder steel via hot isostatic pressing diffusion bonding
    Gao, Lei
    Xu, Chunguo
    Ge, Xueyuan
    Hu, Qipeng
    Wang, Xianglong
    Meng, Yuan
    Lu, Shiteng
    Liu, Bo
    MATERIALS TODAY COMMUNICATIONS, 2024, 41
  • [6] Hot isostatic pressing diffusion bonding of V4Cr4Ti alloy/RAFM steel and interface properties of the joints
    Hanjie Xuebao/Transactions of the China Welding Institution, 2022, 43 (07): : 57 - 62
  • [7] A dense Fe-Al/Al2O3 coating as tritium permeation barrier on CLAM steel by hot-dipping aluminizing
    Shao, Zongming
    Yang, Hao
    Zhang, Siwei
    Liu, Weiping
    Xiao, Zunqi
    Zheng, Mingjie
    SURFACE & COATINGS TECHNOLOGY, 2022, 440
  • [8] Hot Isostatic Pressing Diffusion Bonding and Interface Residual Stress Analysis of CuCr1Zr Alloy and 25Cr2Ni4MoV Steel
    Wu, Zhanfang
    Che, Lida
    Wang, Kai
    Lv, Zhoujin
    Li, Xiangyang
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024,
  • [9] Study on the preparation of FeAl/Al2O3 as tritium permeation barrier on 316L stainless steel
    Feng, Jun
    Tong, Hong-Hui
    Jin, Fan-Ya
    Dan, Min
    Shen, Li-Ru
    Chen, Mei-Yan
    Nai, Xin-Chun
    Gongneng Cailiao/Journal of Functional Materials, 2015, 46 (05): : 05101 - 05105