Al-Si alloys; casting; additive manufacturing; Al-Si eutectic; fatigue; mechanical behavior; LOW-CYCLE FATIGUE; TEMPERATURE MECHANICAL-PROPERTIES; MEAN STRESS-RELAXATION; CONTAINING INTERMETALLIC PHASES; WORK-HARDENING CHARACTERISTICS; CAST-ALUMINUM ALLOYS; CU-MG ALLOYS; LOW-PRESSURE; TENSILE PROPERTIES; HEAT-TREATMENT;
D O I
10.3390/met13030609
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
While research on lightweight materials has been carried out for decades, it has become intensified with recent climate action initiatives leading pathways to net zero. Aluminum alloys are at the pinnacle of the light metal world, especially in the automotive and aerospace industries. This review intends to highlight recent developments in the processing, structure, and mechanical properties of structural Al-Si alloys to solve various pressing environmental issues via lightweighting strategies. With the excellent castability of Al-Si alloys, advancements in emerging casting methods and additive manufacturing processes have been summarized in relation to varying chemical compositions. Improvements in thermal stability and electrical conductivity, along with superior mechanical strength and fatigue resistance, are analyzed for advanced Al-Si alloys with the addition of other alloying elements. The role of Si morphology modification, along with particle distribution, size, and precipitation sequencing, is discussed in connection with the improvement of static and dynamic mechanical properties of the alloys. The physics-based damage mechanisms of fatigue failure under high-cycle and low-cycle fatigue loading are further elaborated for Al-Si alloys. The defect, porosity, and surface topography related to manufacturing processes and chemical compositions are also reviewed. Based on the gaps identified here, future research directions are suggested, including the usage of computational modeling of microstructures and the integration of artificial intelligence to produce mass-efficient and cost-effective solutions for the manufacturing of Al-Si alloys.
引用
收藏
页数:64
相关论文
共 50 条
  • [31] The processing-microstructure-property relationship for a multicomponent Nb-Ti-Al alloy
    Loria, EA
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1999, 271 (1-2): : 430 - 438
  • [32] Eutectic modification and microstructure development in Al-Si alloys
    Dahle, AK
    Nogita, K
    McDonald, SD
    Dinnis, C
    Lu, L
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 413 : 243 - 248
  • [33] Microstructure selections in the undercooled hypereutectic Al-Si alloys
    Kang, HS
    Yoon, WY
    Kim, KH
    Kim, MH
    Yoon, YP
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 404 (1-2): : 117 - 123
  • [34] DEFORMATION OF THE ALLOYS AL-SI BY TEMPERATURE-CHANGES
    STETINA, K
    KAFKA, V
    KOVOVE MATERIALY-METALLIC MATERIALS, 1984, 22 (05): : 566 - 576
  • [35] MICROSTRUCTURE AND THERMAL VOLUME CHANGES OF AL-SI ALLOYS
    GAN, CY
    HORNBOGEN, E
    ZEITSCHRIFT FUR METALLKUNDE, 1989, 80 (10): : 692 - 697
  • [36] The Influence of Microstructure and Composition on the Machinability of Al-Si Alloys
    Zedan, Y.
    Samuel, A. M.
    Samuel, F. H.
    Alkahtani, S.
    PROCEEDINGS OF THE 13TH INTERNATIONAL CONFERENCE ON ALUMINUM ALLOYS (ICAA13), 2012, : 843 - 848
  • [37] Effect of barium on the microstructure and properties of Al-Si alloys
    Li, Wei
    Sheng, Xianfeng
    Ji, Jiaqi
    Hu, Yongsha
    Xu, Jin
    Rejiagong Gongyi/Hot Working Technology, 1995, (06): : 27 - 29
  • [38] IMPROVEMENT OF MICROSTRUCTURE IN HYPEREUTECTIC AL-SI ALLOYS BY RHEOCASTING
    ICHIKAWA, K
    ISHIZUKA, S
    TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1987, 28 (05): : 434 - 444
  • [39] Hot deformation behavior and microstructure evolution of a DC cast hypereutectic Al-Si alloy
    He, Kezhun
    Yu, Fuxiao
    Zhao, Dazhi
    Zuo, Liang
    NEW TRENDS IN MECHATRONICS AND MATERIALS ENGINEERING, 2012, 151 : 332 - +
  • [40] A Glance at Processing-Microstructure-Property Relationships for Magnetoelectric Particulate PZT-CFO Composites
    Galizia, Pietro
    Baldisserri, Carlo
    Mercadelli, Elisa
    Capiani, Claudio
    Galassi, Carmen
    Alguero, Miguel
    MATERIALS, 2020, 13 (11)