Bonding durability and remineralizing efficiency of orthodontic adhesive containing titanium tetrafluoride: an invitro study

被引:6
|
作者
Khalifa, Omnia Mahmoud [1 ]
Badawi, Manal Farouk [1 ]
Soliman, Tarek Ahmed [1 ,2 ]
机构
[1] Mansoura Univ, Fac Dent, Dent Biomat Dept, Mansoura, Egypt
[2] New Mansoura Univ, Fac Dent, Prosthet Dent Dept, Mansoura, Egypt
关键词
Bonding; Cariogenic challenge; Orthodontic adhesive; Titanium tetrafluoride; DENTIN PRETREATMENT; ENAMEL; STRENGTH; TIF4; LESIONS; CARIES; DEMINERALIZATION; INHIBITION; INTERFACE; CEMENT;
D O I
10.1186/s12903-023-03063-2
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
BackgroundTitanium tetrafluoride has been shown to protect tooth enamel from demineralization. This study investigated the effect of incorporating different concentrations of TiF4 (1, 2 and 3 Wt.%) into an orthodontic primer on the shear bond strength of orthodontic brackets and the enamel microhardness after cariogenic challenges.MethodsThree different TiF4 concentrations (1, 2 and 3 Wt.%) were prepared and added to the etch and rinse orthodontic primer. Ninety freshly extracted premolars were randomly divided into five groups according to the experimental primers and ageing conditions: TF0, TF0C, TF1C, TF2C, and TF3C. The TF0C group had no TiF4 in the primer, while TF1C, TF2C, and TF3C had 1, 2 and 3 Wt.% TiF4 in the primer, respectively. In the TF0 group, specimens were immersed in deionized water for 24 h as a control group, while all other groups were immersed in a demineralizing solution for 28 days. Each of the five groups was divided into two subgroups: The first group was subjected to shear bond strength and adhesive remnant index testing (N = 50 teeth, 10/group), while the second group was subjected to enamel surface microhardness testing (N = 25 teeth, 50 tooth halves, 10 tooth halves/group). Fifteen teeth (N = 15 teeth, n = 3/group) representing the five groups were subjected to SEM and microelemental analysis (EDX). SBS, ARI, microhardness, and Ca/P ratio were measured, and the data were analyzed using ANOVA and Tukey's tests.ResultsThe TF2C group had the highest SBS value (9.93 +/- 1.23), while the TF0C (5.24 +/- 0.65) and TF3C (5.13 +/- 0.55) had the lowest SBS values. The enamel microhardness in the TF0C group was significantly reduced (p < .001). Enamel microhardness values were significantly (p < .001) higher in groups TF1C, TF2C, and TF3C than in TF0C. The highest Ca/P ratio was significantly recorded for the TF2C group (2.65 +/- 0.02).ConclusionsIncorporation of 1 and 2 Wt.% TiF4 into the orthodontic primers showed adequate bond strength and better remineralization effect. However, 1 Wt.% TiF4 showed lower ARI values than 2 Wt.% TiF4.
引用
收藏
页数:9
相关论文
共 50 条
  • [1] Bonding durability and remineralizing efficiency of orthodontic adhesive containing titanium tetrafluoride: an invitro study
    Omnia Mahmoud Khalifa
    Manal Farouk Badawi
    Tarek Ahmed Soliman
    BMC Oral Health, 23
  • [2] Acid neutralizing and remineralizing orthodontic adhesive containing hydrated calcium silicate
    Yang, Song-Yi
    Han, A. Ruem
    Kim, Kwang-Mahn
    Kwon, Jae-Sung
    JOURNAL OF DENTISTRY, 2022, 123
  • [3] Durability of adhesive bonding of titanium in radiation and aerospace environments
    Bhowmik, S.
    Bonin, H.W.
    Bui, V.T.
    Weir, R.D.
    International Journal of Adhesion and Adhesives, 2006, 26 (06): : 400 - 405
  • [4] Durability of adhesive bonding of titanium in radiation and aerospace environments
    Bhowmik, S
    Bonin, HW
    Bui, VT
    Weir, RD
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2006, 26 (06) : 400 - 405
  • [5] Bonding durability of titanium tetrafluoride treated glass fiber post with resin cement
    Elsaka, Shaymaa E.
    Elnaghy, Amr M.
    DENTAL MATERIALS JOURNAL, 2019, 38 (02) : 189 - 195
  • [6] Fluoride-containing adhesive: Durability on dentin bonding
    Shinohara, Mirela S.
    De Goes, Mario F.
    Schneider, Luis Felipe J.
    Ferracane, Jack L.
    Pereira, Patricia N. R.
    Di Hipolito, Vinicius
    Nikaido, Toru
    DENTAL MATERIALS, 2009, 25 (11) : 1383 - 1391
  • [7] Antibacterial and remineralizing orthodontic adhesive containing quaternary ammonium resin monomer and amorphous calcium phosphate nanoparticles
    Liu, Yan
    Zhang, Ling
    Niu, Li-na
    Yu, Tao
    Xu, Hockin H. K.
    Weir, Michael D.
    Oates, Thomas W.
    Tay, Franklin R.
    Chen, Ji-hua
    JOURNAL OF DENTISTRY, 2018, 72 : 53 - 63
  • [8] DIRECT ORTHODONTIC BONDING TO PORCELAIN - AN INVITRO STUDY
    WINCHESTER, LJ
    REYNOLDS, IR
    JOURNAL OF DENTAL RESEARCH, 1989, 68 (04) : 578 - 578
  • [9] Development of a remineralizing calcium phosphate nanoparticle-containing self-etching system for orthodontic bonding
    Noor M. H. Garma
    Ali I. Ibrahim
    Clinical Oral Investigations, 2023, 27 : 1483 - 1497
  • [10] Development of a remineralizing calcium phosphate nanoparticle-containing self-etching system for orthodontic bonding
    Garma, Noor M. H.
    Ibrahim, Ali I.
    CLINICAL ORAL INVESTIGATIONS, 2023, 27 (04) : 1483 - 1497